study on corrosion electrochemical behavior of silane coating with flaked
Zhou Wen-Juan;Likun Xu;Jia Wang;;;
中船重工725所
Cite this article: 

Zhou Wen-Juan; Likun Xu; Jia Wang. study on corrosion electrochemical behavior of silane coating with flaked. Acta Metall Sin, 2007, 43(9): 983-988 .

Download:  PDF(368KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The corrosion electrochemical behavior of a silane coating with flaked Zn-Al powder on carbon steel was studied in 3.5% NaCl solution using open circuit potential monitoring, potentiodynamic polarization, electrochemical impedance spectroscopy(EIS) and scanning electron microscope(SEM). The results indicated that the process of deterioration of the coating presented three stages with immersion. At the initial stage, the flaked zinc powder on the surface layer of the coating started to activate with the attack of the electrolyte; the middle stage showed the feature of electrochemical protection of the coating for the substrate; and the barrier protection of the coating predominated in the last stage. The middle stage lasted a long period while the third stage had a short time, suggesting a strong cathodic protection and a weak barrier mechanism of corrosion prevention of the silane coating with zinc and aluminum powder.
Key words:  Zn-Al coating      silane      corrosion      
Received:  16 January 2007     
ZTFLH:  TG142.2  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I9/983

[1]Fourez M,Gheno F,White P E.Trans Inst Met Finish, 1993;71:21
[2]Lonca M.Finishing,1990;14:35
[3]Wynn P.Trans Inst Met Finish,2003;81:16
[4]Bastos A C,Ferreira M G S.Simoes A M.Prog Org Coat, 2005;52:339
[5]Zubielewicz M,Gnot W.Prog Organic Coat,2004;49:358
[6]Le Pen C,Vereecken J.J Appl Electrochem,2005;35: 1303
[7]Ferreira M G S,Duarte R G,Montemo M F,Sim(?)es A M P.Electrochimica Acta,2004;49:2927
[8]Xie D M,Feng H,Ms X C.Corros Sci Prot Technol,2005; 17:237 (谢德明,冯海,马晓春.腐蚀科学与防护技术,2005;17:237)
[9]Marchebois H,Savall C,Bernard J,Touzain S.Elec- trochim Acta,2004;49:2945
[10]Zhang J T.Doctoral Dissertation,Zhejiang University, Hangzhou,2005 (张金涛.浙江大学博士学位论文,杭州,2005)
[11]Xie D M,Tong S P,Feng H,Zhang J Q.Acta Metall Sin, 2005;41:769 (谢德明,童少平,冯海,张鉴清.金属学报,2005;41:769)
[12]Ostanina T N,Rudo V M i,Yaroslavtseva O V,Solov'ev A S,Subbotina O Y,Dokashenko S I.Russ J Electrochem, 2004;40:1019
[13]Wen G N.J Northeast Univ(Nat Sci),1999;20:65 (文光男.东北大学学报(自然科学版),1999;20:65)
[14]Marchebois H,Touzain S,Joiret S,Bernard J,Savall C. Prog Org Coat,2002;15:454
[15]Sun Q X,Zhang J Q,Lin C J.Acta Phys Chim Sin,2004; 20:1297 (孙秋霞,张鉴清,林昌健.物理化学学报,2004;20:1297)
[16]Xie D M,Hu J M,Tong S P,Wang J M,Zhang J Q.Acta Metall Sin,2004;40:103 (谢德明,胡吉明,童少平,王建明,张鉴清.金属学报,2004;40:103)
[17]Senkevich J J.J Mater Sci,2000;35:1359
[18]Liu J G,Gong G P,Yah C W.Electrochim Acta,2005; 50:332.
[1] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[2] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[3] CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang. Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment[J]. 金属学报, 2023, 59(7): 926-938.
[4] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[5] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[6] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[7] XU Linjie, LIU Hui, REN Ling, YANG Ke. Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy[J]. 金属学报, 2023, 59(4): 577-584.
[8] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[9] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[10] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[11] LIAO Jingjing, ZHANG Wei, ZHANG Junsong, WU Jun, YANG Zhongbo, PENG Qian, QIU Shaoyu. Periodic Densification-Transition Behavior of Zr-Sn-Nb-Fe-V Alloys During Uniform Corrosion in Superheated Steam[J]. 金属学报, 2023, 59(2): 289-296.
[12] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[13] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[14] HU Wenbin, ZHANG Xiaowen, SONG Longfei, LIAO Bokai, WAN Shan, KANG Lei, GUO Xingpeng. Corrosion Behavior of AlCoCrFeNi2.1 Eutectic High-Entropy Alloy in Sulfuric Acid Solution[J]. 金属学报, 2023, 59(12): 1644-1654.
[15] SONG Jialiang, JIANG Zixue, YI Pan, CHEN Junhang, LI Zhaoliang, LUO Hong, DONG Chaofang, XIAO Kui. Corrosion Behavior and Product Evolution of Steel for High-Speed Railway Bogie G390NH in Simulated Marine and Industrial Atmospheric Environment[J]. 金属学报, 2023, 59(11): 1487-1498.
No Suggested Reading articles found!