Composition Optimization of the Zr-Al-Co Bulk Metallic Glasses
ZHANG Xinfang; WANG Yingmin; PENG Min; WANG Qing; LI Dejun; DONG Chuang
State Key Laboratory of Materials Modification & Department of Materials Engineering; Dalian University of Technology; Dalian 116024
Cite this article: 

ZHANG Xinfang; WANG Yingmin; PENG Min; WANG Qing; LI Dejun; DONG Chuang. Composition Optimization of the Zr-Al-Co Bulk Metallic Glasses. Acta Metall Sin, 2004, 40(10): 1103-1103 .

Download:  PDF(5950KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Composition optimization for locating the composition zone with the largest glass forming ability (GFA) in the Zr-Al-Co system is attempted. The criteria that we have developed are respectively related to the conduction electron concentration, termed the e/a-constant criterion, and to the special cluster structure, termed the e/a-variant criterion. For this system, the two criteria are incarnated into the e/a-constant line with constant e/a=1.5 and the (Zr9Co4-Al and (Zr78.5Co21.5)-Al e/a--variant lines. Bulk metallic glasses (BMGs) are obtained by suction casting for alloys on the (Al50Co50-Ale/a$--constant line and Zr9Co4-Al e/a--variant line. On the (Zr9Co4-Al e/a-variant line, the thermal stability and glass forming ability of BMGs are increased with increasing e/a ratio. The Zr53Al23.5Co23.5 BMG with the largest thermal stability and GFA locates in the intersecting point of the two lines, its characteristic thermodynamic indices are Tg=783 K, Tx=849K, Tg/Tm=0.637, Tg}/Tl=0.590.
Key words:  bulk metallic glass      transition metal      
Received:  17 November 2003     
ZTFLH:  TG139  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I10/1103

[1] LI Ning, HUANG Xin. Recent Advances on 3D Printed Bulk Metallic Glasses[J]. 金属学报, 2021, 57(4): 529-541.
[2] Yanchun ZHAO, Hao SUN, Chunling LI, Jianlong JIANG, Ruipeng MAO, Shengzhong KOU, Chunyan LI. High Temperature Deformation Behavior of High Strength and Toughness Ti-Ni Base Bulk Metallic Glass Composites[J]. 金属学报, 2018, 54(12): 1818-1824.
[3] Yuanyuan ZHANG,Xin LIN,Lei WEI,Yongming REN. Crystallization Behavior of Laser Solid Forming of Annealed Zr55Cu30Al10Ni5 Powder[J]. 金属学报, 2017, 53(7): 824-832.
[4] Yufeng ZHENG,Yuanhao WU. Revolutionizing Metallic Biomaterials[J]. 金属学报, 2017, 53(3): 257-297.
[5] YANG Bin, LI Xin, LUO Wendong, LI Yuxiang. EFFECT OF MINOR Sn AND Nb ADDITIONS ON THE THERMAL STABILITY AND COMPRESSIVE PLASTICITY OF Zr-Cu-Fe-Al BULK METALLIC GLASS[J]. 金属学报, 2015, 51(4): 465-472.
[6] Yong SHEN,Jian XU. PREPARATION AND MECHANICAL PROPERTIES OF Zr46.9Cu45.5Al5.6Y2.0 IN SITU BMG COMPOSITES WITH B2-CuZr PHASE[J]. 金属学报, 2015, 51(11): 1407-1415.
[7] MA Guangcai, FU Huameng, WANG Zheng, XU Qingliang, ZHANG Haifeng. STUDY ON FABRICATION AND PROPERTIES OF 304 STAINLESS STEEL CAPILLARY TUBES/Zr53.5Cu26.5Ni5Al12Ag3 BULK METALLIC GLASS COMPOSITES[J]. 金属学报, 2014, 50(9): 1087-1094.
[8] YANG Gaolin, LIN Xin, HU Qiao, SONG Menghua, WANG Zhitai, HUANG Weidong. EFFECT OF SPECIMEN TEMPERATURE ON CRYSTALLIZATION DURING LASER REMELTITNG Zr55Cu30Al10Ni5 BULK METALLIC GLASS[J]. 金属学报, 2013, 49(8): 925-931.
[9] YANG Gaolin, LIN Xin, HU Qiao, ZHANG Ying, WANG Zhitai, LI Peng, HUANG Weidong. CRYSTALLIZATION BEHAVIOR OF ANNEALED Zr55Cu30Al10Ni5 BULK METALLIC GLASS  DURING PULSED LASER REMELTING[J]. 金属学报, 2013, 49(6): 649-657.
[10] MA Guofeng, HE Chunlin, LI Zhengkun, ZHANG Bo, LI Hong, ZHANG Haifeng, HU Zhuangqi. EFFECTS OF THE ADDITION OF Ti OR Al ON THE WETTING BEHAVIORS AND INTERFACIALCHARACTERISTICS OF Zr50Cu50 BULK METALLIC GLASS/W SUBSTRATE[J]. 金属学报, 2013, 29(4): 495-500.
[11] HU Qiang ZENG Xierong QIAN Haixia XIE Shenghui SHENG Hongchao. CORRELATION BETWEEN THE GLASS-FORMING ABILITY AND CHARACTERISTIC FREE VOLUMES OF THE IRON BASE BULK METALLIC GLASSES[J]. 金属学报, 2012, 48(11): 1329-1334.
[12] YUAN Liang QIANG Jianbing PANG Chang WANG Yinmin WANG Qing DONG Chuang. COMPOSITION DESIGN OF Ni–Nb–(Zr, Ta, Ag) TERNARY BULK METALLIC GLASSES BASED ON CLUSTER FORMULA OF Ni–Nb EUTECTIC[J]. 金属学报, 2011, 47(8): 1003-1008.
[13] LIU Tong ZHU Yarong ZHANG Tongwen ZHANG Tao. EFFECTS OF PREANNEALING UNDER PRESSURE ON THE CRYSTALLIZATION BEHAVIOR AND THERMAL STABILITY OF Gd36La20Al24Co20 BULK
METALLIC GLASS
[J]. 金属学报, 2011, 47(4): 502-506.
[14] ZHANG Jianting QIAO Junwei ZHANG Yong. SYNTHESIS OF PLASTIC LIGHTWEIGHT Ti-BASED METALLIC-GLASS-MATRIX COMPOSITES BY BRIDGMAN SOLIDIFICATION[J]. 金属学报, 2011, 47(2): 236-240.
[15] HUANG Caiyun CHEN Qi LIU Lin. FRICTION AND WEAR PROPERTIES OF Ni–FREE Zr–BASED BULK METALLIC GLASSES IN SIMULATED BODY FLUID[J]. 金属学报, 2010, 46(6): 681-686.
No Suggested Reading articles found!