| EFFECTS OF ABSORPTION/DESORPTION CYCLES ON HYDROGEN STORAGE PROPERTIES OF V AND V0.9Cr0.1 ALLOY |
| ;;Honghui Cheng;Shenlan Li;Manqi Lv; |
| 中国科学院金属研究所专用器件部 |
|
Cite this article:
Honghui Cheng; Shenlan Li; Manqi Lv. EFFECTS OF ABSORPTION/DESORPTION CYCLES ON HYDROGEN STORAGE PROPERTIES OF V AND V0.9Cr0.1 ALLOY. Acta Metall Sin, 2007, 43(9): 977-982 .
|
|
|
|
|
Received: 10 January 2007
|
|
|
[1]Schober T,Wenzl H,Alefeld G.Hydrogen in Metals II. Vol.29,Berlin:Springer-Verlag,1978:11 [2]Reilly J J,Wiswall R H.Inorg Chem,1970;9:1678 [3]Lynch J F,Libowitz G G,Maeland A J.J Less-Common Met,1984;103:117 [4]Libowitz G G,Maeland A J.J Less-Common Met,1987; 131:275 [5]Esayed A Y,Northwood D O.Int J Hydrogen Energy, 1992;17:211 [6]Lynch J F,Maeland A J,Libowitz G G.Z Phys Chem Neue Folge,1985;145:51 [7]Libowitz G G,Maeland A J,Lynch J F.Brookhaven National Laboratory Rep,BNL 37866,Brookhaven Na- tional Laboratory Associated Universities,Inc.,Upton, New York,1985 [8]Rutherford W M.Mater Sci Forum,1988;31:19 [9]Wiswall R H Jr,Reilly J.J Inorg Nucl Chem,1972;11: 1691 [10]LüM Q,Zhang H F,Wang Y L,Wei W D.J Alloys Compd,1993;191:319 [11]Ko S M,Schmidt L D.Surf Sci,1974;42:508 [12]Ko S M,Schmidt L D.Surf Sci,1975:47:557 [13]Miguel Lagos.Surf Sci,1984;138:L161 [14]Kim J H,Lee H,Lee P S,Seo C Y,Lee J Y.J Alloys Compd,2003;348:293 [15]Liang H,Chen Y G,Yan Y G,Wu C L,Tao M D.Mater Sci Eng,2007;A448:128 [16]Park J G,Kim D M,Jang K J,Han J S,Cho K,Lee J Y. J Alloys Compd,1999;293:150 [17]Shirasaki K,Tamura T,Kuriiwa T,Goto T,Kamegawa A,Takamura H,Okada M.Mater Trans,2002;43:1115 [18]Kagawa A,Ono E,Kusakabe T,Sakamoto Y.J Less- Common Met,1991;172-174:64 [19]Cantrell J S,Bowman R C Jr.J Alloys Compd,1999; 293-295:156 [20]Itoh H,Arashima H,Kubo K,Kabutomori T,Ohnishi K. J Alloys Compd,2005;404-406:417 [21]Schlapbach I.Solid State Commun,1981;38:117 [22]Li S L,Cheng H H,Deng X X,LǜM Q,Chen D M,Yang K.Rare Met Mater Eng,in press (李慎兰,程宏辉,邓小霞,吕曼棋,陈德敏,杨柯.稀有金属材料与工程,待发表) [23]Lynch J F,Maeland A J,Libowitz G G.Z Phys Chem Neue Folgc,Bd,1985;145:S51 [24]Lynch J F,Reilly J J,Millot F.J Phys Chem Solids,1978; 39:883 [25]Lundin C E,Lynch F E,Magee C B.J Less-Common Met,1977;56:19 [26]Mowickand A S,Burton J.Diffusion in Solids.Chap.5, New York:Academic Press,1974 [27]Mordkovich V Z,Korostyshevsky N N,Baychtok Y K, Mazus E I,Dudakova N V,Mordovin V P.Int J Hydro- gen Energy,1990;15:723 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|