Acta Metall Sin  2018, Vol. 54 Issue (3): 393-403    DOI: 10.11900/0412.1961.2017.00284
Orginal Article Current Issue | Archive | Adv Search |
Finite Element Simulation of the Temperature Field and Residual Stress in GH536 Superalloy Treated by Selective Laser Melting
Shu WEN1, Anping DONG1,2(), Yanling LU3, Guoliang ZHU1,2, Da SHU1,2, Baode SUN1,2,4
1 School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
2 Shanghai Key Lab of Advanced High-Temperature Materials and Precision Forming, Shanghai Jiao Tong University, Shanghai 200240, China
3 Shanghai Institute of Applied Physics, Chinese Academy of Sciences, Shanghai 201800, China
4 State Key Laboratory of Metal Matrix Composites, Shanghai Jiao Tong University, Shanghai 200240, China
Cite this article: 

Shu WEN, Anping DONG, Yanling LU, Guoliang ZHU, Da SHU, Baode SUN. Finite Element Simulation of the Temperature Field and Residual Stress in GH536 Superalloy Treated by Selective Laser Melting. Acta Metall Sin, 2018, 54(3): 393-403.

Download:  HTML  PDF(4416KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

In the aerospace industry, due to the increasing hardness and tensile strength of nickel-based superalloys, the traditional manufacturing methods are difficult to produce, which limits the freedom of part design and process. Selective laser melting (SLM) has great potential in this field with its additive manufacturing concept and full melting during the process. Although the dense part can be easily obtained in SLM, the residual stresses and micro-cracks in the machining process still affect the dimensional accuracy and reliability of the parts. In SLM process, rapid and complex changes of temperature and stress are observed in the vicinity of the molten pool. Understanding these changes will help to improve the quality of the process. In this work, a finite element model (FEM) is established to calculate the temperature and residual stress distribution near the weld pool during the SLM of Hastelloy X superalloy, The model uses a composite Gauss heat source to consider the influence of optical penetration depth, and implements the transformation of powder, molten pool and solid metal by changing the material properties with temperature. Comparison with the test results shows that the model can simulate the distribution of temperature field and the residual stress in SLM process well. The simulation results show that with the increase of laser power, the width, length and depth of melting pool were enlarged, the cooling rate decreases; with the increase of the scanning speed, the width and depth of melting pool decreases, the length remained unchanged, the cooling rate increase. After cooling, there is a large tensile stress on the surface of the model. As the depth increases, the tensile stress decreases rapidly and eventually becomes compressive stress.

Key words:  GH536 superalloy      selective laser melting      residual stress      finite element simulation     
Received:  07 July 2017     
Fund: Supported by National Natural Science Foundation of China (Nos.51771118, U1760110 and 51674237) and Aeronautical Science Foundation of China (No.2015ZE57011)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2017.00284     OR     https://www.ams.org.cn/EN/Y2018/V54/I3/393

Fig.1  Finite element model of the selective laser melting (SLM) process
Process parameter Value Unit
Powder bed thickness h 40 μm
Hatch spacing Hs 90 μm
Laser spot size D 100 μm
Scanning speed v 900, 1100, 1300 mms-1
Initial temperature T0 20 ℃
Power P 150, 200, 250 W
Table 1  Process parameters for simulation
Fig.2  Low magnified OM (a) and high magnified SEM (b) images show the melt pool morphologies of GH536 superalloy treated by SLM under P=200 W and v=1100 mm/s
Fig.3  Predicted profile temperature contours (a, b) and predicted top surface temperature contours (c, d) at node 1 (a, c) and node 6 (b, d) in Fig.1 under P=200 W and v=1100 mm/s
Fig.4  Predicted profile temperature contours (a, b) and top surface temperature contours (c, d) at node 6 in Fig.1 under P=150 W (a, c) and P=250 W (b, d)
Fig.5  Predicted melt pool size (a) and the ratio of length to width (b) as function of laser power
Fig.6  Predicted profile temperature contours (a, b) and top surface temperature contours (c, d) at node 6 in Fig.1 under v=900 mm/s (a, c) and v=1300 mm/s (b, d)
Fig.7  Predicted melt pool size (a) and the ratio of length to width (b) as function of scanning speed
Fig.8  Cyclic heating and cooling curves at the nodes 2, 3, 4 and 5 in Fig.1 under P=200 W and v=1100 mm/s (Tm—melting point)
Fig.9  Cyclic heating and cooling curves at the node 3 in Fig.1 under v=1100 mm/s and different P
Fig.10  Cyclic heating and cooling curves at the node 3 under P=200 W and different v
Fig.11  Sample for stress test prepared by SLM under P=200 W and v=1100 mm/s
Fig.12  Equivalent residual stress σMises along depth direction with different parameters of v=1100 mm/s (a) and P=200 W (b)
Fig.13  Distributions of residual stress along line 1 in Fig.1 with different parameters(a) x direction and v=1100 mm/s(b) x direction and P=200 W(c) y direction and v=1100 mm/s(d) y direction and P=200 W
Fig.14  Distributions of residual stress along line 2 in Fig.1 with different parameters(a) x direction and v=1100 mm/s(b) x direction and P=200 W(c) y direction and v=1100 mm/s(d) y direction and P=200 W
[1] Huang W P, Yu H C, Yin J, et al.Microstructure and mechanical properties of K4202 cast nickel base superalloy fabricated by selective laser melting[J]. Acta Metall. Sin., 2016, 52: 1089(黄文普, 喻寒琛, 殷杰等. 激光选区熔化成形K4202镍基铸造高温合金的组织和性能 [J]. 金属学报, 2016, 52: 1089)
[2] Jia Q B, Gu D D.Selective laser melting additive manufacturing of Inconel 718 superalloy parts: Densification, microstructure and properties[J]. J. Alloys Compd., 2014, 585: 713
[3] Zhang B C, Fenineche N E, Liao H L, et al.Microstructure and magnetic properties of Fe-Ni alloy fabricated by selective laser melting Fe/Ni mixed powders[J]. J. Mater. Sci. Technol., 2013, 29: 757
[4] Kruth J P, Mercelis P, Van Vaerenbergh J, et al.Binding mechanisms in selective laser sintering and selective laser melting[J]. Rapid Prototyping J., 2005, 11: 26
[5] Yadroitsev I, Bertrand P, Smurov I.Parametric analysis of the selective laser melting process[J]. Appl. Surf. Sci., 2007, 253: 8064
[6] Yang J X, Xu F T, Zhou D L, et al.Effects of re-melting processes on the tensile properties of K452 alloy at high temperature[J]. Acta Metall. Sin., 2017, 53: 703(杨金侠, 徐福涛, 周动林等. 重熔工艺对K452合金高温拉伸性能的影响 [J]. 金属学报, 2017, 53: 703)
[7] Wang F D.Mechanical property study on rapid additive layer manufacture Hastelloy? X alloy by selective laser melting technology[J]. Int. J. Adv. Manuf. Technol., 2012, 58: 545
[8] Song B, Zhao X, Li S, et al.Differences in microstructure and properties between selective laser melting and traditional manufacturing for fabrication of metal parts: A review[J]. Front. Mech. Eng., 2015, 10: 111
[9] Roberts I A, Wang C J, Esterlein R, et al.A three-dimensional finite element analysis of the temperature field during laser melting of metal powders in additive layer manufacturing[J]. Int. J. Mach. Tools Manuf., 2009, 49: 916
[10] Zhang D Q, Cai Q Z, Liu J H, et al.Select laser melting of W-Ni-Fe powders: Simulation and experimental study[J]. Int. J. Adv. Manuf. Technol., 2010, 51: 649
[11] Hussein A, Hao L, Yan C Z, et al.Finite element simulation of the temperature and stress fields in single layers built without-support in selective laser melting[J]. Mater. Des., 2013, 52: 638
[12] Cheng B, Shrestha S, Chou K.Stress and deformation evaluations of scanning strategy effect in selective laser melting[J]. Addit. Manuf., 2016, 12: 240
[13] Papadakis L, Loizou A, Risse J, et al.A computational reduction model for appraising structural effects in selective laser melting manufacturing: A methodical model reduction proposed for time-efficient finite element analysis of larger components in selective laser melting[J]. Virt. Phys. Prototyping, 2014, 9: 17
[14] Dai K, Shaw L.Finite element analysis of the effect of volume shrinkage during laser densification[J]. Acta Mater., 2005, 53: 4743
[15] Yilbas B S, Arif A F M. Material response to thermal loading due to short pulse laser heating[J]. Int. J. Heat Mass Transfer, 2001, 44: 3787
[16] Tsirkas S A, Papanikos P, Kermanidis T.Numerical simulation of the laser welding process in butt-joint specimens[J]. J. Mater. Process. Technol., 2003, 134: 59
[17] Yin J, Zhu H H, Ke L D, et al.Simulation of temperature distribution in single metallic powder layer for laser micro-sintering[J]. Comput. Mater. Sci., 2012, 53: 333
[18] Foroozmehr A, Badrossamay M, Foroozmehr E, et al.Finite element simulation of selective laser melting process considering optical penetration depth of laser in powder bed[J]. Mater. Des., 2016, 89: 255
[19] Ma L, Bin H Z.Temperature and stress analysis and simulation in fractal scanning-based laser sintering[J]. Int. J. Adv. Manuf. Technol., 2007, 34: 898
[20] Hou H P, Liang Y C, He Y L, et al.Microstructural evolution and tensile property of hastelloy-X alloys produced by selective laser melting[J]. Chin. J. Lasers, 2017, 44: 0202007(侯慧鹏, 梁永朝, 何艳丽等. 选区激光熔化Hastelloy-X合金组织演变及拉伸性能 [J]. 中国激光, 2017, 44: 0202007)
[21] Fischer P, Romano V, Weber H P, et al.Sintering of commercially pure titanium powder with a Nd: YAG laser source[J]. Acta Mater., 2003, 51: 1651
[22] Zhou W X, Wang X, Hu J B, et al.Melting process and mechanics on laser sintering of single layer polyamide 6 powder[J]. Int. J. Adv. Manuf. Technol., 2013, 69: 901
[23] Yin J, Zhu H H, Ke L D, et al.A finite element model of thermal evolution in laser micro sintering[J]. Int. J. Adv. Manuf. Technol., 2016, 83: 1847
[24] Tolochko N K, Khlopkov Y V, Mozzharov S E, et al.Absorptance of powder materials suitable for laser sintering[J]. Rapid Prototyping J., 2000, 6: 155
[25] Zhao M, Xu L Y, Zhang K S.Low cycle creep-fatigue behavior of nickel base superalloy GH536[J]. Mech. Sci. Technol., 2003, 22: 639(赵明, 徐林耀, 张克实. GH536合金高温低周疲劳/蠕变交互作用性能研究 [J]. 机械科学与技术, 2003, 22: 639)
[26] Criales L E, Ar?soy Y M, ?zel T.Sensitivity analysis of material and process parameters in finite element modeling of selective laser melting of Inconel 625[J]. Int. J. Adv. Manuf. Technol., 2016, 86: 2653
[27] Dong L, Makradi A, Ahzi S, et al.Three-dimensional transient finite element analysis of the selective laser sintering process[J]. J. Mater. Process. Technol., 2009, 209: 700
[28] Yu H C, Wu X R.Material Data Book for Aircraft Engine Design: Fourth Volume [M]. Beijing: Aviation Industry Press, 2010: 107(于慧臣, 吴学仁. 航空发动机设计用材料数据手册: 第四册 [M]. 北京: 航空工业出版社, 2010: 107)
[29] Li Y L, Gu D D.Parametric analysis of thermal behavior during selective laser melting additive manufacturing of aluminum alloy powder[J]. Mater. Des., 2014, 63: 856
[30] Alimardani M, Toyserkani E, Huissoon J P, et al.On the delamination and crack formation in a thin wall fabricated using laser solid freeform fabrication process: An experimental-numerical investigation[J]. Opt. Lasers Eng., 2009, 47: 1160
[31] Gu D D, Shen Y F.Balling phenomena in direct laser sintering of stainless steel powder: Metallurgical mechanisms and control methods[J]. Mater. Des., 2009, 30: 2903
[32] Li R D, Liu J H, Shi Y S, et al.Balling behavior of stainless steel and nickel powder during selective laser melting process[J]. Int. J. Adv. Manuf. Technol., 2012, 59: 1025
[33] Harrison N J, Todd I, Mumtaz K.Reduction of micro-cracking in nickel superalloys processed by selective laser melting: A fundamental alloy design approach[J]. Acta Mater., 2015, 94: 59
[34] Davies H A, Shohoji N, Warrington D H.The structure of rapidly quenched nickel-based superalloy ribbons produced by melt spinning [A]. Proceedings of the 2nd International Conference on Rapid Solidification Processing [C]. Baton Rouge, LA: Claitor's Publishing Division, 1980
[35] Shiomi M, Osakada K, Nakamura K, et al.Residual stress within metallic model made by selective laser melting process[J]. CIRP Ann., 2004, 53: 195
[36] Zaeh M F, Branner G.Investigations on residual stresses and deformations in selective laser melting[J]. Prod. Eng., 2010, 4: 35
[37] Vrancken B, Cain V, Knutsen R, et al.Residual stress via the contour method in compact tension specimens produced via selective laser melting[J]. Scr. Mater., 2014, 87: 29
[1] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[2] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[3] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[4] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[5] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[6] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[7] TANG Weineng, MO Ning, HOU Juan. Research Progress of Additively Manufactured Magnesium Alloys: A Review[J]. 金属学报, 2023, 59(2): 205-225.
[8] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[9] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[10] QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng. Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects[J]. 金属学报, 2023, 59(10): 1411-1418.
[11] LU Haifei, LV Jiming, LUO Kaiyu, LU Jinzhong. Microstructure and Mechanical Properties of Ti6Al4V Alloy by Laser Integrated Additive Manufacturing with Alternately Thermal/Mechanical Effects[J]. 金属学报, 2023, 59(1): 125-135.
[12] WANG Meng, YANG Yongqiang, Trofimov Vyacheslav, SONG Changhui, ZHOU Hanxiang, WANG Di. Effects of Particle Size on Processability of AlSi10Mg Alloy Manufactured by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 147-156.
[13] YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi. Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 55-74.
[14] ZHU Guoliang, KONG Decheng, ZHOU Wenzhe, HE Jian, DONG Anping, SHU Da, SUN Baode. Research Progress on the Crack Formation Mechanism and Cracking-Free Design of γ' Phase Strengthened Nickel-Based Superalloys Fabricated by Selective Laser Melting[J]. 金属学报, 2023, 59(1): 16-30.
[15] PENG Liming, DENG Qingchen, WU Yujuan, FU Penghuai, LIU Ziyi, WU Qianye, CHEN Kai, DING Wenjiang. Additive Manufacturing of Magnesium Alloys by Selective Laser Melting Technology: A Review[J]. 金属学报, 2023, 59(1): 31-54.
No Suggested Reading articles found!