Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (3): 375-380     DOI:
Research Articles Current Issue | Archive | Adv Search |
Effect of Swirling Flow out of Nozzle on Flow Field in Continuous Casting of Billet
Cite this article: 

. Effect of Swirling Flow out of Nozzle on Flow Field in Continuous Casting of Billet. Acta Metall Sin, 2008, 44(3): 375-380 .

Download:  PDF(802KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Electromagnetic stirrer was fixed on intermediate zone of the nozzle to make molten steel outflow with swirling flow, reduce dashing depth of molten steel and form a up reversing flow. All of these were to get the mold powder melted, shell solidified and uniform composition in the continuous casting of special steel billet. This paper was to simulate the effect of electromagnetic stirring in submerged entry nozzle (SEN) through setting a swirl blade in SEN of the hydromechanics mode. This method used was to impart swirl to the flow. On the basic of this, the vertical velocity and horizon velocity of liquid level in the model were measured using Ultrasonic Doppler Velocity (UDV).The effectiveness of electromagnetic stirrer and analyzing technological parameter were examined. Following issues were obtained: (1) Swirling flow was in favor of flow field in mold. (2)The dashing depth can be reduced effectively. (3)The reversing flow and heat transmission of meniscus were enlarged. (4)The horizon circulating was formed so the activity of liquid level and the effectiveness of molten slag were increased.
Key words:  Billet      Continuous casting      Swirling flow nozzle      Magnetic stirring      Water simulation      
Received:  29 August 2007     
ZTFLH:  TF777  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I3/375

[1]Yokoya S,Asako Y,Hara S,Szekely J.ISIJ Int,1994;34: 883
[2]Yokoya S,Westoff R,Asako Y,Hara S,Szekely J.ISIJ Int,1994;34:889
[3]Yeong H H.ISIJ Int,1996;36:1030
[4]Yokoya S,Takagi S,Iguchi M,Asako Y,Westoff R,Hara S.ISIJ Int,1998;38:827
[5]Yokoya S,Takagi S,Iguchi M,Marukawa K,Yasugaira W, Hara S.ISIJ Int,2000;40:584
[6]Yokoya S,Takagi S,Tada K,Iguchi M,Marukawa K,Hara S.ISIJ Int,2001;41:1201
[7]Yokoya S,Takagi S,Ootani S,Iguchi M,Marukawa K, Hara S.ISIJ Int,2001;41:1208
[8]Yokoya S.ISIJ Int,2001;41(Suppl.):S47
[9]Zhang H,Wang T F,Wang J F,Jin Y.J Chem Eng Chin Univ,2002;16:408 (张欢,王铁峰,王金福,金涌.高校化学工程学报,2002;16:408)
[10]Yu Z,Lei Z S,Jia H H,Jin X L,Ren Z M,Deng K,Zhong Y B.Shanghai Met,2007;29(2):54 (于湛,雷作胜,贾洪海,金小礼,任忠鸣,邓康,钟云波.上海金属,2007;29(2):54)
[11]Li B K,Li D H.Acta Metall Sin,2002;38:315 (李宝宽,李东辉.金属学报,2002;38:315)
[1] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[2] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[3] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[4] JIANG Jufu, ZHANG Yihao, LIU Yingze, WANG Ying, XIAO Guanfei, ZHANG Ying. Research on AlSi7Mg Alloy Semi-Solid Billet Fabricated by RAP[J]. 金属学报, 2021, 57(6): 703-716.
[5] GUO Zhongao, PENG Zhiqiang, LIU Qian, HOU Zibing. Nonuniformity of Carbon Element Distribution of Large Area in High Carbon Steel Continuous Casting Billet[J]. 金属学报, 2021, 57(12): 1595-1606.
[6] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[7] ZHANG Lin, GUO Xiao, GAO Jianwen, DENG Anyuan, WANG Engang. Effect of Electromagnetic Stirring on Microstructure and Mechanical Properties of TiB2 Particle-Reinforced Steel[J]. 金属学报, 2020, 56(9): 1239-1246.
[8] CAI Laiqiang, WANG Xudong, YAO Man, LIU Yu. Meshless Method for Non-Uniform Heat Transfer/Solidification Behavior of Continuous Casting Round Billet[J]. 金属学报, 2020, 56(8): 1165-1174.
[9] REN Zhongming,LEI Zuosheng,LI Chuanjun,XUAN Weidong,ZHONG Yunbo,LI Xi. New Study and Development on Electromagnetic Field Technology in Metallurgical Processes[J]. 金属学报, 2020, 56(4): 583-600.
[10] LI Yaqiang, LIU Jianhua, DENG Zhenqiang, QIU Shengtao, ZHANG Pei, ZHENG Guiyun. Peritectic Solidification Characteristics and Mechanism of 15CrMoG Steel[J]. 金属学报, 2020, 56(10): 1335-1342.
[11] Chunlei WU,Dewei LI,Xiaowei ZHU,Qiang WANG. Influence of Electromagnetic Swirling Flow in Nozzle on Solidification Structure and Macrosegregation of Continuous Casting Square Billet[J]. 金属学报, 2019, 55(7): 875-884.
[12] GUO Junli, WEN Guanghua, FU Jiaojiao, TANG Ping, HOU Zibing, GU Shaopeng. Influence of Cooling Rate on the Contraction of Peritectic Transformation During Solidification of Peritectic Steels[J]. 金属学报, 2019, 55(10): 1311-1318.
[13] Zibing HOU, Rui XU, Yi CHANG, Jianghai CAO, Guanghua WEN, Ping TANG. Time-Series Fluctuation Characteristics of Segregation Carbon Element Distribution Along Casting Direction in High Carbon Continuous Casting Billet[J]. 金属学报, 2018, 54(6): 851-858.
[14] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[15] Xinhua LIU, Huadong FU, Xingqun HE, Xintong FU, Yanqing JIANG, Jianxin XIE. Numerical Simulation Analysis of Continuous Casting Cladding Forming for Cu-Al Composites[J]. 金属学报, 2018, 54(3): 470-484.
No Suggested Reading articles found!