| Effects of TiC on the Conductivities of Titania Slag |
| ZHONG Hexiang; WANG Shulan; ZHANG Lijun |
| Department of Chemistry; Northeastern University; Shenyang 110004 |
|
Cite this article:
ZHONG Hexiang; WANG Shulan; ZHANG Lijun. Effects of TiC on the Conductivities of Titania Slag. Acta Metall Sin, 2004, 40(5): 515-517 .
|
|
|
Abstract By an a.c. impedance technique, the effects of TiC particle on the
conductivities of titania slag with composition of
24.3%CaO-23.3%SiO2-13.8%Al2O3-15.3%MgO-23.3%TiO2
were studied in the temperature range of 1723 K to 1633 K. TiC
particles in the slag are charge carriers and decrease the
conductivities of the slag. The slag containing
0.5%TiC has the lowest conductivity. Increasing the particle
size, the conductivities increase. The rate
constants and the activation energy of the
crystallization reaction of CaTiO3 were
calculated based on the first-order kinetic equation.
|
|
Received: 20 August 2003
|
|
|
[1] Xu C D, Lin R. Iron Steel Vanadium Titanium, 1980; 1: 1(徐采栋,林蓉.钢铁钒钛,1980;1:1) [2] Ma J Y, Sun X W, Sheng S X. Iron Steel, 2000; 35:4(马家源,孙希文,盛世雄.钢铁,2000;35:4) [3] Wan X, Pei H N, Bai C G, Zhou P T. J Chongqing Univ (Nat Sci), 2000; 23:37(万新,裴鹤年,白晨光,周培土.重庆大学学报(自然科学版),2000;23:37) [4] Bai C G, Pei H N, Zhao S J, Zhou P T. Iron Steel Vanadium Titanium, 1995; 16:6(白晨光,裴鹤年,赵诗金,周培土.钢铁钒钛,1995;16:6) [5] Wang S L, Li G Q, Sui Z T. ISIJ Int, 1999; 39:11 [6] Lou T P, Li Y H, Li L S, Sui Z T. Acta Metall Sin, 2000; 36:141(娄太平,李玉海,李辽沙,隋智通.金属学报,2000;36:141) [7] Hu Y, L ü R D, Liu G J, Lu Y N. Physical Chemist. Vol.2, 3nd ed., Beijing: High Education Press, 1988:232(胡英,吕瑞东,刘国杰,陆曜南.物理化学(下册).第3版,北京:高等教育出版社,1988;223) [8] Allibert M. Verein Deutscher Eisenhuttenleute (VDEH). Slag Atlas. 2nd ed., Diisseldorf: Verlag Stahleisen GmbH Press, 1995:2J |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|