Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (4): 353-357     DOI:
Research Articles Current Issue | Archive | Adv Search |
Multi-stage reversible transformation types and their evolving processes of Ti-Ni base shape memory alloys
Zhi-rong HE
陕西理工学院材料科学与工程学院
Cite this article: 

Zhi-rong HE. Multi-stage reversible transformation types and their evolving processes of Ti-Ni base shape memory alloys. Acta Metall Sin, 2007, 43(4): 353-357 .

Download:  PDF(469KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The multi-stage reversible transformation types and their evolving processes of Ti-Ni base shape memory alloys (SMAs) under various heat treatment processes have been investigated by differential scanning calorimetry (DSC) with partial thermal cycling method. The Ti-Ni base SMAs show many kinds of multi-stage reversible transformation types after various heat treatment processes. If expresses transformation type with peak numbers of cooling transformation / peak numbers of heating transformation on DSC curves, the 2/1, 2/2 and 3/2 type transformations occur upon cooling and heating in 350-550℃ annealed alloys; the 1/1 type transformation occurs when the annealed temperature is high than 600℃; the 3/2 and 3/3 type transformations occur in 300℃ aged alloys; the 2/2 type transformation occurs in 400℃ aged alloys; the 2/1 type transformation occurs in 500℃ aged alloys. The multi-stage reversible transformation is a gradually changing process. When partial thermal cycling was carried out within the temperature range of cooling transformation, the transformation temperature of reverse transformation decreases with decreasing thermal cycling start temperature.
Key words:  Ti-Ni alloy      shape memory alloy      superelasticity alloy      transformation      
Received:  01 August 2006     
ZTFLH:  TG113.25  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I4/353

[1]Otsuka K,Ren X.Mater Sci Eng,1999;A273-275:89
[2]Favier D,Liu Y,McCormick P G.Scr Metall Mater,1993; 28:669
[3]Khalil A J,Ren X,Eggeler G.Acta Mater,2002;50:793
[4]Kim J I,Liu Y,Miyazaki S.Acta Mater,2004;52:487
[5]He Z R,Zhou J E,Miyazaki S.Acta Metall Sin,2003;39: 617 (贺志荣,周敬恩,宫崎修一.金属学报,2003;39:617)
[6]He Z R,Zhang Y H,Wang Y S,Zhou J E.Acta Metall Sin,2004;40:46 (贺志荣,张永宏,王永善,周敬恩.金属学报,2004;40:46)
[7]He Z R,Wang F,Zhou J E.Heat Treat Met,2006;31(9): 18 (贺志荣,王芳,周敬恩.金属热处理,2006;31(9):18)
[8]Fukuda T,Saburi T,Chihara T,Tsuzuki Y.Mater Trans JIM,1995;36:1244
[9]Liu Y,Kim J I,Miyazaki S.Philos Mag,2004;84A:2083
[10]Chrobak D,Stroz D.Scr Mater,2005;52:757
[11]Kim J I,Miyazaki S.Mater Sci Forum,2002;394-395: 225
[12]Ziolkowski A,Raniecki B,Miyazaki S.Mater Sci Eng, 2004;A378:86
[13]Kim J I,Miyazaki S.Acta Mater,2005;53:4545
[14]Todoroki T,Tamura H.Trans JIM,1987;28(2):83
[15]He Z R,Miyazaki S.Acta Metall Sin,1996;32:251 (贺志荣,宫崎修一.金属学报,1996;32:251)
[16]Nishida M,Wayman C M,Honma T.Metall Trans,1986; 17A:1505
[17]He Z R.Funct Mater,1998;29:157 (贺志荣.功能材料,1998;29:157)6
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[4] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[5] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[6] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[7] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[8] YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi. Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 55-74.
[9] CHEN Fei, QIU Pengcheng, LIU Yang, SUN Bingbing, ZHAO Haisheng, SHEN Qiang. Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition[J]. 金属学报, 2023, 59(1): 180-190.
[10] ZHANG Xin, CUI Bo, SUN Bin, ZHAO Xu, ZHANG Xin, LIU Qingsuo, DONG Zhizhong. Effect of Y Element on the Properties of Cu-Al-Ni High Temperature Shape Memory Alloy[J]. 金属学报, 2022, 58(8): 1065-1071.
[11] SUN Yi, ZHENG Qinyuan, HU Baojia, WANG Ping, ZHENG Chengwu, LI Dianzhong. Mechanism of Dynamic Strain-Induced Ferrite Transformation in a 3Mn-0.2C Medium Mn Steel[J]. 金属学报, 2022, 58(5): 649-659.
[12] LI Wei, JIA Xingqi, JIN Xuejun. Research Progress of Microstructure Control and Strengthening Mechanism of QPT Process Advanced Steel with High Strength and Toughness[J]. 金属学报, 2022, 58(4): 444-456.
[13] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[14] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[15] YANG Ping, WANG Jinhua, MA Dandan, PANG Shufang, CUI Feng'e. Influences of Composition on the Transformation-Controlled {100} Textures in High Silicon Electrical Steels Prepared by Mn-Removal Vacuum Annealing[J]. 金属学报, 2022, 58(10): 1261-1270.
No Suggested Reading articles found!