| ATMOSPHERIC CORROSION OF PURE COPPER DURING INITIAL EXPOSURE STAGE IN SHENYANG ATMOSPHERE |
| Bai-Gang AN;; |
| 中科院金属研究所;鞍山科技大学 |
|
Cite this article:
Bai-Gang AN. ATMOSPHERIC CORROSION OF PURE COPPER DURING INITIAL EXPOSURE STAGE IN SHENYANG ATMOSPHERE. Acta Metall Sin, 2007, 42(1): 77-81 .
|
|
|
Abstract Atmospheric corrosion of pure copper under sheltered and unsheltered exposure condition during 1 year period in Shenyang atmosphere was studied. Atmospheric corrosion rate of pure copper, composition and protectiveness of corrosion product of pure copper was different under the different exposure conditions. Corrosion rate of pure copper exposed to unsheltered condition was higher than that exposed to shelter. Especially during rainy season, runoff by rain made the copper experience the longer wet time, and thus accelerated corrosion of pure copper evidently. The main corrosion product of copper under the different exposure conditions was Cu2O, there were still Cu4SO4(OH)6.H2O and (Cu4SO4(OH)6) under shelter. However, effects of runoff and dissolution by rain on corrosion products made a low formation process of Cu4SO4(OH)6.H2O, only Cu2O was identified after 6 months exposure under unsheltered exposure condition, Cu4SO4(OH)6.H2O was not found until 12 months exposure period. The thicker and compact corrosion product film had been formed under the unsheltered exposure, which could inhibit the cathodic reaction of copper corrosion effectively, and thus had the better protectiveness.
|
|
Received: 27 April 2006
|
|
|
[1] Mendoza A R, Corvo F.Corros Sci, 2000:12:1123 [2] Graedel T E.Corros Sci, 1987:27:72l [3] Mattsson E.Mater Perform, 1982; 2l:9 [4] Leygraf C,Graedel T.Atmospheric Corrosion.New York: John Wiley&Sons, Inc, 2000:140 [5] Rosales B,Vera R,Moriena G.Corros Sci,1999;41:625 [6] Vilche J R,Varela F E,Codaro E N,Rosales B M, Moriena G, Fernandez A.Corros Sci, 1997; 39:655 [7] Mendoza A R,Corvo F,Gomez A,Gomez J.Corros Sci, 2004; 46:1189 [8] Odnevall I,Leygraf C.Corros Sci,1997;36:2039 [9] Lobing R E, Frankenthal R P,Siconolfi D J,Sinclair J D, Stratmann M.J Electrochem Soc, 1981; 128:275 [10] Eriksson P, Johansson L G, Strandberg H. J Electrochem Soc, 1993; 140:53 [11] Veleva L,Quintana P,Ramanauskas R,Pomes R, Mal—donado L.Electochim Acta, 1996; 41:1641 [12] Nairn J,Fitzgerald K,Aterns A.In:Apsa A, ed., Proc Australasian Corrosion Association Conf, Melbourne: Australasian Corrosion Association Inc, 1994:168 [13] Zakipour S,Tidblad J,Leygraf C.J Electrochem Soc, 1995;142:757 [14] Tidblad J,Leygraf C.J Electrochem Soc,1995;142:749 [15] Nairn J, Fitzgerald K P, Atrens A.In:MacLeod I I),St Pennec L,Robbiola L,eds., Metal 95,London:James&James (Science Publisher) Ltd,1995:86 [16] Feliu S, Morcillo M,Feliu S Jr.Corros Sci,1993;34:403 [17] Feliu S, Morcillo M,Feliu S Jr.Corros Sci,1993; 34: 415 [18] Arroyave C,Lopez F A,Morcillo M.Corros Sci,1995;37: 1751 [19] Kucera V,Tidblad J,Leygraf C,Henriksen J,Kreislova K, AshaIl G, Stckle B.In:Corrosion Prevention Centre of Australasia Inc,ed., 13th Int Corrosion Conf, Melbourne, Australasian Corrosion Association Inc, 1996:193 [20] Nassau K,Gallagher P K,Miller A E,Graedel T.Corros Sci,1987;27:669 [21] Odnevall I, Leygraf C.J Electrochem Soc, 1995; 142:3682 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|