Acta Metall Sin  2004, Vol. 40 Issue (9): 972-974     DOI:
Research Articles Current Issue | Archive | Adv Search |
Phase Transformation in Ni52Mn21+xGa27-x(x =0-5) Magnetic Shape Memory Alloys
GUO Shihai; ZHANG Yanghuan; LI Jianliang; QI Yan; WANG Xinlin
Department of Functional Material Research; Central Iron and Steel Research Institute; Beijing 100081
Cite this article: 

GUO Shihai; ZHANG Yanghuan; LI Jianliang; QI Yan; WANG Xinlin. Phase Transformation in Ni52Mn21+xGa27-x(x =0-5) Magnetic Shape Memory Alloys. Acta Metall Sin, 2004, 40(9): 972-974 .

Download:  PDF(6827KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The martensitic and magnetic phase transformations in polycrystalline non-stoichiometric Ni52Mn21+xGa27-x(x=0-5) alloys were investigated. The experimental results show that the alloys exhibit ferromagnetic and thermo-elastic martensitic transformations. The martensitic transformation temperatures (Ms) increase with increasing Mn content and reach above room temperature when x>4. The martensitic transformation hysteresis (δT) decrease with increasing x. The magnetic phase transformation temperatures (Curie temperature TC increase with an increase of x within a small range and keep around 348 K when x>2. In addition, an alloy composition of Ni52Mn25Ga23 with potential practicality was obtained, which has a higher martensitic transformation temperature than room temperature and a transformation hysteresis of only 5 K.
Key words:  Ni-Mn-Ga      martensitic transformation      ferromagnetic phase transformation      
Received:  29 August 2003     
ZTFLH:  TG139.6  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I9/972

[1] Ullakko K, Huang J K, Kantner C, O'Handley R C. Appl Phys Lett, 1996; 69: 1966
[2] Murray S J, Hayashi R, Marioni M, Allen S M, O'Handley R C. In: Wuttig M ed., Smart Structures and Materials 1999: Smart Materials Technologies, Newport Beach, CA: The Society of Photo-Optical Instrumentation Engineers (SPIE), 3675, 1999: 204
[3] Schlagel D L, Wu Y L, Zhang W, Lograsso T A. J Alloys Compd, 2000; 312: 77
[4] Henry C P, Bono D, Feuchtwanger J, Allen S M, O'Handley R C. J Appl Phys, 2002; 91: 7810
[5] Ezera Y, Sozinov A, Kimmel G, Etelaniemi V, Glavatskaya N I, D'Anci A, Podgursky V, Lindroos V K, Ullakko K. In: Wuttig M ed., Smart Structures and Materials 1999: Smart Materials Technologies, Newport Beach, GA: The Society of Photo-Optical Instrumentation Engineers (SPIE), 3675, 1999: 244
[6] Webster P J. Philos Mag, 1984; 49B: 295
[7] Wang W H, Wu G H, Chen J L, Yu C H, Gao S X, Zhan W S. J Phys Lett, 2000; 11: 3245
[8] Sozinov A, Likhachev A A, Ullakko K. IEEE Trans Magn, 2002; 38: 2814
[9] Murakami Y, Shindo D, Suzuki M, Ohtsuka M, Itagaki K.Acta Mater, 2003; 51: 485
[10] Ma Y Q, Jiang C B, Feng G, Xu H B. Scr Mater, 2003;48: 365
[11] Vasil'ev A, Bozhko A, Khovailo V, Dikshtein I, Shavrov V, Seletskii S, Buchelnikov V. J Magn Magn Mater, 1999; 197: 837
[1] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[2] LI Wei, JIA Xingqi, JIN Xuejun. Research Progress of Microstructure Control and Strengthening Mechanism of QPT Process Advanced Steel with High Strength and Toughness[J]. 金属学报, 2022, 58(4): 444-456.
[3] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[4] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[5] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[6] ZUO Liang, LI Zongbin, YAN Haile, YANG Bo, ZHAO Xiang. Texturation and Functional Behaviors of Polycrystalline Ni-Mn-X Phase Transformation Alloys[J]. 金属学报, 2021, 57(11): 1396-1415.
[7] XIAO Fei, CHEN Hong, JIN Xuejun. Research Progress in Elastocaloric Cooling Effect Basing on Shape Memory Alloy[J]. 金属学报, 2021, 57(1): 29-41.
[8] Jing BAI, Shaofeng SHI, Jinlong WANG, Shuai WANG, Xiang ZHAO. First-Principles Calculations of Phase Stability and Magnetic Properties of Ni-Mn-Ga-Ti FerromagneticShape Memory Alloys[J]. 金属学报, 2019, 55(3): 369-375.
[9] CHEN Lei , HAO Shuo , MEI Ruixue , JIA Wei , LI Wenquan , GUO Baofeng . Intrinsic Increment of Plasticity Induced by TRIP and Its Dependence on the Annealing Temperature in a Lean Duplex Stainless Steel[J]. 金属学报, 2019, 55(11): 1359-1366.
[10] Lishan CUI, Daqiang JIANG. Progress in High Performance Nanocomposites Based ona Strategy of Strain Matching[J]. 金属学报, 2019, 55(1): 45-58.
[11] Cheng WEI, Changbo KE, Haitao MA, Xinping ZHANG. A Modified Phase Field Model Based on Order Parameter Gradient and Simulation of Martensitic Transformation in Large Scale System[J]. 金属学报, 2018, 54(8): 1204-1214.
[12] Zhaozhao WEI, Xiao MA, Xinping ZHANG. Topological Modelling of the B2-B19' Martensite Transformation Crystallography in NiTi Alloy[J]. 金属学报, 2018, 54(10): 1461-1470.
[13] Jilan YANG, Yuankai JIANG, Jianfeng GU, Zhenghong GUO, Haiyan CHEN. Effect of Austenitization Temperature on the Dry Sliding Wear Properties of a Medium Carbon Quenching and Partitioning Steel[J]. 金属学报, 2018, 54(1): 21-30.
[14] Kejian LI,Zhipeng CAI,Yao WU,Jiluan PAN. Research on Austenite Transformation of FB2 Heat-Resistant Steel During Welding Heating Process[J]. 金属学报, 2017, 53(7): 778-788.
[15] Xue WANG,Lei HU,Dongxu CHEN,Songtao SUN,Liquan LI. Effect of Martensitic Transformation on Stress Evolution in Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes[J]. 金属学报, 2017, 53(7): 888-896.
No Suggested Reading articles found!