| EXPERIMENTAL STUDY ON NON-PROPORTIONALLY MULTIAXIAL TIME-DEPENDENT CYCLIC DEFORMATIONS OF SS304 STAINLESS STEEL AT HIGH TEMPERATURE |
| KAN Qianhua; KANG Guozheng; ZHANG Juan; LIU Yujie |
| Department of Applied Mechanics and Engineering; Southwest Jiaotong University; Chengdu 610031 |
|
Cite this article:
KAN Qianhua; KANG Guozheng; ZHANG Juan; LIU Yujie. EXPERIMENTAL STUDY ON NON-PROPORTIONALLY MULTIAXIAL TIME-DEPENDENT CYCLIC DEFORMATIONS OF SS304 STAINLESS STEEL AT HIGH TEMPERATURE. Acta Metall Sin, 2005, 41(9): 963-968 .
|
|
|
Abstract The time-dependent strain cyclic characteristics and ratcheting behavior of SS304 stainless steel were studied
by experiments under non-proportionally multiaxial cyclic loading and at 973 K. The effects of loading path, straining/stressing rate and holding-time at peak/valley of each cycle on cyclic softening/hardening behavior and ratcheting were discussed. It is shown from experimental results that the cyclic
softening/hardening behavior and ratcheting of the material are characterized by apparent time-dependence, i.e., the cyclic deformation behaviors depend not only greatly on
loading rate, but also apparently on holding-time, besides, the ratcheting behavior of the material also presents a great dependence on loading path at high temperature. Some results
obtained are helpful to construct a time-dependent constitutive model of ratcheting.
|
|
Received: 10 January 2005
|
|
|
[1] McDowell D L. ASMS J Appl Mech.1987;54:323 [2] Abdel-Karim M, Ohno N. Int. J Plast,2000;16:225 [3] Benallal A, Marquis D. ASME J Eng Mater Technol, 1987; 109: 326 [4] Kobayashi M, Ohno N, Igari T. Int. J Plast,1998;11:397 [5] Chaboche J L, Nouailhas D. ASME J Eng Mater Technol, 1989; 111: 384 [6] McDoewll D L. ASME J Appl Mech,1985;52:298 [7] Ohno N, Wang J D. Int J Plant,1993;9:375 [8] Yaguchi M, Takahashi Y. JMSE Int J, 1999; 42A(1): 1 [9] Jiang Y, Sehitogu H. Int J Plast, 1994; 10:579 [10] Kang G Z, Gao Q, Yang X J. Int. J Non-Linear Mech, 2004; 39: 843 [11] Kang G Z, Gao Q, Yang X J. Mech Mater,2002;34:521 [12] Kang G Z, Gao Q, Cai L X. Ada Metall Sin, 2000;36: 497 (康国政,高庆,蔡力勋.金属学报, 2000;36:497) [13] Kang G Z, Gao Q, Yang X J, Sun Y F. Acta Mech Sin, 2001; 33: 692 (康国政,高庆,杨显杰,孙亚芳.力学学报,2001;33:692) [14] Chen X, Jiao R. Int J Plast, 2004; 20: 871 [15] Chen X, Jiao R, Kim K S. Int J Plast,2005;21:161 [16] Kang G Z, Sun Y F, Zhang J, Kan Q H. Acta Metall Sin, 2005; 41: 277 (康国政,孙亚芳,张娟,阚前华.金属学报,2005;41:277) [17] Kang G Z, Ohno N, Nebu, A. Int J Plast, 2003;19:1801 [18] Kang G Z , Gao Q. Mech Mater, 2004; 36: 299 [19] Kang G Z, Gao Q. Mech Mater,2002;34:809 [20] Kang G Z, Gao Q, Cai L X. J Mater Sci Technol,2002; 18: 13 [21] Kang G Z, Gao Q. Mech Mater, 2002;34:145 [22] Chen X, Tian T, An K. Acta Mech Sin, 2001; 33:698 (陈旭,田涛,安柯.力学学报,2001;33:398) [23] Tian T, Chen X, An K. Mater Mech Eng,2002;26(1):19 (田 涛,陈旭,安柯.机械工程材料,2002;26(1):19) |