| Effects of Twin Size on the Dislocation Configuration During Cyclic Deformation of Polycrystalline Twin Copper |
| GUO Xiaolong; LU Lei; LI Shouxin |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
GUO Xiaolong; LU Lei; LI Shouxin. Effects of Twin Size on the Dislocation Configuration During Cyclic Deformation of Polycrystalline Twin Copper. Acta Metall Sin, 2005, 41(1): 23-.
|
|
|
Abstract Symmetrical push-pull fatigue tests were conducted on as--electrodeposited
polycrystalline twin copper. Different dislocation configurations were
formed in twins with different
widths. When the twin width $W_{\rm t} >1~ \mu$m, loop patches and
walls were found in twins, the same as that in single
crystal; when 1um>W>200 nm,
ladder--like structures formed in twin, which like persistent slip
bands (PSBs); when 200 nm>W>20 nm, only some
dislocation fragments were found; when W<20 nm,
no stable crystal dislocation segments exist in the twin.
|
|
Received: 19 February 2004
|
|
|
[1] Laird C, Charsley P, Mugurabi H. Mater Sci Eng. 1986;81: 433 [2] Jia W P, Li S X, Wang Z G, Li X W, Li G Y. Acta Mater,1999; 47: 2165 [3] Feltner C E, Laird C. Aata Metall, 1967; 15:1633 [4] Vinogradov A, Kaneko Y, Kitagawa K, Hashimoto S, Stol-yarov V, Valiev R. Scr Mater, 1997; 36: 1345 [5] Witney A B, Sanders P G, Weertman J R, Eastman J A.Scr Metall Mater, 1995; 33: 2025 [6] Lu L, Shen Y F, Chen X H, Qian L H, Lu K. Science,2004; 16: 422 [7] Guo X L, Shen Y F, Lu L, Li S X. Aata Metall Sin, 2004,40: 337(郭小龙,申勇峰,卢磊,李守新.金属学报,2004;40:337) [8] Wu S D, Wang Z G, Jiang C B, Li G Y, Alexandrov I V,Valiev R Z. Scr Mater, 2003; 48: 1605 [9] Kawazoe H, Yoshida M, Basinski Z S, Niewczas M. ScrMater. 1999; 40: 639 [10] Konopka K, Mizera J. Wyrzykowski J W. J Mater ProcTechnol, 2000; 99: 255 [11] Neumann P. Fatigue. In: Cahn R W, Haasen P eds, Physical Metallurgy, Amsterdam: Elsevier Science, 1983: 1554 |