| Phase Transformation in Ni52Mn21+xGa27-x(x =0-5) Magnetic Shape Memory Alloys |
| GUO Shihai; ZHANG Yanghuan; LI Jianliang; QI Yan; WANG Xinlin |
| Department of Functional Material Research; Central Iron and Steel Research Institute; Beijing 100081 |
|
Cite this article:
GUO Shihai; ZHANG Yanghuan; LI Jianliang; QI Yan; WANG Xinlin. Phase Transformation in Ni52Mn21+xGa27-x(x =0-5) Magnetic Shape Memory Alloys. Acta Metall Sin, 2004, 40(9): 972-974 .
|
|
|
Abstract The martensitic and magnetic phase transformations in
polycrystalline non-stoichiometric
Ni52Mn21+xGa27-x(x=0-5) alloys
were investigated. The experimental results show that the alloys
exhibit ferromagnetic and thermo-elastic martensitic
transformations. The martensitic transformation temperatures
(Ms) increase with increasing Mn content and reach
above room temperature when x>4. The martensitic transformation
hysteresis (δT) decrease with increasing x. The magnetic
phase transformation temperatures (Curie temperature TC
increase with an increase of x within a small range and keep
around 348 K when x>2. In addition, an alloy composition of
Ni52Mn25Ga23 with potential practicality was obtained,
which has a higher martensitic transformation temperature than
room temperature and a transformation hysteresis of only 5 K.
|
|
Received: 29 August 2003
|
|
|
[1] Ullakko K, Huang J K, Kantner C, O'Handley R C. Appl Phys Lett, 1996; 69: 1966 [2] Murray S J, Hayashi R, Marioni M, Allen S M, O'Handley R C. In: Wuttig M ed., Smart Structures and Materials 1999: Smart Materials Technologies, Newport Beach, CA: The Society of Photo-Optical Instrumentation Engineers (SPIE), 3675, 1999: 204 [3] Schlagel D L, Wu Y L, Zhang W, Lograsso T A. J Alloys Compd, 2000; 312: 77 [4] Henry C P, Bono D, Feuchtwanger J, Allen S M, O'Handley R C. J Appl Phys, 2002; 91: 7810 [5] Ezera Y, Sozinov A, Kimmel G, Etelaniemi V, Glavatskaya N I, D'Anci A, Podgursky V, Lindroos V K, Ullakko K. In: Wuttig M ed., Smart Structures and Materials 1999: Smart Materials Technologies, Newport Beach, GA: The Society of Photo-Optical Instrumentation Engineers (SPIE), 3675, 1999: 244 [6] Webster P J. Philos Mag, 1984; 49B: 295 [7] Wang W H, Wu G H, Chen J L, Yu C H, Gao S X, Zhan W S. J Phys Lett, 2000; 11: 3245 [8] Sozinov A, Likhachev A A, Ullakko K. IEEE Trans Magn, 2002; 38: 2814 [9] Murakami Y, Shindo D, Suzuki M, Ohtsuka M, Itagaki K.Acta Mater, 2003; 51: 485 [10] Ma Y Q, Jiang C B, Feng G, Xu H B. Scr Mater, 2003;48: 365 [11] Vasil'ev A, Bozhko A, Khovailo V, Dikshtein I, Shavrov V, Seletskii S, Buchelnikov V. J Magn Magn Mater, 1999; 197: 837 |