Please wait a minute...
Acta Metall Sin  2012, Vol. 48 Issue (6): 717-724    DOI: 10.3724/SP.J.1037.2012.00019
论文 Current Issue | Archive | Adv Search |
INFLUENCE OF ROLLING TEMPERATURE ON THE {1011}-{1012} TWINNING IN ROLLED AZ31 MAGNESIUM ALLOY SHEETS
LUO Jinru1, LIU Qing2, LIU Wei1, Godfrey Andrew1
1. Laboratory of Advanced Materials, Department of Materials Science and Engineering, Tsinghua University,Beijing 100084
2. School of Materials Science and Engineering, Chongqing University, Chongqing 400044
Cite this article: 

LUO Jinru, LIU Qing, LIU Wei, Godfrey Andrew. INFLUENCE OF ROLLING TEMPERATURE ON THE {1011}-{1012} TWINNING IN ROLLED AZ31 MAGNESIUM ALLOY SHEETS. Acta Metall Sin, 2012, 48(6): 717-724.

Download:  PDF(5691KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The most common manufacturing process for wrought magnesium alloy sheet is warm--rolling and the microstructure and properties of the product are strongly related with the rolling temperature. In particular, {1011}-{1012} double twinning is an important supplemental mechanism for the deformation of magnesium alloys during rolling at low or moderate temperatures. Therefore, the present work studies the microstructural variation of magnesium alloy sheets AZ31 rolled to 9% at different temperatures in the range of 150-350 ℃, and discusses the influence of rolling temperature on the quantity and variety of {1011}-{1012} double twins, as well as recrystallization related to the double twins. The mechanical properties of the rolled sheets and the influences of twins on the mechanical properties have also been discussed. The results show that {1011}-{1012} double twins are observed in the sheets rolled at temperature ranging from 150 to 300 ℃. The fraction of double twin per unit area, and the number of variant types within each primary twin, decreases with the increasing rolling temperature. At the temperature above 250 ℃, only co--planar double twins are observed in each primary twin. Recrystallized grains are observed to nucleate at the twin boundaries in the sheets rolled above 250 ℃, these can consume the twin boundaries and resulting in merging of the twin grains. No {1011}-{1012} twins are found in the AZ31 magnesium alloy sheet rolled at 350 ℃. With the increase of rolling temperature, the yield strength decreases and the ductile elongation increase for the rolled magnesium alloy sheet.
Key words:  AZ31 Mg alloy      rolling temperature      {1011}-{1012} double twin      recrystallization     
Received:  09 January 2012     
ZTFLH: 

TG335.12

 

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2012.00019     OR     https://www.ams.org.cn/EN/Y2012/V48/I6/717

[1] Maksoud I A, Ahmed H, Rodel J.  Mater Sci Eng, 2009; A504: 40

[2] Jain A, Agnew S R.  Mater Sci Eng, 2007; A462: 29

[3] Watanabe H, Mukai T, Ishikawa K.  J Mater Process Technol,2007; 182: 644

[4] Cho J, Kim H, Kang S, Han T.  Acta Mater, 2011; 59: 5638

[5] Ji Y H, Park J J.  Mater Sci Eng, 2008; A485: 299

[6] Bruni C, Forcellese A, Gabrielli F, Simoncini M. J Mater Process Technol, 2010; 210: 1354

[7] Miao Q, Hu L, Wang G, Wang E.  Mater Sci Eng, 2011; A528: 6694

[8] Thirumurugan M, Kumaran S, Suwas S, Srinivasa R T. Mater Sci Eng, 2011; 528: 8460

[9] Beausir B, Biswas S, Kim D I, Toth L S, Suwas S. Acta Mater, 2009; 57: 5061

[10] Perez--Prado M T, del Valle J A, Contreras J M, Ruano O A. Scr Mater, 2004; 50: 661

[11] Liu Q.  Acta Metall Sin, 2010; 46: 1458

     (刘庆. 金属学报, 2010; 46: 1458)

[12] Chapuis A, Driver J H.  Acta Mater, 2011; 59: 1986

[13] Hutchinson W B, Barnett M R.  Scr Mater, 2010; 63: 737

[14] Yoshinaga H, Obara T, Morozumi S.  Mater Sci Eng, 1973; 12: 255

[15] Luo J R, Liu Q, Liu W, Godfrey A.  Acta Metall Sin, 2011; 47: 1567

     (罗晋如, 刘庆, 刘伟, Godfrey A. 金属学报, 2011; 47: 1567)

[16] Yang X Y, Jiang Y P.  Acta Metall Sin, 2010; 46: 451

     (杨续跃, 姜育培. 金属学报, 2010; 46: 451)

[17] Barnett M R, Nave M D, Bettles C J.  Mater Sci Eng, 2004; A386: 205

[18] Reed--Hill R E.  Trans Metall Soc AIME, 1960; 28: 554

[19] Reed--Hill R E, Robertson W D.  Acta Metall, 1957; 5: 717

[20] Barnett M R, Nave M D, Bettles C J.  Mater Sci Eng, 2004; A386: 205

[21] Ando D, Koike J, Sutu Y.  Acta Mater, 2010; 58: 4316

[22] Tang W N, Chen R S, Han E H.  Acta Metall Sin, 2006; 42: 1096

     (唐伟能, 陈荣石, 韩恩厚. 金属学报, 2006; 42: 1096)

[23] Luo J R, Chen X P, Xin R L, Huang G J, Liu Q.  Trans Nonferrous Met Soc Chin, 2008; 18: s194

[24] Martin E, Jonas J J.  Acta Mater, 2010; 58: 4253

[25] Yang X Y, Sun Z Y, Zhang L.  Acta Metall Sin, 2010; 46: 607

     (杨续跃, 孙争艳, 张雷. 金属学报, 2010; 46: 607)

[26] Li X, Yang P, Meng L, Cui F E.  Acta Metall Sin, 2010; 46: 147

     (李萧, 杨平, 孟利, 崔凤娥. 金属学报, 2010; 46: 147)

[27] Luo J R, Godfrey A, Liu W, Liu Q.  Acta Mater, 2011; 60: 1986

[28] Martin E, Capolungo L, Jiang L, Jonas J J.  Acta Mater, 2010; 58: 3970

[29] Barnett M R, Keshavarz Z, Beer A G, Ma X.  Acta Mater, 2008; 56: 5

[30] Kim K H, Suh B C, Bae J H, Shim M S, Kim S, Kim N J.  Scr Mater,2010; 63: 716

[31] Sandlobes S, Zaefferer S, Schestakow I, Yi S, Gonzalez-Martinez R. Acta Mater, 2011; 59: 429

[32] Yang P, Mao W M, Ren X P, Tang Q B.  Trans Nonferrous Met Soc Chin,2004; 14: 851

[33] Ion S E, Humphreys F J, White S H.  Acta Metall, 1982; 30: 1909

[34] Myshlyaev M M, McQueen H J, Mwembela A, Konopleva E.  Mater Sci Eng,2002; A337: 121

[35] Ma Q, Li B, Marin E B, Horstemeyer S J.  Scr Mater, 2011; 65: 823

[36] Ando D, Koike J, Sutou Y.  Acta Mater, 2010; 58: 4316

[37] Hartt W H, Reed--Hill R E.  Trans Metall Soc AIME, 1967; 239: 1511

[38] Ma Q, Kadiri H E, Oppedal A L, Baird J C, Horstemeyer M F, Cherkaoui M. Scr Mater, 2011; 64: 813

[39] Luo J R, Godfrey A, Liu W, Liu Q.  Acta Mater, 2012; 60: 1986

[40] Mahajan S, Chin G Y.  Acta Metall, 1973; 21: 173

[41] Mahajan S, Chin G Y.  Acta Metall, 1974; 22: 1113
[1] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[3] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[4] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[5] CHEN Jilin, FENG Guanghong, MA Honglei, YANG Dong, LIU Wei. Microstructure, Mechanical Properties, and Strengthening Mechanism of Cr-Mo Microalloy Cold Heading Steel[J]. 金属学报, 2022, 58(9): 1189-1198.
[6] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[7] REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong. Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism[J]. 金属学报, 2022, 58(2): 129-140.
[8] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[9] HU Chen, PAN Shuai, HUANG Mingxin. Strong and Tough Heterogeneous TWIP Steel Fabricated by Warm Rolling[J]. 金属学报, 2022, 58(11): 1519-1526.
[10] JIANG Jufu, ZHANG Yihao, LIU Yingze, WANG Ying, XIAO Guanfei, ZHANG Ying. Research on AlSi7Mg Alloy Semi-Solid Billet Fabricated by RAP[J]. 金属学报, 2021, 57(6): 703-716.
[11] LI Yanmo, GUO Xiaohui, CHEN Bin, LI Peiyue, GUO Qianying, DING Ran, YU Liming, SU Yu, LI Wenya. Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel[J]. 金属学报, 2021, 57(3): 363-374.
[12] NI Ke, YANG Yinhui, CAO Jianchun, WANG Liuhang, LIU Zehui, QIAN Hao. Softening Behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N Low Nickel-Type Duplex Stainless Steel During Hot Compression Deformation Under Large Strain[J]. 金属学报, 2021, 57(2): 224-236.
[13] LI Jinshan, TANG Bin, FAN Jiangkun, WANG Chuanyun, HUA Ke, ZHANG Mengqi, DAI Jinhua, KOU Hongchao. Deformation Mechanism and Microstructure Control of High Strength Metastable β Titanium Alloy[J]. 金属学报, 2021, 57(11): 1438-1454.
[14] LIU Chao, YAO Zhihao, JIANG He, DONG Jianxin. The Feasibility and Process Control of Uniform Equiaxed Grains by Hot Deformation in GH4720Li Alloy with Millimeter-Level Coarse Grains[J]. 金属学报, 2021, 57(10): 1309-1319.
[15] XU Zhanyi, SHA Yuhui, ZHANG Fang, ZHANG Huabing, LI Guobao, CHU Shuangjie, ZUO Liang. Orientation Selection Behavior During Secondary Recrystallization in Grain-Oriented Silicon Steel[J]. 金属学报, 2020, 56(8): 1067-1074.