| Effect of Swirling Flow out of Nozzle on Flow Field in Continuous Casting of Billet |
|
Cite this article:
. Effect of Swirling Flow out of Nozzle on Flow Field in Continuous Casting of Billet. Acta Metall Sin, 2008, 44(3): 375-380 .
|
|
|
Abstract Electromagnetic stirrer was fixed on intermediate zone of the nozzle to make molten steel outflow with swirling flow, reduce dashing depth of molten steel and form a up reversing flow. All of these were to get the mold powder melted, shell solidified and uniform composition in the continuous casting of special steel billet. This paper was to simulate the effect of electromagnetic stirring in submerged entry nozzle (SEN) through setting a swirl blade in SEN of the hydromechanics mode. This method used was to impart swirl to the flow. On the basic of this, the vertical velocity and horizon velocity of liquid level in the model were measured using Ultrasonic Doppler Velocity (UDV).The effectiveness of electromagnetic stirrer and analyzing technological parameter were examined. Following issues were obtained: (1) Swirling flow was in favor of flow field in mold. (2)The dashing depth can be reduced effectively. (3)The reversing flow and heat transmission of meniscus were enlarged. (4)The horizon circulating was formed so the activity of liquid level and the effectiveness of molten slag were increased.
|
|
Received: 29 August 2007
|
|
|
[1]Yokoya S,Asako Y,Hara S,Szekely J.ISIJ Int,1994;34: 883 [2]Yokoya S,Westoff R,Asako Y,Hara S,Szekely J.ISIJ Int,1994;34:889 [3]Yeong H H.ISIJ Int,1996;36:1030 [4]Yokoya S,Takagi S,Iguchi M,Asako Y,Westoff R,Hara S.ISIJ Int,1998;38:827 [5]Yokoya S,Takagi S,Iguchi M,Marukawa K,Yasugaira W, Hara S.ISIJ Int,2000;40:584 [6]Yokoya S,Takagi S,Tada K,Iguchi M,Marukawa K,Hara S.ISIJ Int,2001;41:1201 [7]Yokoya S,Takagi S,Ootani S,Iguchi M,Marukawa K, Hara S.ISIJ Int,2001;41:1208 [8]Yokoya S.ISIJ Int,2001;41(Suppl.):S47 [9]Zhang H,Wang T F,Wang J F,Jin Y.J Chem Eng Chin Univ,2002;16:408 (张欢,王铁峰,王金福,金涌.高校化学工程学报,2002;16:408) [10]Yu Z,Lei Z S,Jia H H,Jin X L,Ren Z M,Deng K,Zhong Y B.Shanghai Met,2007;29(2):54 (于湛,雷作胜,贾洪海,金小礼,任忠鸣,邓康,钟云波.上海金属,2007;29(2):54) [11]Li B K,Li D H.Acta Metall Sin,2002;38:315 (李宝宽,李东辉.金属学报,2002;38:315) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|