| Multi-stage reversible transformation types and their evolving processes of Ti-Ni base shape memory alloys |
| Zhi-rong HE |
| 陕西理工学院材料科学与工程学院 |
|
Cite this article:
Zhi-rong HE. Multi-stage reversible transformation types and their evolving processes of Ti-Ni base shape memory alloys. Acta Metall Sin, 2007, 43(4): 353-357 .
|
|
|
Abstract The multi-stage reversible transformation types and their evolving processes of Ti-Ni base shape memory alloys (SMAs) under various heat treatment processes have been investigated by differential scanning calorimetry (DSC) with partial thermal cycling method. The Ti-Ni base SMAs show many kinds of multi-stage reversible transformation types after various heat treatment processes. If expresses transformation type with peak numbers of cooling transformation / peak numbers of heating transformation on DSC curves, the 2/1, 2/2 and 3/2 type transformations occur upon cooling and heating in 350-550℃ annealed alloys; the 1/1 type transformation occurs when the annealed temperature is high than 600℃; the 3/2 and 3/3 type transformations occur in 300℃ aged alloys; the 2/2 type transformation occurs in 400℃ aged alloys; the 2/1 type transformation occurs in 500℃ aged alloys. The multi-stage reversible transformation is a gradually changing process. When partial thermal cycling was carried out within the temperature range of cooling transformation, the transformation temperature of reverse transformation decreases with decreasing thermal cycling start temperature.
|
|
Received: 01 August 2006
|
|
|
[1]Otsuka K,Ren X.Mater Sci Eng,1999;A273-275:89 [2]Favier D,Liu Y,McCormick P G.Scr Metall Mater,1993; 28:669 [3]Khalil A J,Ren X,Eggeler G.Acta Mater,2002;50:793 [4]Kim J I,Liu Y,Miyazaki S.Acta Mater,2004;52:487 [5]He Z R,Zhou J E,Miyazaki S.Acta Metall Sin,2003;39: 617 (贺志荣,周敬恩,宫崎修一.金属学报,2003;39:617) [6]He Z R,Zhang Y H,Wang Y S,Zhou J E.Acta Metall Sin,2004;40:46 (贺志荣,张永宏,王永善,周敬恩.金属学报,2004;40:46) [7]He Z R,Wang F,Zhou J E.Heat Treat Met,2006;31(9): 18 (贺志荣,王芳,周敬恩.金属热处理,2006;31(9):18) [8]Fukuda T,Saburi T,Chihara T,Tsuzuki Y.Mater Trans JIM,1995;36:1244 [9]Liu Y,Kim J I,Miyazaki S.Philos Mag,2004;84A:2083 [10]Chrobak D,Stroz D.Scr Mater,2005;52:757 [11]Kim J I,Miyazaki S.Mater Sci Forum,2002;394-395: 225 [12]Ziolkowski A,Raniecki B,Miyazaki S.Mater Sci Eng, 2004;A378:86 [13]Kim J I,Miyazaki S.Acta Mater,2005;53:4545 [14]Todoroki T,Tamura H.Trans JIM,1987;28(2):83 [15]He Z R,Miyazaki S.Acta Metall Sin,1996;32:251 (贺志荣,宫崎修一.金属学报,1996;32:251) [16]Nishida M,Wayman C M,Honma T.Metall Trans,1986; 17A:1505 [17]He Z R.Funct Mater,1998;29:157 (贺志荣.功能材料,1998;29:157)6 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|