| CRYSTALLOGRAPHIC ANALYSIS OF THE FRACTURE FACETS IN LOW TEMPERATURE BRITTLE FRACTURE OF A HIGH NITROGEN BEARING AUSTENITIC STEEL |
| ;;; |
| 大连交通大学 |
|
Cite this article:
;. CRYSTALLOGRAPHIC ANALYSIS OF THE FRACTURE FACETS IN LOW TEMPERATURE BRITTLE FRACTURE OF A HIGH NITROGEN BEARING AUSTENITIC STEEL. Acta Metall Sin, 2007, 43(12): 1233-1238 .
|
|
|
Abstract Microstructures and crystallographic features in low temperature brittle fracture of 18Cr-18Mn-0.7N high nitrogen bearing austenitic steel were investigated by means of scanning electronic microscopy. The results showed that there are three kinds of fracture facets on the fracture surface: annealing twin boundary fracture facet, intergranular fracture facet and transgranular fracture facet. Annealing twin boundary facture facet is one of planar and smooth {111} planes, with bent steps on it, and the planar deformations proceeding on the other three sets of {111} planes form a pattern of three sets of straight-lines intersected at 60º on the annealing twin boundary facet. Intergranular facture facet is a kind of smoothly curved facet on which the planar deformations proceeding on {111} planes form a pattern of several sets of curved parallel lines that intersect each other at different angles. Transgranular facture facet is rough and uneven, with steps parallel to {111} plane and river patterns or edge patterns on it, which is the consequence of coalescence of cracks propagating on different {111} planes.
|
|
Received: 01 February 2007
|
|
|
[1]Cui D W,Qu X H,Li K.Mater Rev,2005;19(12):64 (崔大伟,曲选辉,李科.材料导报,2005;19(12):64) [2]Tsuchiyama T,Ito H,Kataoka K.Metall Mater Trans, 2003;34A:1626 [3]Tobler R L,Leyn D.Metall Thins,1988;19A:1626 [4]Tomota Y,Endo S.Iron Steel lnst Jpn Int,1990;30:656 [5]Tomota Y,Xia Y,Inoue K.Acta Mater,1998;46:1577 [6]Chen K M,Dai Q X.J Iron Steel Res,1998;10(1):38 (陈康敏,戴起勋.钢铁研究学报,1998;10(1):38) [7]Wang A D,Dai Q X,Cheng X N.J Jiangsu Univ Sci Technol(Nat Sci),2000;21(5):59 (王安东,戴起勋,程晓农.江苏理工大学学报(自然版),2000;21(5):59) [8]Liu S C,Hashida T,Takahashi H,Kuwano H,Hamaguchi Y.Metall Mater Trans,1998;29A:791 [9]Liu S C,Liu D Y,Dai Y K.Acta Metall Sin,2002;38: 1042 (刘世程,刘德义,戴雅康.金属学报,2002;38:1042) [10]Liu S Y,Liu S C,Liu D Y.J Mater Sci,2004;39:28418 [11]Liu S C,Liu D Y,Chen R S,Dai Y K.Trans Mater Heat Treat,2005;26(4):33 (刘世程,刘德义,陈汝淑,戴雅康.材料热处理学报,2005;26(4):33) [12]Liao Q C,Sun F Y,Lan F L.Acta Metall Sin,1979;15(1): 77 (廖乾初,孙福玉,蓝芬兰.金属学报,1979;15(1):77) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|