Export:  BibTeX | EndNote (RIS)      
Abstract  Electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization procedures were used to investigate the pitting corrosion behaviors in the simulated body fluid of AISI 316L stainless steel treated by high current pulsed electron beam (HCPEB). The results showed that the corrosion resistance of 316L samples was significantly improved after HCPEB treatment, which was demonstrated by the increased polarization resistance (Rp) and decreased interface capacitance. The samples after 5 pulses are prone to pitting due to the existence of remnant MnS inclusions or holes in the crater centers. Comparatively, the sample after 20 pulses of HCPEB treatment shows the best corrosion resistance. Its corrosion current density has been decreased to 1/15 of the initial samples, which can be attributed to the selective surface purification effect and removal of physical damages with increasing number of pulses.
Key words:  High current pulsed electron beam      Electrochemical impedance spectroscopy (EIS)      Polarization curves      C     
Received:  04 April 2006     
ZTFLH:  O482.2  
  TG172  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V42/I1/71

[1] Wranglen G.Corros Sci,1974;14:331
[2] Eklund G S.J Electrochem Soc,1974;121:467
[3] Ryan M P,Williams D E,Chater R J,Hutton B M, McPhail D S.Nature,2002;415:770
[4] Gurappa I.Mater Charact,2002;49:73
[5] Newman R C.Nature,2002;415:743
[6] Yue T M,Yu J K,Man H C.Surf Coat Technol,2001; 137:65
[7] Lo K H,Cheng F T,Kwok C T,Man H C.Surf Coat Technol,2003;165:258
[8] Meinert K,wolf G K.Surf Coat Technol,1998;98:l148
[9] Liu C L,Lin G Q,Yang D Z,Qi M.Surf Coat Technol, 2006;200:4011
[10] Proskurovsky D I,Rotshtein V P,Ozur G E,Markov A B,Nazarov D S.J Vac Sci Technol,1998;16A:2480
[11] Dong C,Wu A M,Hao S Z,Zou J X,Liu Z M,Zhong P, Zhang A M,Xu T,Chen J M,Xu J,Liu Q,Zhou Z R.Surf Coat Technol,2003;163—164:620
[12] Zhang K M,Yang D Z,Zou J X,Dong C.Acta Metall Sin,2007;43:64 (张可敏,杨大智,邹建新,董闯.金属学报,2007;43:64)
[13] Norlin A,Pan J,Leygraf C.Biomol Eng,2002;19:67
[14] Li M C,Luo S Z,Zeng C L,Shen J N,Lin H C,Cao C N.Corros Sci,2004;46:1369
[15] Williams D E,Mohiuddin T F,Zhu Y Y.J Electrochem Soc,1998;145:2664
[16] Cao C N.The Principle of Corrosion Electrochemistry.2nd Edition,Beijing:Chemical Industry Press,2004:262 (曹楚南.腐蚀电化学原理.第2版,北京:化学工业出版社, 2004:262)
[17] Liu C,Leyland A,Lyon S,Matthews A.Surf Coat Tech—nol, 1995;76—77:615
[18] Cao C N,Zhang J Q.An Introduction to Electrochemical Impedance Spectroscopy.Beijing:Science Press,2002:86 (曹楚南,张鉴清.电化学阻抗谱导论.北京:科学出版社,2002: 86)Y
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[5] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[6] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[7] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[8] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[9] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[10] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[11] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[12] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[13] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[14] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[15] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
No Suggested Reading articles found!