Abstract Phase distribution and grain size are the key factors controlling the coercivity of nanocomposite permanent magnets. Assuming three simple physical models, we have calculated the dependence of coercivity on the grain size, phase distribution and volume fraction of two phases. The calculation results show that the different phase distributions lead to the variation of grain-interface fractions, and then make the intergrain exchange-coupling fluctuate randomly. Phase distribution influences the values of coeicivity of nanocomposites, but does not change the variation tendency of coercivity on hard grain size. High coercivity can be probably obtained by designing an ideal phase distribution and controlling the grain sizes.
[1]Manaf A,Buckley R A,Davies H A,Leonowicz M.J Magn Magn Mater,1991;101:360 [2]Betancourt J I,Davies R H A.J Magn Magn Mater,2002; 246:6 [3]Billona O V,Urreta S E,Fabietti L M,Bertorello H R.J Magn Magn Mater,1998;187:371 [4]Feng W C,Gao R W,Yan S S,Li W,Zhu M G.J Appl Phys,2005;98:044305 [5]Fukunaga H,Kuma J,Kanai Y.IEEE Trans Magn,1999; 35:3235 [6]Sun X K,Zhang J,Chu Y L,Liu W,Cui B Z,Zhang Z D.Appl Phys Lett,1999;74:1740 [7]Bauer J,Seager M,Zero A,Kronmüller H.J Appl Phys, 1996;80:1667 [8]Xiao Q F,Zhao T,Zhang Z D.J Magn Magn Mater,2001; 223:215 [9]Liu W,Zhang Z D,Liu J P,Chen L J,He L H,Liu Y, Sun X K,Sellmyer D J.Adv Mater,2002;14:1832 [10]Liu W,Zhang Z D,Liu J P,Dai Z R,Wang Z L,Sun X K,Sellmyer D J.J Phys,2003;36D:63 [11]Skomski R,Coey J M D.IEEE Trans Magn,1993;29: 2860 [12]Arcas J,Hernando A,Barandiaran J M.Phys Rev,1998; 58B:5193 [13]Chena Z M,Wu Y Q,Kramerb M J,Smith B R,Ma B M,Huang M W.J Magn Magn Mater,2004;268:105 [14]Melsheimer A,Seeger M,Kronmüller H.J Magn Magn Mater,1999;202:458 [15]Kronmiiller H,Fischer R,Seeger M,Zern A.J Phys,1996; 29D:2274 [16]Kneller E F,Hawig R.IEEE Trans Magn,1991;27:3588 [17]Feng W C,Gao R W,Han G B,Zhu M G,Li W.Acta Phys Sin,2004;53:3171 (冯维存,高汝伟,韩广兵,朱明刚,李卫.物理学报,2004;53:3171)