| Superplastic Flow Behavior of Zr Base Bulk Metallic Glass in Supercooled Liquid Region |
| SHEN Jun; WANG Gang; SUN Jianfei;CHEN Demin; XING Dawei; ZHOU Bide |
| School of Material Science and Engineering; Harbin Institute of Technology; Harbin 150001; Department of Aerospace Engineering; Harbin Engineering University; Harbin 150001 |
|
Cite this article:
SHEN Jun; WANG Gang; SUN Jianfei; CHEN Demin; XING Dawei; ZHOU Bide. Superplastic Flow Behavior of Zr Base Bulk Metallic Glass in Supercooled Liquid Region. Acta Metall Sin, 2004, 40(5): 518-522 .
|
|
|
Abstract Isothermal tensile tests of
Zr41.25Ti13.75Ni10Cu12.5Be22.5
bulk metallic glass in supercooled liquid region
are carried out at four characteristic temperatures
of 616 , 636, 656 and 676 K which are in the vicinity of
the end temperature of glass transition. Experimental results
indicate that the superplastic flow behaviors of the
material, viz., the flow stress and the elongation
depend strongly on the testing temperature and tensile rate. The
elongation increases firstly and then decreases with increasing
rate and the maximum elongation reaches
1625% at 656 K and 5 mm/min. The strain rate sensitivity
exponents determined by using Backofen method are
0.25, 0.65 and 0.93 at 636 , 656 and 676 K,
respectively. The free volume model is used to interpret the
observed superplastic flow behavior.
|
|
Received: 29 May 2003
|
|
|
[1] Zhang Q S, Guo D Y, Wang A M, Zhang H F, Ding B Z, Hu Z Q. Intermetallics, 2002; 10:1197 [2] Wang W H, Wei Q, Friedrich S. J Mater Sci, 2000; 35: 2291 [3] Jiang S W, Qi M. Res Met Mater, 2003; 29(1) : 44(姜淑文,齐民.金属材料研究,2003;29(1) :44) [4] Bian Z, Chen G L, He G, Hui X D. Mater Sci Eng, 2001; A316:135 [5] Liu L, Wu Z F, Zhang J. J Alloys Compd, 2002; 339:90 [6] Zhang Y, Ji Y F, Zhao D Q, Wang R J, Pan M X, Dong Y D, Wang W H. Scr Mater, 2001; 44:1107 [7] Kawamura Y, Shibata T, Inoue A, Masumoto T. Scr Mater, 1997; 37: 431. [8] Kawamura Y, Nakamura T, Kato H, Mano H, Inoue A. Mater Sci Eng, 2001; A304-306:674 [9] Kawamura Y, Nakamura T, Inoue A. Scr Mater, 1998; 39: 301 [10] Nieh T G, Wadsworth J, Liu C T, Ohkubo T, Hirotsu Y. Acta Mater, 2001; 49:2887 [11] Nieh T G, Mukai T, Liu C T. Scr Mater, 1999; 40:1021 [12] Reger-Leonhard A, Heilmaier M, Eckert J. Scr Mater, 2000; 43:459 [13] Johnson W L, Lu J, Demetriou M D. Intermetallics, 2002; 10:1039 [14] Lee K S, Ha T K, Ahn S, Chang Y W. J Non-Cryst Solids, 2003; 317:193 [15] Saotome Y, Hatori T, Zhang T, Inoue A. Mater Sci Eng, 2001; A304-306:716 [16] Saotome Y, Itoh K, Zhang T, Inoue A. Scr Mater, 2001; 44:1541 [17] Wu S D. The Principle of Metal Superplastic Formation. Beijing: National Defense Industry Press, 1997:9(吴诗惇.金属超塑性变形理论.北京;国防工业出版社,1997:9) [18] Wang W H, Bai H Y, Luo J L, Wang R J, Jin D. Phys Rev, 2000, 62B: 25 [19] Spaepen F. Acta Metall, 1977; 25:407 [20] Beukel V D. Key Eng Mater, 1993; 81-83: 3 |