| SUPERPLASTICITY OF ALUMINIUM SERIES INTERMETALLIC COMPOUND |
| ;; |
| 吉林大学超塑性与塑性研究所 |
|
Cite this article:
. SUPERPLASTICITY OF ALUMINIUM SERIES INTERMETALLIC COMPOUND. Acta Metall Sin, 2008, 44(1): 1-7 .
|
|
|
Abstract Based on basic conceptions of superplasticity and intermetallic compound, the significance of studying the supeplasticity of intermetallic compound is adressed. And recent advances in superplasticity in Ni-Al, Ti-Al and Fe-Al aluminium series intermetallic componund are reviewd.
|
|
Received: 15 August 2007
|
|
|
[1]Wu S D.Theory of Metal Superplastic Deformation.Bei- jing:National Defence Industry Press,1997:1 (吴诗惇.金属超塑性变形理论.北京:国防工业出版社,1997:1) [2]Chokshi A H,Mukherjee A K,Langdon T G.Mater Sci Eng,1993;R10:237 [3]Song Y Q.Aeronaut Manuf Technol,2003;(7):17 (宋玉泉.航空制造技术,2003;(7):17) [4]Chen G L.Shanghai Met,2002;24(4):1 (陈国良.上海金属,2002;24(4):1) [5]Fan R H,Bian X F,Yin Y S.Shandong Sci,1997;10(1): 6 (范润华,边秀房,尹衍升.山东科学,1997;10(1):6) [6]Zhang L T,Mao DL,Wu J S.Shanghai Met,1999;21(2): 18 (张澜庭,毛大立,吴建生.上海金属,1999;21(2):18) [7]Nieh T G,Wadsworth J.Acta Metall Sin(Engl Lett), 1995;8(Z1):405 [8]Liu C T,White C L,Horton J A.Acta Metall,1985;33: 213 [9]Wright R N,Sikka V K.J Mater Sci,1988;23:4315 [10]Mukhopadhyay J,Kaschner G,Mukherjee A K.Scr Met- all Mater,1990;24:857 [11]Valiev R Z,Gayanov R M,Yang H S,Mukherjee A K.Scr Metall Mater,1991;25:1945 [12]Guo J T.Ordered Intermetallic Compound NiAl Alloy. Beijing:Science Press,2003:231 (郭建亭.有序金属间化合物镍铝合金.北京:科学出版社,2003:231) [13]Mishra R S,Valiev R Z,McFadden S X,Mukherjee A K. Mater Sci Eng,1998;A252:174 [14]McFadden S X,Valiev R Z,Mukherjee A K.Mater Sci Eng,2001;A319-321:849 [15]Gu Y F,Lin D L,Shan A D,Liu Y,Liu Z Y.Acta Metall Sin,1997;33:325 (谷月峰,林栋梁,单爱党,刘毅,刘震云.金属学报,1997;33:325) [16]Guha S,Baker I,Munroe P R.J Mater Sci,1996;31: 4055 [17]Chen R S,Guo J T,Yin W M,Zhou J Y.Acta Metall Sin,1998;34:1121 (陈荣石,郭建亭,殷为民,周继扬.金属学报,1998;34:1121) [18]Chen R S,Guo J T,Yin W M,Zhou J Y.Scr Mater,1999; 40:209 [19]Zhou W L,Guo J T,Chen R S,Zhou J Y.Acta Metall Sin,1999;35:995 (周文龙,郭建亭,陈荣石,周继扬.金属学报,1999;35:995) [20]Zhou W L,Guo J T,Chen R S,Li G S,Zhou J Y.Mater Lett,2001;47:30 [21]Zhou W L,Guo J T,Chen R S,Zhou J Y.Acta Metall Sin,2000;36:796 (周文龙,郭建亭,陈荣石,周继扬.金属学报,2000;36:796) [22]Zhou W L,Guo J T,Chen R S,Zhou J Y.Mater Lett, 2001;51:342 [23]Du X H,Guo J T,Zhou B D.Acta Metall Sin,2001;37: 1112 (杜兴蒿,郭建亭,周彼德.金属学报,2001;37:1112) [24]Du X H,Guo J T,Zhou B D.Mater Lett,2002;52:442 [25]Sundar R S,Kitazono K,Sato E,Kuribayashi K.Acta Mater,2001;49:1717 [26]Du X H,Guo J T,Zhou B D.Scr Mater,2001;45:69 [27]Du X H,Guo J T,Zhou B D.Acta Metall Sin,2001;37: 144 (杜兴蒿,郭建亭,周彼德.金属学报,2001;37:144) [28]Du X H,Guo J T,Zhou B D,Xiong L Y.J Mater Sci Technol,2003;19:373 [29]Hu J,Lin D L.Mater Lett,2004;58:1297 [30]Jiang D M,Lin D L.Mater Lett,2002;57:747 [31]Jiang D M,Lin D L.J Shanghai Jiaotong Univ,2002;36: 597 (蒋冬梅,林栋梁.上海交通大学学报,2002;36:597) [32]Qi Y H,Guo J T,Cui C Y,Li G S.Mater Lett,2002;57: 552 [33]Cui C Y,Guo J T,Qi Y H,Ye H Q.Acta Metall Sin, 2002;38:679 (崔传勇,郭建亭,齐义辉,叶恒强.金属学报,2002;38:679) [34]Qi Y H,Guo J T,Cui C Y.Chin J Nonferrous Met,2002; 12:245 (齐义辉,郭建亭,崔传勇,中国有色金属学报,2002;12:245) [35]Zhang J M,Li S Q,Zou D X,Zhong Z Y.J Iron Steel Res,1995;7(6):75 (张建民,李世琼,邹敦叙,仲增墉.钢铁研究学报,1995;7(6):75) [36]Ameyama K,Fujii T,Okumura T,Sodeoka S,Tokizane M.Mater Sci Forum,1997;233-234:287 [37]Bohn R,Klassen T,Bormann,R.Intermetallics,2001;9: 559 [38]Lu S Q,Huang B Y,He Y H.J Nanchang Inst Aeronaut Technol(Nat Sci),2001;15(4):6 (鲁世强,黄伯云,贺跃辉.南昌航空工业学院学报(自然科学版),2001;15(4):6) [39]Sun J,Wu J S,Zhang H Y,He Y H,Deng Z Y.Rare Met Mater Eng,2000;29:13 (孙坚,吴建生,张惠义,贺跃辉,邓忠勇.稀有金属材料与工程,2000;29:13) [40]Huang B Y,He Y H,Deng Z Y,Wang J N,Sun J.Acta Metall Sin,1998;34:1173 (黄伯云,贺跃辉,邓忠勇,王健农,孙坚.金属学报,1998;34:1173) [41]Sun F,Lin D L.J Shanghai Jiaotong Univ,2001;35:380 (孙锋,林栋梁.上海交通大学学报,2001;35:380) [42]Deng Z Y,Huang B Y,He Y H,Liu Y.J Mater Eng,1999; (12):26 (邓忠勇,黄伯云,贺跃辉,刘咏.材料工程,1999;(12):26) [43]Mishra R S,Mukherjee A K.d Mater Sci,2000;35:147 [44]Imayev R M,Kaibyshev O A,Salishchev G A.Acta Metall Mater,1992;40:581 [45]Imayev V M,Imayev R M,Kuznetsov A V,Shagiev M R, Salishchev G A.Mater Sci Eng,2003;A348:15 [46]Zhou K C,Huang B Y,Qu X H.J Central South Univ Technol,1998;29:559 (周科朝,黄伯云,曲选辉.中南工业大学学报,1998;29:559 [47]Zhou K C,Huang B Y,Qu X H,Chen X Q.Rare Met Mater Eng,1998;27:336 (周科朝,黄伯云,曲选辉,陈小群.稀有金属材料与工程,1998;27:336) [48]Zhou K C,Huang B Y,Qu X H.Chin J Rare Met,1999; 23:394 (周科朝,黄伯云,曲选辉.稀有金属,1999;23:394) [49]Sun J,Liu R K,Wu J S,He Y H.Acta Metall Sin,2001; 37:95 (孙坚,刘润开,吴建生,贺跃辉.金属学报,2001;37:95) [50]Sun J,Fu Y F,Wu J S,He Y H.J Mater Eng,1999;(9): 13 (孙坚,傅拥峰,吴建生,贺跃辉.材料工程,1999;(9):13) [51]Shi X H,Zhang D,Ge Y,Qin J N,Zhang G D.Mater Sci Eng,1998;16:24 (施幸华,张荻,葛云,覃继宁,张国定.材料科学与工程,1998;16:24) [52]Zhang D,Qin J N,Shi X H.Rare Met Mater Eng,1998; 27:210 (张荻,覃继宁,施幸华.稀有金属材料与工程,1998;27:210) [53]Sun F,Lin D Y.Trans Nonferrous Met Soc Chin,2002; 12:615 [54]Durra A,Banerjee D.Scr Metall Mater,1990;24:1319 [55]Yang H S,]in P,Mukherjee A K.Mater Sci Eng,1992; A153:457 [56]Wang B,Jia T C,Zou D X,Mall P,Zhong Z Y.Mater Sci Eng,1992;A153:422 [57]Wang B,Jia T C,Wang Y Q,Zou D X,Zhong Z Y.Acta Metall Sin,1994;30:B309 (王斌,贾天聪,王跃群,邹敦叙,仲增墉.金属学报,1994;30:B309) [58]Song D,Ding H,Wang D L.J Northeastern Univ(Nat Sci),2001;22:660 (宋丹,丁桦,王殿梁.东北大学学报(自然科学版),2001;22:660) [59]Ding H,Song D,Du Y H,Zhang C B,Cui J Z,Bai B Z, Wan C J.J Iron Steel Res,1999;11(3):34 (丁桦,宋丹,杜云蕙,张彩碚,崔建忠,白秉哲,万初杰.钢铁研究学报,1999;11(3):34) [60]Sun F S,Ma J M,Cao C X.Acta Metall Sin,1994;30: B465 (孙福生,马济民,曹春晓.金属学报,1994;30:B465) [61]Imayev R M,Gabdullin N,Salishchev G.Intermetallics, 1997;5:229 [62]Rosenberg Y,Mukherjee A K.Mater Sci Eng,1995; A192/193:788 [63]Li D Q,Liu Y,Shan A D,Lin D L.Acta Metall Sin,1996; 32:417 (郦定强,刘毅,单爱党,林陈梁.金属学报,1996;32:417) [64]Li D Q,Shan A D,Liu Y,Lin D L.Scr Metall Mater, 1995;33:681 [65]Liu Y,Li D Q,Lin D L,Chen S P,Zhao X N,Hong J M. J Chin Electron Microsc Soc,1995;14:421 (刘毅,郦定强,林栋梁,陈世仆,赵晓宁,洪建明.电子显微学报,1995;14:421) [66]Li D Q,Lin D L,Liu J L,Liu Y.Acta Metall Sin,1997; 33:897 (郦定强,林栋梁,刘俊亮,刘毅.金属学报,1997;33:897) [67]Lin D,Li D,Liu Y.Intermetallics,1998;6:243 [68]Lin D,Liu Y.Mater Sci Eng,1999;A268:83 [69]Lin D,Shan A,Li D.Scr Metall Mater,1994;31:1455 [70]Lin D,Lin T L,Shan A,Chen M.Intermetallics,1996;4: 489 [71]Hu J,Lin D L.Trans Mater Heat Treat,2003;24:31 (胡静,林栋梁.材料热处理学报,2003;24:31) [72]Chen M W,Shan A D,Lin D L.Trans Met Heat Treat, 1995;16(3):9 (陈明伟,单爱党,林栋梁.金属热处理学报,1995;16(3):9) [73]Yang Y J,Shan A D,Lin D L.J Shanghai College Metall, 1999;20(3):140 (羊忆军,单爱党,林栋梁.上海冶金高等专科学校学报,1999;20(3):140) [74]Gao D C,Yang W Y,Huang X X,Sun Z Q.Acta Metall Sin,2001;37:291 (高德春,杨王玥,黄晓旭,孙祖庆.金属学报,2001;37:291) [75]Sharma G,Kishore R,Sundararaman M,Ramanujan R V.Mater Sci Eng,2006;A419:144 [76]Guo J T,Zhou W L.Mater Rev,2000;14(5):18 (郭建亭,周文龙.材料导报,2000;14(5):18) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|