Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (8): 875-878     DOI:
Research Articles Current Issue | Archive | Adv Search |
THE SHAPE DISTORTION IN DRAWING PROCESS WITH TC1Mδ0.8 TITANIUM ALLOY SHEETS
沈阳航空工业学院航空宇航工程学院
Cite this article: 

. THE SHAPE DISTORTION IN DRAWING PROCESS WITH TC1Mδ0.8 TITANIUM ALLOY SHEETS. Acta Metall Sin, 2007, 43(8): 875-878 .

Download:  PDF(488KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Titanium alloy sheets exhibit significant plastic anisotropy that can be attributed principally to the presence of texture. Such plastic anisotropy has pronounced effects on subsequent sheet metal forming and springback processes. In the present paper, cylindrical cup drawing processes with titanium alloy sheets TC1M of 0.8mm thickness were simulated using ADINA FEM software. Three sorts of shape distortions phenomena exhibit in the drawing cups fabricated in room temperature after elastic recovery process: the inner wall is no longer a cylindrical surface, the lip periphery becomes wavy and the thickness distribution becomes unhomogeneous. A series of cup drawing tests were conducted and reasonable agreement was obtained between the predicted and measured profiles.
Key words:  titanium alloy sheet      shape distortion      anisotropy      drawing      
Received:  09 November 2006     
ZTFLH:  TG113.26  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I8/875

[1]Hu J G,Jonas J J,Ishikawa T.Mater Sci Eng,1998; A256:51
[2]Heiduschke K.Int J Solid Struct,1997;34:2339
[3]Yoon J W,Yang D Y,Chung K,Barlat F.Int J Plast, 1999;15:35
[4]Zhang L Y,Cui J Z,Cui X.Nat Technol Sci,2004;14: 133 (2004; 14:133)
[5]Zhang L Y,Cui J Z,Zhang F Y.Mater Sci Technol,2005; 13:609 (张凌云,崔建忠.张风阳.材料科学与工艺.2005;13:609)
[6]Zhang L Y,Cui J Z.J Northeastern Univ(Nat Sci),2005; 26:1164 (张凌云,崔建忠.东北大学学报(自然科学版),2005;26:1164)
[7]Zhang L Y,Cui J Z.J Plast Eng,2005;12(5):21 (张凌云,崔建忠.塑性工程学报,2005;12(5):21)
[8]Boubakar M L,Boisse P,Gelin J C.J Mater Process Tech- nol,1997; 65:143
[9]Kawka M,Olejnik L,Rosochowski A,Sunaga H,Maki- nouchi A.J Mater Process Technol,2001;109:283
[10]Kim Y,Son Y.J Mater Process Technol,2000;97:88
[1] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[2] ZHANG Zixuan, YU Jinjiang, LIU Jinlai. Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432[J]. 金属学报, 2023, 59(12): 1559-1567.
[3] GE Jinguo, LU Zhao, HE Siliang, SUN Yan, YIN Shuo. Anisotropy in Microstructures and Mechanical Properties of 2Cr13 Alloy Produced by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(1): 157-168.
[4] GAO Yubi, DING Yutian, LI Haifeng, DONG Hongbiao, ZHANG Ruiyao, LI Jun, LUO Quanshun. Effect of Deformation Rate on the Elastic-Plastic Deformation Behavior of GH3625 Alloy[J]. 金属学报, 2022, 58(5): 695-708.
[5] LU Lei, ZHAO Huaizhi. Progress in Strengthening and Toughening Mechanisms of Heterogeneous Nanostructured Metals[J]. 金属学报, 2022, 58(11): 1360-1370.
[6] WANG Di, HUANG Jinhui, TAN Chaolin, YANG Yongqiang. Review on Effects of Cyclic Thermal Input on Microstructure and Property of Materials in Laser Additive Manufacturing[J]. 金属学报, 2022, 58(10): 1221-1235.
[7] BI Sheng, LI Zechen, SUN Haixia, SONG Baoyong, LIU Zhenyu, XIAO Bolv, MA Zongyi. Microstructure and Mechanical Properties of Carbon Nanotubes-Reinforced 7055Al Composites Fabricated by High-Energy Ball Milling and Powder Metallurgy Processing[J]. 金属学报, 2021, 57(1): 71-81.
[8] LIU Jinlai, YE Lihua, ZHOU Yizhou, LI Jinguo, SUN Xiaofeng. Anisotropy of Elasticity of a Ni Base Single Crystal Superalloy[J]. 金属学报, 2020, 56(6): 855-862.
[9] HU Bin,LI Shusuo,PEI Yanling,GONG Shengkai,XU Huibin. Influence of Small Misorientation from <111> on Creep Properties of a Ni-Based Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1204-1210.
[10] WANG Li,HE Yufeng,SHEN Jian,ZHENG Wei,LOU Langhong,ZHANG Jian. Effect of Secondary Orientation on Oxidation Anisotropy Around the Holes of Single Crystal Superalloy During Thermal Fatigue Tests[J]. 金属学报, 2019, 55(11): 1417-1426.
[11] HE Xianmei, TONG Liuniu, GAO Cheng, WANG Yichao. Effect of Nd Content on the Structure and Magnetic Properties of Si(111)/Cr/Nd-Co/Cr Thin Films Prepared by Magnetron Sputtering[J]. 金属学报, 2019, 55(10): 1349-1358.
[12] Xiaoqin MA, Qingfeng ZHAN, Jincai LI, Qingfang LIU, Baomin WANG, Runwei LI. Influence of Oblique Sputtering on Stripe Magnetic Domain Structure and Magnetic Anisotropy of CoFeB Thin Films[J]. 金属学报, 2018, 54(9): 1281-1288.
[13] Mingliang HUANG, Hongyu SUN. Interaction Between β-Sn Grain Orientation and Electromigration Behavior in Flip-Chip Lead-Free Solder Bumps[J]. 金属学报, 2018, 54(7): 1077-1086.
[14] Xudong LI, Pingli MAO, Yanyu LIU, Zheng LIU, Zhi WANG, Feng WANG. Anisotropy and Deformation Mechanisms ofAs-Extruded Mg-3Zn-1Y Magnesium AlloyUnder High Strain Rates[J]. 金属学报, 2018, 54(4): 557-565.
[15] Peibei JI, Lichu ZHOU, Xuefeng ZHOU, Feng FANG, Jianqing JIANG. Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire[J]. 金属学报, 2018, 54(4): 494-500.
No Suggested Reading articles found!