| THE SHAPE DISTORTION IN DRAWING PROCESS WITH TC1Mδ0.8 TITANIUM ALLOY SHEETS |
| 沈阳航空工业学院航空宇航工程学院 |
|
Cite this article:
. THE SHAPE DISTORTION IN DRAWING PROCESS WITH TC1Mδ0.8 TITANIUM ALLOY SHEETS. Acta Metall Sin, 2007, 43(8): 875-878 .
|
|
|
Abstract Titanium alloy sheets exhibit significant plastic anisotropy that can be attributed principally to the presence of texture. Such plastic anisotropy has pronounced effects on subsequent sheet metal forming and springback processes. In the present paper, cylindrical cup drawing processes with titanium alloy sheets TC1M of 0.8mm thickness were simulated using ADINA FEM software. Three sorts of shape distortions phenomena exhibit in the drawing cups fabricated in room temperature after elastic recovery process: the inner wall is no longer a cylindrical surface, the lip periphery becomes wavy and the thickness distribution becomes unhomogeneous. A series of cup drawing tests were conducted and reasonable agreement was obtained between the predicted and measured profiles.
|
|
Received: 09 November 2006
|
|
|
[1]Hu J G,Jonas J J,Ishikawa T.Mater Sci Eng,1998; A256:51 [2]Heiduschke K.Int J Solid Struct,1997;34:2339 [3]Yoon J W,Yang D Y,Chung K,Barlat F.Int J Plast, 1999;15:35 [4]Zhang L Y,Cui J Z,Cui X.Nat Technol Sci,2004;14: 133 (2004; 14:133) [5]Zhang L Y,Cui J Z,Zhang F Y.Mater Sci Technol,2005; 13:609 (张凌云,崔建忠.张风阳.材料科学与工艺.2005;13:609) [6]Zhang L Y,Cui J Z.J Northeastern Univ(Nat Sci),2005; 26:1164 (张凌云,崔建忠.东北大学学报(自然科学版),2005;26:1164) [7]Zhang L Y,Cui J Z.J Plast Eng,2005;12(5):21 (张凌云,崔建忠.塑性工程学报,2005;12(5):21) [8]Boubakar M L,Boisse P,Gelin J C.J Mater Process Tech- nol,1997; 65:143 [9]Kawka M,Olejnik L,Rosochowski A,Sunaga H,Maki- nouchi A.J Mater Process Technol,2001;109:283 [10]Kim Y,Son Y.J Mater Process Technol,2000;97:88 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|