| Influence of Trace Ge on Oxidation of Liquid Tin in Atmosphere |
| GONG Guoliang; XIAN Aiping |
| Shenyang National Laborary for Materials Science; Institute of Metal Research; Chinese Academy of Sciences |
|
Cite this article:
GONG Guoliang; XIAN Aiping. Influence of Trace Ge on Oxidation of Liquid Tin in Atmosphere. Acta Metall Sin, 2007, 43(7): 759-763 .
|
|
|
|
|
Received: 22 November 2006
|
|
|
[1]Glazer J.Int Mater Rev,1995;40(2):65 [2]Kim K S,Huh S H,Suganuma K.Mater Sci Eng,2002; A333:106 [3]Zeng Q L,Wang Z G,Xian A P,Shang J K.J Electron Mater,2005;34(1):62 [4]Zhang L,Xian A P,Wang Z G,Han E H,Shang J K.Acts Metall Sin,2004;40:1151 (张黎,冼爱平,王中光,韩恩厚,尚建库.金属学报,2004; 40:1151) [5]Zeng K,Tu K N.Mater Sci Eng,2002;R38:55 [6]Li F,Liu C Z,Xian A P,Shang J K.Acts Metall Sin, 2004;40:815 (李飞,刘春中,冼爱平,尚建库,金属学报,2004;40:815) [7]Jiang B,Xian A P.Philos Mag Lett,2006;86:521 [8]Jiang B,Xian A P.Surf Technol,2006;35(4):1 (江波,冼爱平,表面技术,2006;35(4):1) [9]hang W D.Practical Surface Mounting Technology.Bei- jing:Publishing House of Electronics Industry,2002:136 (张文典.实用表面组装技术.北京,电子工业出版社,2002: 136) [10]Farrell T.Met Sci,1976;10:87 [11]Xian A P,Guo J J,Shang J K.Chin Pat,No. ZL03133847.X,2005 (冼爱平,郭建军,尚建库.中国发明专利,ZL03133847.X, 2005) [12]http://srdata.nist.gov/XPS/,06/06/2000 [13]Huang H Z.Analysis of Nano-materials,Beijing:Chem- ical Industry Press,2003:107 (黄惠忠.纳米材料分析.北京:化学工业出版社,2003:107) [14]Kleppa O J,King R C.Acts Metall,1962;10:1183 [15]Beardmore P,Howlett B W,Lichter B D,Bever M B. Trans AIME,1966;236:102 [16]Thurmond C D.J Phys Chem,1953;57:827 [17]Liang Y J,Che Y C.Thermodynamic Handbook of In- organic Compounds.Shenyan:Northeastern University Press,1993:11 (梁英教,车荫昌.无机物热力学数据手册.沈阳:东北大学出版社,1993:11) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|