Microstructure of Cyclically Deformed Titanium with Low Hydrogen Concentration I. |
CHEN Changqiang; LI Shouxin; LI Guangyi; AI Suhua |
Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences |
|
Cite this article:
CHEN Changqiang; LI Shouxin; LI Guangyi; AI Suhua. Microstructure of Cyclically Deformed Titanium with Low Hydrogen Concentration I.. Acta Metall Sin, 2004, 40(3): 235-240 .
|
Abstract Cyclic testes were conducted on commercially pure titanium with low hydrogen concentration, in which hydrides dispersed homogenously. It was found that dislocations can transfer through the coherent interface only before the hydride was fragmented, after fragmentation, dislocations would tangle at the fragments and do not penetrate the interface again due to the decrease of the maximum stress in the fragments. At least three sets of dislocations can be activated in hydrides during the cyclic deformation. To accommodate the inhomogenous strain between the matrix and hydrides, the crystal rotation occurred in both of them. A mechanism for the crystal rotation has been proposed.
|
Received: 07 April 2003
|
|
[1] Grange M, Besson J, Andrieu E. Metall Mater Trans, 2000: 31A:679 [2] Puls M P. Metall Trans, 1991; 22A: 2327 [3] Bai J B, Prioul C, Francois D. Metal1 Mater Trans, 1994; 25A:1185 [4] Teter D F, Robertson I M, Birnbaum H K. Acta Mater, 2001; 49:4313 [5] Shih D S, Robertson I M, Birnbaum H K. Acta Metall, 1988; 32:111 [6] Huez J, Feaugas X, Helbert A L, Guillot I, Clavel M. Metall Mater Trans, 1998; 29A:1615 [7] Guillot I, Feaugas X, Clavel M. Scr Mater, 2001; 44:1011 [8] Bai J B, Ji N, Gilbon D, Leburn J L. Scr Metall Mater, 1992; 26:369 [9] Chen C Q, Li S X. Lu K. Acta Mater, 2003; 51:931 [10] Chen C Q, Li S X, Lu K. Acta Metall Sin, 2003; 39:120(陈常强,李守新,卢柯.金属学报,2003; 39:120) [11] Stevenson R, Breedis J F. Acta Metall, 1975; 23:1419 [12] Naka S, Lasalmonie A, Costa P, Kubin L. Philos Mag, 1988; 57:717 [13] Dickson J I, Handfirtd L, L'Esperance G. Mater Sci Eng, 1983; 60:L3 [14] Song S, Gray Ⅲ G T. Philos Mag, 1995; 71:263 [15] Crecy A D, Bourret A, Naka S, Lasalmonie A. Philos Mag, 1983; 47:245 [16] Chateau J P, Delafosse D, Magnin T. Acta Mater, 2002; 50:1507 [17] Bourret A, Lasalmonie A, Naka S. Scr Metall, 1986; 20: 861 [18] Gibson M A, Forwood C T. Philos Mag, 2000; 80:2747 [19] Eshelby J D. Proc Roy Soc, 1957; A241:376 [20] Beremin F M. Metall Trans, 1981; 12A: 723 [21] Calabrese C, Laird C. Mater Sci Eng, 1974; 13:141 [22] Panin V E. Acta Metall Sin, 1997; 33:187 (Panin V E.金属学报,1997; 33: 187) [23] Konig G, Blum W. Acta Metall, 1980; 28:519 [24] Holt D L. J Appl Phys, 1970; 41:3197 |