IN SITU STUDY OF MARTENSITE TRANSFORMATION , PLASTIC DEFORMATION AND CRACK NUCLEATION FOR NI2MNGA FERROMAGNETIC SHAPE MEMORY ALLOY
;;;;
北京科技大学
Cite this article:
. IN SITU STUDY OF MARTENSITE TRANSFORMATION , PLASTIC DEFORMATION AND CRACK NUCLEATION FOR NI2MNGA FERROMAGNETIC SHAPE MEMORY ALLOY. Acta Metall Sin, 2006, 42(8): 810-814 .
Abstract The interrelationship of crack nucleation to martensite transformation and plastic deformation has been studied in situ using a differential interference constrast (DIC) microscopy for a notched sample of Ni2MnGa ferromagnetic shape memory alloy . The result showed that martensites form firstly during loading and there was a plastic zone when stress concentration ahead of a crack is large enough . Microcrack initiated preferentially along the interface of martensite , but also initiated in the plastic zone . With increasing the load , microcracks initiated discontinuously along the martensites and connected through shear microcracks in the ligaments , resulting in a resistance curve increase behavior .
[1]Sozinov A,Likhachev A A,Lanska N,Ullakko K.Appl Phys Lett,2002;80:1746 [2]Murray S J,O'Handley R C,Allen S M.J Appl Phys,2001;89:1295 [3]Chernenko V A,L'vov V,Pons J,Cesari E.J Appl Phys,2003;93:2394 [4]Deng L F,Li Y,Jiang C B,Xu H B.Acta Metall Sin,2004;40:1290 (邓丽芬,李岩,蒋成保,徐惠彬.金属学报,2004;40:1290) [5]Chu W Y,Thompson A W.Metall Trans,1992;23A:1299 [6]Lu Y H,Zhang Y G,Qiao L J,Chu W Y.Intermetallics,2000;8:1443 [7]Miyazaki S,Totsuka K.ISIJ Int,1989;29:353 [8]Lu Y H,Qiao L J,Chu W Y.Sci China,2001;44A:932 [9]Lu Y H,Qiao L J,Chu W Y.Fatigue Fract Eng Mater Struct,2002;25:509 [10]Chu W Y,Qiao L J,Chen Q Z,Gao K W.Fracture and Environment Fracture.Beijing:Science Press,2000:5 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京:科学出版社,2000:5)P