| ELECTROCHEMICAL BEHAVIOR OF B30 Cu-Ni ALLOY WITH SUPER-HYDROPHOBIC SURFACE IN 3.5%NaCl SOLUTION |
| XU Qunjie1, 2), DENG Xianqin1, 2), PAN Hongtao1, 2), YUN Hong1, 2) |
1) Key Laboratory of Shanghai Colleges and Universities for Corrosion Control in Electric Power System and Applied Electrochemistry, Institute of Energy and Environment Engineering, Shanghai University of Electric Power, Shanghai 200090
2) Shanghai Engineering Research Center of Energy-Saving in Heat Exchange Systems, Institute of Energy and Environment Engineering, Shanghai University of Electric Power, Shanghai 200090 |
|
Cite this article:
XU Qunjie DENG Xianqin PAN Hongtao YUN Hong. ELECTROCHEMICAL BEHAVIOR OF B30 Cu-Ni ALLOY WITH SUPER-HYDROPHOBIC SURFACE IN 3.5%NaCl SOLUTION. Acta Metall Sin, 2012, 48(1): 94-98.
|
|
|
Abstract Super-hydrophobic surface has been considered a new and promising anti-corrosion technology, recently. A super-hydrophobic film has been fabricated on Cu-Ni alloy (B30) substrates by chemical etching and self-assembly. The effects of etching process and self-assembly technology on the property of filmed B30 had been investigated by means of contact angle measurement and electrochemical test. The results show that suitable surface roughness played a vital role in preparing super-hydrophobic surface with excellent corrosion resistance in comparison with the electrochemical test results of different hydrophobic B30 surface. Moreover, the results indicated that the corrosion resistance of B30 in 3.5%NaCl solution could greatly improved by the super-hydrophobic surface (contact angle 152.8o), and the inhibition efficiency reached 96.1%.
|
|
Received: 22 July 2011
|
| Fund: Supported by National Natural Science Foundation of China (No.21003089) |
| [1] Chen H, Yin R H, Wan Z Y. Corros Sci, 2008; 50: 3527[2] Wan Z, Zhang L, Yin R H. Acta Metall Sin, 2008; 2: 203(万宗跃, 张利, 印仁和. 金属学报, 2008; 2: 203)[3] Xu Q J, Zhu L J, Qi H. Acta Metall Sin, 2008; 44: 1360(徐群杰, 朱律均, 齐 航. 金属学报, 2008; 44: 1360)[4] Xu Q J, Zhu L J, Cao W M. Acta Phys–Chim Sin, 2008; 24: 1724(徐群杰, 朱律均, 曹为民. 物理化学学报, 2008; 24: 1724)[5] Guo L, Yuan W, Li J. Appl Surf Sci, 2008; 254: 2158[6] Chen L J, Chen M, Zhou H D. Appl Surf Sci, 2008; 255: 3459[7] Wang P, Qiu R, Zhang D. Electrochim Acta, 2010; 56: 517[8] Ishizaki T, Hieda J, Saito N. Electrochim Acta, 2010; 55: 7094[9] He T, Wang Y, Zhang Y. Corros Sci, 2009; 51: 1757[10] Qian B T, Shen Z Q. Langmuir, 2005; 21: 9007[11] Liu T, Yin Y S, Chen S G. Electrochim Acta, 2007; 52: 3709[12] Sarkar D K, Farzaneh M, Paynter R W. Appl Surf Sci, 2010; 256: 3698[13] Tsougeni K, Vourdas N, Tserepi A. Langmuir, 2009; 25: 11748[14] Li S M, Zhou S Z, Liu J H. Acta Phys–Chim Sin, 2009; 25: 2581(李松梅, 周思卓, 刘建华. 物理化学学报, 2009; 25: 2581)[15] Zhang Q, Zhu Y R, Huang Z Y. Chem J Chin Univ, 2009; 30: 2210(张芹, 朱元荣, 黄志勇. 高等学校化学学报, 2009; 30: 2210)[16] Yang H, Pi P, Cai Z. Appl Surf Sci, 2010; 256: 4095[17] Wu X, Zheng L, Wu D. Langmuir, 2005; 21: 2665[18] Kato C, Castle J E, Ateya B C, Pickexing H W. J Electrochem Soc, 1980; 127: 1897[19] Li Y F, Yu Z J, Yu Y F. J Chem Ind Eng (China), 2008; 22: 6(李艳峰, 于志家, 于跃飞. 高等化学工程学报, 2008; 22: 6)[20] Gu C D, Ren H, Tu J P. Langmuir, 2009; 25: 12299[21] Liao Q Q, Yue Z W, Zhu Z W. Acta Phys–Chim Sin, 2009; 25: 1655(廖强强, 岳忠文, 朱忠伟. 物理化学学报, 2009; 25: 1655)[22] Fu X Y, He X H. Appl Surf Sci, 2008; 255: 1776[23] Cassie A B, Bxater S. Faraday Soc, 1944; 40: 546[24] Liu T, Liu T, Chen S G. Chin J Inorg Chem, 2008; 24: 1859(刘通, 刘涛, 陈守刚. 无机化学学报, 2008; 24: 1859)[25] Liu T, Chen S G, Cheng S. Electrochim Acta, 2007; 52: 8003 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|