Abstract A cluster–plus–glue atom model was employed to design Ni–Nb based ternary bulk metallic glasses. The binary eutectic point Ni59.5Nb40.5 was first interpreted by the model in form of a cluster formula [(Ni0.5Nb0.5)–Ni6Nb6]Ni3, where the cluster is (Ni0.5Nb0.5)–centered icosahedron derived from a eutectic phase Ni6Nb7 (Fe7W6 type). It was then pointed out that the best binary glass former Ni62Nb38 could be interpreted based on the eutectic cluster formula by replacing the cluster center Nb0.5 with Ni0.5, namely [Ni–Ni6Nb6]Ni3=Ni62.5Nb37.5. To further improve the glass–forming ability, Zr, Ta and Ag are selected as alloying additions to partially replace Nb in the [Ni–Ni6Nb6]Ni3 cluster formula, and glassy rods with a critical size of 3 mm are achieved at appropriate ternary compositions by copper–mould suction–casting. DTA measurements indicate these bulk metallic glasses exhibit high thermal stabilities, among which the [Ni–Ni6Nb5Ta]Ni3 alloy has the highest Tg (glass transition temperature)of 935 K and Tx (crystallization temperature) of 952 K. Room–temperature compressive curves of [Ni–Ni6Nb5Zr]Ni3 and [Ni–Ni6Nb5Ta]Ni3 alloys show they have limited plasticity with a elongation of about 0.3%, fracture strength of the [Ni–Ni6Nb5Zr]Ni3 and [Ni–Ni6Nb5Ta]Ni3 BMGs are about 3.2 GPa and 3.4 GPa, respectively.
|
|
Received: 14 February 2011
|
|
|
| Fund: Supported by National Science Foundation of China (Nos.50901012 and 51041011), National Basic Research Program of China (No.2007CB613902) and Cultivation Fund of the Key Scientific and Technical Innovation Project, Ministry of Education of China (No.707015) |
| [1] Inoue A. Acta Mater, 2000; 48: 279[2] Inoue A, Shen B L, Takeuchi A. Mater Trans, 2006; 47: 1275[3] Kimura H, Inoue A, Yamaura S. Mater Trans, 2003; 62: 1167[4] Xu D H, Duan G, Johnson W L, Garland C. Acta Mater, 2004; 52: 3493[5] Ruhl R C, Giessen B C, Cohen M, Grant N J. Acta Metall, 1967; 15: 1693[6] Xia L, Li W H, Fang S S, Wei B C, Dong Y D. J Appl Phys, 2006; 99: 26103[7] Choi–Yim H, Xu D H, JohnsonWL. Appl Phys Lett, 2003; 82: 1030[8] Chen L Y, Hu H T, Zhang G Q, Jiang J Z. J Alloys Comp, 2007; 443: 109[9] Zhu Z W, Zhang H F, Ding B Z, Hu Z Q. Mater Sci Eng, 2008; 492: 221[10] Zhang J L, Wang Y M, Shek C H, Wang Q, Dong C. J Alloys Comp, 2010; 491: 513[11] Eckert J, Mattern N, Zinkevitch M, Seidel M. Mater Trans, 1998; 39: 623[12] Waniuk T A, Schroers J, Johnson W L. Phys Rev, 2003; 67B: 184203[13] Miracle D B, Sanders W S. Philos Mag, 2003; 83: 2409[14] Miracle D B. Nature Mater, 2004; 3: 697[15] Miracle D B. Acta Mater, 2006; 54: 4317[16] Dong C, Wang Q, Qiang J B, Wang Y M, Jiang N, Han G, Li Y H, Wu J, Xia J H. J Phys, 2007; 40D: 273[17] Wang Q, Qiang J B, Wang Y M, Xia J H, Zhang X F, Dong C. Intermetallics, 2004; 12: 1229[18] Xia J H, Qiang J B, Wang Y M, Wang Q, Dong C. Appl Phys Lett, 2006; 88: 101907[19] Wang Q, Zhu C L, Dong C, Qiang J B, Zhang W, Inoue A. J Phys: Confer Ser, 2008; 98: 12017[20] Yuan L, Pang C, Wang Y M, Wang Q, Dong C. Intermetallics, 2010; 18: 1800[21] Ma D, Tan H, Zhang Y, Li Y. Mater Trans, 2003; 44: 2007[22] Pearson W B. Crystal Chemistry and Physics of Metals and Alloys. New Jersey: Wiley, 1972: 1[23] Chen J X,Wang Q,Wang Y M, Qiang J B, Dong C. Philos Mag Lett, 2010; 90: 683[24] Lu Z P, Liu C T. J Mater Sci, 2004; 39: 3965[25] Yan M, Zou J, Shen J. Acta Mater, 2006; 54: 3627 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|