MODELING AND SIMULATION OF DIRECTIONAL SOLIDIFICATION BY LMC PROCESS FOR NICKEL BASE SUPERALLOY CASTING |
Xuewei YAN1,Ning TANG1,Xiaofu LIU2,Guoyan SHUI2,Qingyan XU1( ),Baicheng LIU1 |
1 Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing 100084 2 Shenyang Research Institute of Foundry, Shenyang 110022 |
|
Cite this article:
Xuewei YAN,Ning TANG,Xiaofu LIU,Guoyan SHUI,Qingyan XU,Baicheng LIU. MODELING AND SIMULATION OF DIRECTIONAL SOLIDIFICATION BY LMC PROCESS FOR NICKEL BASE SUPERALLOY CASTING. Acta Metall Sin, 2015, 51(10): 1288-1296.
|
|
|
|
Fund: Supported by National Basic Research Program of China (No.2011CB706801), National Natural Science Foundation of China (Nos.51171089 and 51374137) and National Science and Technology Major Projects of China (Nos.2012ZX04012-011 and 2011ZX04014-052) |
[1] | Nabarro F R. Mater Sci Eng, 1994; A184: 167 | [2] | Huang Q Y,Li H K. Superalloys. Beijing: Metallurgical Industry Press, 2000: 4 (黄乾尧,李汉康. 高温合金. 北京: 冶金工业出版社, 2000: 4) | [3] | Guo R F, Liu L, Li Y F, Zhao X B, Zhang J, Fu H Z. Foundry, 2014; 63: 145 (郭如峰, 刘 林, 李亚峰, 赵新宝, 张 军, 傅恒志. 铸造, 2014; 63: 145) | [4] | Bridgman P W. US Pat, 88650, 1926 | [5] | Tang N, Wang Y L, Xu Q Y, Zhao X H, Liu B C. Acta Metall Sin, 2015; 51: 499 (唐 宁, 王艳丽, 许庆彦, 赵希宏, 柳百成. 金属学报, 2015; 51: 499) | [6] | Pan D, Xu Q Y, Yu J, Liu B C, Li J R, Yuan H L, Jin H P. Int J Cast Met Res, 2008; 21: 308 | [7] | Liu L, Zhang J, Shen J, Huang T W, Fu H Z. Mater China, 2010; 29(7): 1 (刘 林, 张 军, 沈 军, 黄太文, 傅恒志. 中国材料进展, 2010; 29(7): 1) | [8] | Pan D, Xu Q Y, Liu B C, Li J R, Yuan H L, Jin H P. JOM, 2010; 62(5): 30 | [9] | Tang N, Xu Q Y, Liu B C. Spec Casting Nonferrous Alloy, 2011; 31: 1028 (唐 宁, 许庆彦, 柳百成. 特种铸造及有色合金, 2011; 31: 1028) | [10] | Tang N, Xu Q Y, Liu B C. Foundry Technol, 2012; 33: 558 (唐 宁, 许庆彦, 柳百成. 铸造技术, 2012; 33: 558) | [11] | Rzyankina E, Szeliga D, Mahomed N, Nowotnik A. Appl Mech Mater, 2013; 372: 54 | [12] | Seth B B. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S L, Schirra J J eds., Superalloys 2000, Warrendale, PA: TMS, 2000: 16 | [13] | Singer R F. In: Coutsouradis D, Davidson J H, Ewald J, Greenfield P, Khan T, Malik M, Meadowcroft D B, RegisV, Scarlin R B, Schubert F, Thornton D V eds., Materials for Advanced Power Engineering. Dordrecht, Netherlands: Kluwer Academic Publishers Group, 1994: 1707 | [14] | Lund C H, Hockin J. In: Sims C T, Hagel W C eds., Superalloys 1972, New York: John Wiley & Sons, 1972: 403 | [15] | Kermanpur A, Rappaz M, Varahram N, Davami P. Metall Mater Trans, 2000; 31B: 1293 | [16] | Konter M, Kats E, Hofmann N. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S L, Schirra J J eds., Superalloys 2000, Warrendale, PA: TMS, 2000: 189 | [17] | Nakagawa Y G, Ohotomo Y, Saiga Y. In: Tien J K, Wlodek S T, Morrow H I, Gell M, Mauer G E eds., Superalloys 1980, Metals Park, OH: American Society for Metals, 1980: 267 | [18] | Graham L D, Rauguth B L. US Pat, 6443213, 2002 | [19] | Tschinkel J G, Giamei A F, Kearn B H. US Pat, 3763926, 1973 | [20] | Giamei A F, Tschinkel J G. Metall Trans, 1976; 7A: 1427 | [21] | Elliott A J, Karney G B, Pollock T M. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale, PA: TMS, 2004: 421 | [22] | Liu J H, Liu L, Huang T W, Ge B M, Zhang J, Fu H Z, Yu B, Su G Q. Foundry, 2010; 59: 822 (刘金洪, 刘 林, 黄太文, 葛丙明, 张 军, 傅恒志, 于 波, 苏贵桥. 铸造, 2010; 59: 822) | [23] | Elliott A J, Tin S, King W T, Huang S C, Pollock T M. Metall Mater Trans, 2004; 35A: 3221 | [24] | Kermanpur A, Varahram N, Davami P. Metall Mater Trans, 2000; 31B: 1293 | [25] | Miller J D, Yuan L, Lee P D, Pollock T M. Acta Mater, 2014; 69: 47 | [26] | Lu Y Z, Xi H J, Shen J, Zheng W, Xie G, Lou L H, Zhang J. Acta Metall Sin, 2015; 51: 603 (卢玉章, 席会杰, 申 健, 郑 伟, 谢 光, 楼琅洪, 张 健. 金属学报, 2015; 51: 603) | [27] | Tang N, Yan X W, Xu Q Y, Liu B C. Foundry, 2014; 63: 347 (唐 宁, 闫学伟, 许庆彦, 柳百成. 铸造, 2014; 63: 347) | [28] | Rappaz M, Gandin C A. Acta Metall Mater, 1993; 41: 345 | [29] | Nastac L. Acta Mater, 1999; 47: 4253 | [30] | Thevoz P, Desbiolles J L, Rappaz M. Metall Trans, 1989; 20A: 311 | [31] | Kurz W, Giovanola B, Trivedi R. Acta Metall, 1986; 34: 823 | [32] | Wang W, Lee P D, McLean M. Acta Mater, 2003; 51: 2971 | [33] | Tang N, Sun C B, Zhang H, Xu Q Y, Liu B C. Rare Met Mater Eng, 2013; 42: 2298 (唐 宁, 孙长波, 张 航, 许庆彦, 柳百成. 稀有金属材料与工程, 2013; 42: 2298) | [34] | Ren W P, Li Q, Xiao C B, Song J X, He L M, Huang G H, Cao C X. J Mater Eng, 2014; (6): 74 (任维鹏, 李 青, 肖程波, 宋尽霞, 何利民, 黄光宏, 曹春晓. 材料工程, 2014; (6): 74) |
|