| Research on Hot Working Behavior of Low-NickelDuplex Stainless Steel 2101 |
Yusen SU, Yinhui YANG( ), Jianchun CAO, Yuliang BAI |
| School of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China |
|
Cite this article:
Yusen SU, Yinhui YANG, Jianchun CAO, Yuliang BAI. Research on Hot Working Behavior of Low-NickelDuplex Stainless Steel 2101. Acta Metall Sin, 2018, 54(4): 485-493.
|
|
|
Abstract The thermal deformation difference of two phases for duplex stainless steel (DSS) makes hot working difficult, 2101 DSS substitute Mn, N for Ni to stabilize austenite phase, which will significantly affect hot deformation behavior. Hot compression tests in the temperature ranging from 1123 to 1423 K and strain rate ranging from 0.001 to 10 s-1 were carried out on a Gleeble-3800 thermal simulator for 2101 DSS. At the same strain rate, the flow curve characteristics of 2101 DSS changed from dynamic recrystallization (DRX) to dynamic recovery with increasing deformation temperature. Increasing deformation stain rate from 0.001 s-1 to 0.01 and 0.1 s-1 increased DRX temperature range, but higher strain rate of 1 and 10 s-1 is not beneficial to DRX occurrence. In the deformation temperature region of 1253~1323 K and low strain rate of 0.001~0.1 s-1, the smaller strain value corresponding to the peak stress, the austenite DRX is more likely to occur, which is beneficial to the equiaxed recrystallized grains formation. At low strain rate, the recrystallization grain grows up with the increase of deformation temperature, the worse effect of austenite DRX is related to weakened austenite stabilized ability of Mn substitution for Ni at high Zener-Hollomon parameter values. Based on the thermal deformation equation, the apparent activation energy Q was calculated as 464.49 kJ/mol, which is slightly higher than that of 2205 DSS, and the constitutive equation of the peak flow stress was established. By combining with flow curve and microstructure analysis, the processing map exhibits the optimum processing conditions are in deformation temperature ranging from 1220 to 1350 K and strain rate ranging from 0.001 to 0.1 s-1 with high power dissipation coefficient of 0.40~0.47, under which the austenite DRX obviously occurred.
|
|
Received: 25 April 2017
|
|
|
| Fund: Supported by National Natural Science Foundation of China (No.51461024) |
| [1] | Charles J, Chemelle P.The history of duplex developments, nowadays DSS properties andduplex market future trends[J]. World Iron Steel, 2012, 144: 477 | | [2] | Feng H, Zhou X Y, Liu H, et al.Development and trend of hyper duplex stainless steels[J]. J. Iron. Steel. Res., 2015, 27(4): 1(丰涵, 周晓玉, 刘虎等. 特超级双相不锈钢的发展现状及趋势[J]. 钢铁研究学报, 2015, 27(4): 1) | | [3] | Gao W, Luo J M, Yang J J.Research progress and application of double phase stainless steel[J]. Ordnance. Mater. Sci. Eng., 2005, 28(3): 61(高娃, 罗建民, 杨建君. 双相不锈钢的研究进展及其应用[J]. 兵器材料科学与工程, 2005, 28(3): 61) | | [4] | Du C F, Zhan F, Yang Y H, et al.Research progress in nickel-saving duplex stainless steel[J]. Met. Funct. Mater., 2010, 17(5): 63(杜春风, 詹凤, 杨银辉等. 节镍型双相不锈钢的研究进展[J]. 金属功能材料, 2010, 17(5): 63) | | [5] | Nilsson J O, Kangas P, Wilson A, et al.Mechanical properties, microstructural stability and kinetics of σ-phase formation in 29Cr-6Ni-2Mo-0.38N superduplex stainless steel[J]. Metall. Mater. Trans., 2000, 31A: 35 | | [6] | Han D, Jiang Y M, Deng B, et al.Effect of aging time on electrochemical corrosion behavior of 2101 duplex stainless steel[J]. Acta Metall. Sin., 2009, 45: 919(韩冬, 蒋益明, 邓博等. 时效时间对2101双相不锈钢电化学腐蚀行为的影响[J]. 金属学报, 2009, 45: 919) | | [7] | He Y, Zhang C L, Wang J, et al.Effects of aging temperature on intergranular corrosion behavior of S32101 lean duplex stainless steel[J]. Corros. Sci. Prot. Technol., 2016, 28: 241(何燕, 张彩丽, 王剑等. 时效温度对节镍双相不锈钢S32101晶间腐蚀行为影响的研究[J]. 腐蚀科学与防护技术, 2016, 28: 241) | | [8] | Shi F, Wang L J, Cui W F, et al.Precipitation behavior of M2N in a high-nitrogen austenitic stainless steel during isothermal aging[J]. Acta Metall. Sin.(Engl. Lett.), 2007, 20: 95 | | [9] | Fang Y L, Liu Z Y, Wang G D.Effect of isothermal aging on precipitation behavior of lean duplex stainless steel 2101[J]. J. Iron. Steel. Res., 2010, 22(6): 21(方轶琉, 刘振宇, 王国栋. 等温时效对节约型双相不锈钢2101析出行为的影响[J]. 钢铁研究学报, 2010, 22(6): 21) | | [10] | Lin H X, Fan Y G, Zhou S P.Study on uniform corrosion resistance of 22Cr duplex stainless steel[J]. Corros. Protect. Petrochem. Ind., 2008, 25(6): 10(林红先, 樊玉光, 周三平. 22Cr双相不锈钢耐均匀腐蚀性能的研究[J]. 石油化工腐蚀与防护, 2008, 25(6): 10) | | [11] | Yang Y H, Yan B.Effect of high temperature compression deformation strain rate on the microstructure and corrosion behavior of 2205 duplex stainless steel[J]. Anti-Corros. Methods Mater., 2015, 62: 163 | | [12] | Zhao K W.Study on hot deformation behavior of 00Cr22Ni5Mo-3N duplex stainless steel [D]. Lanzhou: Lanzhou University of Technology, 2010(赵科巍. 2205双相不锈钢的高温变形过程及其机理研究 [D]. 兰州: 兰州理工大学, 2010) | | [13] | Wang Y X, Liu Z Y, Wang G D, et al.Laboratory study on hot deformation behavior of 2205 duplex stainless steel[J]. J. Plast. Eng., 2012, 19(4): 89(王月香, 刘振宇, 王国栋等. 双相不锈钢2205热变形行为的实验[J]. 塑性工程学报, 2012, 19(4): 89) | | [14] | Wang J F, Wang Y X, Hua F A, et al.Static softening behavior and microstructures analysis of duplex stainless steel after hot deformation[J]. J. Iron. Steel. Res., 2011, 23(9): 46(王佳夫, 王月香, 花福安等. 双相不锈钢热变形后的静态软化行为及组织分析[J]. 钢铁研究学报, 2011, 23(9): 46) | | [15] | Liu Y Y.Study on microstruture and property evolution of LDX2101 during thermal deformation [D]. Hangzhou: Zhejiang University, 2013(刘彦妍. 2101双相不锈钢热变形过程微观组织与性能演变的研究 [D]. 杭州: 浙江大学, 2013) | | [16] | Fang Y L, Liu Z Y, Zhang W N, et al.Microstructure evolution of lean duplex stainless steel 2101 during hot deformation[J]. Acta Metall. Sin., 2010, 46: 641(方轶琉, 刘振宇, 张维娜等. 节约型双相不锈钢2101高温变形过程中微观组织演化[J]. 金属学报, 2010, 46: 641) | | [17] | Du S W, Chen S M.Hot deformation behavior and processing maps of LZ50 steel[J]. Trans. Mater. Heat. Treat., 2016, 37: 223(杜诗文, 陈双梅. LZ50钢的热变形行为及热加工图[J]. 材料热处理学报, 2016, 37: 223) | | [18] | Sellars C M, Mctegart W J.On the mechanism of hot deformation[J]. Acta Metall., 1966, 14: 1136 | | [19] | Wu K.Study on hot deformation behavior and mechanism of economical duplex stainless steel 2101 [D]. Xi'an: Xi'an University of Architecture and Technology, 2013(吴琨. 经济型双相不锈钢2101高温变形行为及机理研究 [D]. 西安: 西安建筑科技大学, 2013) | | [20] | Duprez L, Cooman B C D, Akdut N. Flow stress and ductility of duplex stainless steel during high-temperature torsion deformation[J]. Metall. Mater. Trans., 2002, 33A: 1931 | | [21] | Chen L, Wang L M, Du X J, et al.Hot deformation behavior of 2205 duplex stainless steel[J]. Acta Metall. Sin., 2010, 46: 52(陈雷, 王龙妹, 杜晓建等. 2205双相不锈钢的高温变形行为[J]. 金属学报, 2010, 46: 52) | | [22] | Cabrera J M, Mateo A, Llanes L, et al. Hot deformation of duplex stainless steels [J]. J. Mater. Process. Technol., 2003, 143-144: 321 | | [23] | Farnoush H, Momeni A, Dehghani K, et al.Hot deformation characteristics of 2205 duplex stainless steel based on the behavior of constituent phases[J]. Mater. Des., 2010, 31: 220 | | [24] | Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242[J]. Metall. Mater. Trans., 1984, 15A: 1883 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|