Abstract The concept of deformation enhanced transformation of ferrite in plain
low carbon steel and its characteristics are presented. The systematic
work indicates that deformation significantly enhances the ferrite
transformation of undercooled austenite in plain low carbon steel.
Nucleation is the dominant process of the transformation. Until the
completion of the transformation, nucleation is always repeated,
especially at the zone in front of the newly formed ferrite grains,
which restricts the grain growth and leads to formation of very fine
ferrite grains. Three stages of kinetics are clearly shown from the
experimental measurement, which correspond to nucleation at grain
boundaries, at the zone in front of newly formed ferrite grains and
at residual austenite.
|
|
Received: 24 February 2003
|
|
|
[1] Sun Z Q, Yang W Y, Qi J J, Hu A M. Mater Sci Eng, 2002; A334: 201 [2] Priestner R, Hodgson P D. Mater Sci Technol, 1992; 8: 849 [3] Sekine H, Maruyama T, Kageyama H, Kawashiwa Y. In: de Ardo A J, Ratz G A, Wray. P J, eds., Themomechanical Processing of Microalloyed Austenite, Warrendale, Pa: TMS-AIME, 1982: 141 [4] Beynon J H, Gloss R, Hodgson P D. Mater Forum, 1992; 16: 37 [5] Sun Z Q, Yang W Y, Hu A M, Yang P. Acta Metall Sin (Engl Lett), 2001; 14: 115 [6] Yang W Y, Hu A M, Qi J J, Sun Z Q. Chin J Mater Res, 2001; 15: 171(杨王玥,胡安民,齐俊杰,孙祖庆.材料研究学报,2001;15:171) [7] Cahn J W. Acta Metall, 1956; 9: 449 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|