VERIFICATION OF THREE 3D INDIVIDUAL GRAIN GROWTH RATES WITH LARGE-SCALE MONTE CARLO SIMULATION
;;
北京科技大学
Cite this article: 

. VERIFICATION OF THREE 3D INDIVIDUAL GRAIN GROWTH RATES WITH LARGE-SCALE MONTE CARLO SIMULATION. Acta Metall Sin, 2008, 44(1): 13-18 .

Download:  PDF(246KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Three existing topological dependence equations for the growth rate of three-dimensional individual grains have been testified using a new Potts model Monte Carlo simulation. The result shown that the volume change rate dVf/dt is related to the face number f by a curve, and thus, Rivier’s grain growth rate equation that predicts dVf/dt ∝f is not confirmed. Yu-Liu’s grain growth rate equation and MacPherson-Srolovitz’s grain growth rate equation are confirmed by mean of the simulation in the case of the face number f≥8. Yu-Liu’s grain growth rate equation and MacPherson-Srolovitz’s grain growth rate equation are not valid in the case of the face number f<8.
Key words:  Three–dimensional grain growth      topology-dependent grain growth rate equation      large-scale Potts Mont     
Received:  28 May 2007     
ZTFLH:  TG111  
  O189  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I1/13

[1]Beck P A,Holaworth M L,Hu H.Phys Rev,1948;73:526
[2]Burke J E.Trans AIME,1949;180:73
[3]Turnbull D.Trans AIME,1951;191:661
[4]von Neumann J.In:Herring C,ed.,Metal Interfaces, Cleveland,American Society for Metals,1952:108
[5]Mullins W W.In:Robertson W D,Gjostein N A,eds., Metal Surfaces:Structure,Energetics,and Kinetics,Met- als Park,OH:American Society for Metals,1963:17
[6]Mullins W W.J Appl Phys,1956;27:900
[7]Rivier N.Philos Mag,1983;47B:245
[8]Yu H B,Liu G Q.Chin Sci Bull,1996;41:2000 (于海波,刘国权.科学通报,1996;41:2000)
[9]Liu G Q,Yu H B,Song X Y,Qin X G.Mater Des,2001; 22:33
[10]Liu G Q,Song X Y,Yu H B,Gu N J.Acta Metall Sin, 1999;35:245 (刘国权,宋晓艳,于海波,谷南驹.金属学报,1999;35:245)
[11]Wang C,Liu G Q,Yu H B.Acta Metall Sin,2004;40: 1233 (王超,刘国权,于海波.金属学报,2004;40:1233)
[12]MacPherson R D,Srolovitz D J.Nature,2007;446:1053
[13]Qin X G.Doctorate Dissertation,University of Science and Technology Beijing,2003 (秦湘阁.北京科技大学博士学位论文,2003)
[14]Glazier J A.Phys Rev Lett,1993;70:2170
[15]Radhakrishnan B,Zacharia T.Metall Mater Trans,1995; 26A:167
[1] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[2] . Analysis of the Correlation between the Energy and Crystallographic Orientation of Grain Boundaries in Fe Based on Atomistic Simulations[J]. 金属学报, 0, (): 0-0.
[3] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[6] . Liquid–solid Phase Separation Process of Pb–Al Alloy Under the Effect of Electric Current Pulses[J]. 金属学报, 0, (): 0-0.
[7] . Phase Transformation Behaviors in the Heat-Affected Zones of Ferritic Heat-Resistant Steels Enabled by In Situ CSLM Observation[J]. 金属学报, 0, (): 0-0.
[8] HAN Weizhong, LU Yan, ZHANG Yuheng. Mechanism of Ductile-to-Brittle Transition in Body-Centered-Cubic Metals:A Brief Review[J]. 金属学报, 2023, 59(3): 335-348.
[9] WANG Meng, YANG Yongqiang, Trofimov Vyacheslav, SONG Changhui, ZHOU Hanxiang, WANG Di. Effects of Particle Size on Processability of AlSi10Mg Alloy Manufactured by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 147-156.
[10] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[11] YANG Ping, WANG Jinhua, MA Dandan, PANG Shufang, CUI Feng'e. Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing[J]. 金属学报, 2022, 58(10): 1261-1270.
[12] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[13] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[14] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[15] PAN Fusheng, JIANG Bin. Development and Application of Plastic Processing Technologies of Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1362-1379.
No Suggested Reading articles found!