| CLUSTER-PLUS-GLUE-ATOM MODEL AND COMPOSITION DESIGN OF BCC Ti-Mo-Nb-Zr SOLID SOLUTION ALLOYS WITH LOW YOUNG'S MODULUS |
| MA Rentao1), HAO Chuanpu1), WANG Qing1), REN Mingfa2), WANG Yingmin1), DONG Chuang1) |
1) Key Laboratory of Materials Modification (Ministry of Education), Dalian University of Technology, Dalian 116024
2) State Key Laboratory of Structural Analysis for Industrial Equipment, Dalian University of Technology, Dalian 116024 |
|
Cite this article:
MA Rentao HAO Chuanpu WANG Qing REN Mingfa WANG Yingmin DONG Chuang. CLUSTER-PLUS-GLUE-ATOM MODEL AND COMPOSITION DESIGN OF BCC Ti-Mo-Nb-Zr SOLID SOLUTION ALLOYS WITH LOW YOUNG'S MODULUS. Acta Metall Sin, 2010, 46(9): 1034-1040.
|
|
|
Abstract The composition characteristics of typical bcc β-Ti solid solution alloys with low Young's modulus were analyzed by using the cluster-plus-glue-atom model, in which an alloy structure is dissociated into a cluster part and a glue atom part, i.e. isolated clusters are linked with glue atoms. The cluster here is the nearest neighbor coordination polyhedron with a coordination number of 14 (CN14). It is confirmed that β-Ti solid solution alloys with low Young's moduli satisfy a universal cluster formula [CN14 cluster](glue atom)x given by this model. Alloys, described by cluster formulas [MoTi14]Ti, [MoTi14]Nb, [MoTi14]Nb2 and [Mo(Ti13Zr)]Nb2, Ti-11.8Mo (mass fraction, %), Ti-11.2Mo-10.8Nb, Ti-10.1Mo-19.5Nb and Ti-9.2Zr-9.6Mo-18.7Nb were designed and the alloy rods with diameters of 3 and 6 mm were prepared by copper-mould suction-cast method, respectively. These suction-cast alloys possess monolithic bcc β-Ti structure. The introduction of low-modulus Nb as glue atoms weakens the cluster linking and decreases the Young's modulus. Further substitutions with low-modulus Zr reduces the Young's modulus to 72 GPa in the [Mo(Ti13Zr)]Nb2 alloy. Solution treatment plus subsequent water quenching decreases slightly the Young's moduli of the suction-cast alloys.
|
|
Received: 21 January 2010
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50901012 and 50631010) and National Basic Research Program of China (No.2007CB613902) |
| [1] Matthew D. Adv Mater Processes, 1998; 154: 63
[2] Niinomi M. Sci Tec Adv Mater Processes, 2003; 4: 445
[3] Leyens C, Peters M, translated by Chen Z H. Titanium and Titanium Alloys. Beijing: Chemical Techonology Press, 2005: 369
(莱茵斯C,皮特尔斯M著,陈振华译.钛与钛合金.北京:化学工业出版社,2005: 369)
[4] Yao Q, Xing H, Meng L J,Sun J. Acta Metall Sin, 2008; 44: 19
(姚强, 邢辉, 孟丽君, 孙坚. 金属学报, 2008; 44: 19)
[5] Wang K. Mater Sci Eng A, 1996; 213: 134
[6] Schuh A, Bigoney J, Ho¨nle W, Zeiler G, Holzwarth U, Forst R. Mat wissu Werkstofftech, 2007; 38: 1003
[7] Xu L J ,Chen Y Y, Liu Z G, Kong F T. J Alloys Compd, 2008; 453: 320
[8] Huang L J. PhD Thesis, Beijing Institute of Aeronautical Material, 2006
(黄利军. 北京航空材料研究院博士论文, 2006)
[9] Niinomi M. Mater Sci Eng A, 1998; 243: 231
[10] Zha S Y, Cui Z D, Liu Y J,Zhu S L, Yang X J.Rare Met Mater Eng, 2007; 36: 20
(查树银, 崔振铎, 刘彦军, 朱胜利, 杨贤金. 稀有金属材料与工程, 2007; 36: 20
[11] Martins D Q, Osório W R, Souza M E P, Caram R, Garcia A. Electrochim Acta , 2008; 53: 2809
[12] Hao Y L, Li S J, Sun S Y, Zheng C Y , Yang R. Acta Biomater, 2007; 3: 277
[13] Breme J, Wadewitz V. Int J Oral Maxillofac Implants. 1989; 4: 113
[14] Abdel-Hady M, Hinoshita K, Morinaga M. Scripta Mater, 2006; 55: 477
[15] Bania P J. In: Eylon D, Boyer R R, Koss D A(eds). Beta titanium alloys in the 1990’s, Warrendale, PA: TMS,1993: 6
[16] Dong C, Wang Q, Qiang J B, Wang Y M, Jiang N, Han G, Li Y H, Wu J, Xia J H. J Phys,2007; 40: 273
[17] Wang Q, Dong C, Qiang J B, Wang Y M. Mater Sci Eng A, 2007; 18: 449
[18] Wang H B, Wang Q, Dong C, Yuan L, Xu F, Sun L X. J Phys: Condens Matert,2008;20: 114110
[19] Zhang J, Wang Q, Wang Y M, Dong C. Acta Metall Sin, 2009; 45: 1390
(张杰, 王清, 王英敏, 董闯. 金属学报, 2009; 45: 1390)
[20] Miracle D B, Sanders W S. Philos Mag, 2003; 83: 2409
[21] Singh J, Singh P, Pattan S K, Prakash S. Phys Rev B Condens Matter, 1994; 49: 932
[22] Zhou Y B. Titanium alloy casting. Beijing: Aviation Industry Press, 2000: 26
(周彦邦. 钛合金铸造概论. 北京: 航空工业出版社, 2000: 26)