Abstract The MgB2 bulks were prepared using the spherical magnesium powder (denoted as Q-Mg) and scrapping magnesium powder (denoted as X-Mg) as raw materials. The two kinds of magnesium powder were mixed with amorphous boron powder with a nominal stoichiometry of MgB2, then pressed into pellets under a pressure of 10MPa. The pellets were sintered at 650℃,700℃,750℃ and 800℃ respectively. The X-ray diffraction analysis results for the sintered samples show that the phase formation rate of Q-Mg series samples is lower than that of X-Mg series samples. The differential scanning calorimetry (DSC) results indicate that the solid-solid reaction , Mg melting and liqiud-solid reaction during the temperature increasing occur in turn at 527.1℃,650.7℃ and 660.8℃ for the X-Mg series samples, but for the Q-Mg series samples, the Mg melting and liqiud-solid reaction occur in turn at 640.9℃ and 712.3℃.
|
Received: 10 August 2006
|
|
[1]Buzea C,Yamashita T.Supercond Sci Technol,2001;14R: 115 [2]Naito M.Ueda K.Supercond Sci Technol,2004;17R:1 [3]Chen C P,Zhou Z J,Li X G,Xu J,Wang Y H.Gao Z X, Feng Q R.Solid State Commun,2004;131:275 [4]Feng Q R,Chen C P,Xu J,Kong L W.Chen X,Wang Y Z,Zhang Y,Gao Z X.Physica,2004;411C:41 [5]Feng Q R,Chen X,Wang Y H,Wang X,Xiong G C,Gao Z X.Physica,2003;386C:653 [6]Yan S C,Yan G.Liu C F,Lu Y F,Zhou L.J Alloys Compd,in press [7]Dong C.J Appl Crystallogr,1999;32:838 [8]Nagamatsu J,Nakagawa N,Zenitani Y,Akimitsu J.Na- ture,2001;410:63 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|