| INFLUENCE OF ANNEALING AND SUBSTITUTION ELEMENTS ON DAMPING CAPACITY AND STRENGTH OF Fe-Cr-Al BASED ALLOYS |
| LIN Renrong; LIU Fang; CAO Mingzhou; YANG Rui |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
LIN Renrong; LIU Fang; CAO Mingzhou; YANG Rui. INFLUENCE OF ANNEALING AND SUBSTITUTION ELEMENTS ON DAMPING CAPACITY AND STRENGTH OF Fe-Cr-Al BASED ALLOYS. Acta Metall Sin, 2005, 41(9): 958-962 .
|
|
|
Abstract The damping capacities and strengths of six alloys, Fe-13Cr-6Al, Fe-11Cr-2 (Mo, Mn or Nb)-6Al, Fe-13Cr-5.5Al-0.5Cu, and Fe-13Cr-5Al-1Cu (atomic fraction, %) were measured. The effects of annealing temperature, cooling
method and substitution elements on the above two properties were discussed by optical microscope observation and internal stresses analysis. The following results were obtained: (1) The damping capacity of Fe-13Cr-6Al based alloys increases with increasing annealing temperature while strength decreases. (2) The damping capacity of
furnace cooling alloys is higher than water quenched alloys while the strength of the former is lower than the latter. (3) The substitution of 0.5\%Cu decreases the interaction between dislocations and solute atoms while increases the elastic interaction between alloying atoms and base atoms, which improves both damping capacity and strength of the alloy.
|
|
Received: 28 March 2005
|
|
|
[1] Zheng W J, Lu J S, Zhang J, Wu B R. J Iron Steel Res, 1997; 9(1): 17 (郑文杰,陆军生,张杰,吴宝榕.钢铁研究学报,1997;9(1): 17) [2] Zhang J X. Dev Appl Mater, 1991; 6(2): 2 (张俊旭.材料开发与应用,1991;6(2):2) [3] Azcoitia C, Karimi A. J Alloys Compd, 2000; 310: 160 [4] Karimi A, Azcoitia C, Degauque J. J Magn Magn Mater, 2000; 215-216: 601 [5] Cochardt A W. J Appl Phys, 1954; 25: 670 [6] Lin R R, Cao M Z, Yang R. Mater Sci Forum, 2005; 475- 479: 261 [7] Lavernia E J, Perez R J, Zhang J. Metall Mater Trans, 1995; 26A: 2803 [8] Smith G W, Birchak J R. J Appl Phys,1968;39: 2311 [9] Smith G W, Birchak J R. J Appl Phys,1969;40:5174 [10] Zener C. Elasticity and Anelasticity of Metals.Chicago: University of Chicago Press,1948: 64 [11] Wang W G, Mo D X,Zhao T T, Zhang Y.J Shandong Inst Technol, 2002; 16(1): 23 (王卫国,莫德秀,赵婷婷,张勇.山东工程学院学报,2002; 16(1):23) [12] Wang W G, Liu S G, Xue B. J Shandong Inst Technol, 2002; 16(4): 41 (王卫国,刘曙光,薛冰.山东工程学院学报,2002;16(4): 41) [13] Ha K F. Microscopic Theory of Metallic Mechanical Properties. Beijing: Science Press, 1983: 350 (哈宽富.金属力学性质的微观理论.北京:科学出版社,1983: 350) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|