Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (1): 60-62    DOI:
Current Issue | Archive | Adv Search |
GROWTH OF LARGE SINGLE CRYSTAL Cu FOR NEUTRON MONOCHROMATOR USE
XUE Bai;LIU Jun Deportment of Physfcs;University of Science and Technology of China;Hefei;ZHANG Taiyong;ZHENG Zhaobo University of Science and Technology of China; Hefei
Cite this article: 

XUE Bai;LIU Jun Deportment of Physfcs;University of Science and Technology of China;Hefei;ZHANG Taiyong;ZHENG Zhaobo University of Science and Technology of China; Hefei. GROWTH OF LARGE SINGLE CRYSTAL Cu FOR NEUTRON MONOCHROMATOR USE. Acta Metall Sin, 1988, 24(1): 60-62.

Download:  PDF(217KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Growth of large single crystal Cu by Bridgman-Stockbarer method was reported.The conditions of growth are: temperature gradient at the level of melting temperature=10℃/cm;the lowering speed of crucible=7-12cm/h. The size of the largest crystal is: diameter=4.1cm; length=18cm; weight=2.1 kg
Key words:  copper      single crystal growth      neutron monochromator      Bridgman-Stockbarer method     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/60

1 Dorner B. Coherent Inelastic Neutron Scattering in Lattice Dynamics, Berlin: Springer-Verlag, 1982, Chapt. 2. 1
2 Wernick J H. Davis H M. J Appl Phys, 1956; 27: 149.
3 Bacon G E,谈洪,乐 英译.中子衍射,北京:科学出版社,1980:72,95
4 Modrzejewski A, Kobla J. Krist Teeh, 1969; 4: 13
[1] CHEN Kaixuan, LI Zongxuan, WANG Zidong, Demange Gilles, CHEN Xiaohua, ZHANG Jiawei, WU Xuehua, Zapolsky Helena. Morphological Evolution of Fe-Rich Precipitates in a Cu-2.0Fe Alloy During Isothermal Treatment[J]. 金属学报, 2023, 59(12): 1665-1674.
[2] ZHAO Naiqin, GUO Siyuan, ZHANG Xiang, HE Chunnian, SHI Chunsheng. Progress on Graphene/Copper Composites Focusing on Reinforcement Configuration Design: A Review[J]. 金属学报, 2021, 57(9): 1087-1106.
[3] PENG Wuqingliang, LI Qiang, CHANG Yongqin, WANG Wanjing, CHEN Zhen, XIE Chunyi, WANG Jichao, GENG Xiang, HUANG Lingming, ZHOU Haishan, LUO Guangnan. A Review on the Development of the Heat Sink of the Fusion Reactor Divertor[J]. 金属学报, 2021, 57(7): 831-844.
[4] HUANG Songpeng, PENG Can, CAO Gongwang, WANG Zhenyao. Corrosion Behavior of Copper-Nickel Alloys Protected by BTA in Simulated Urban Atmosphere[J]. 金属学报, 2021, 57(3): 317-326.
[5] Jianqiang REN, Shuhua LIANG, Yihui JIANG, Xiang DU. Research on the Microstructure and Properties of In Situ (TiB2-TiB)/Cu Composites[J]. 金属学报, 2019, 55(1): 126-132.
[6] Pengyue ZHAO, Yongbo GUO, Qingshun BAI, Feihu ZHANG. Research of Surface Defects of Polycrystalline Copper Nanoindentation Based on Microstructures[J]. 金属学报, 2018, 54(7): 1051-1058.
[7] Tingting ZHAO, Zhixin KANG, Xiayu MA. Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities[J]. 金属学报, 2018, 54(1): 109-117.
[8] Tingbiao GUO, Qi LI, Chen WANG, Feng ZHANG, Zhi JIA. Deformation Characteristics and Mechanical Properties of Single Crystal Copper During Equal Channel Angular Pressing by Route A[J]. 金属学报, 2017, 53(8): 991-1000.
[9] Wei FU,Xiaoguo SONG,Long LONG,Jianhang CHAI,Jicai FENG,Guodong WANG. INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. 金属学报, 2016, 52(6): 734-740.
[10] Zhisheng WANG, Xiang CHEN, Yanxiang LI, Huawei ZHANG, Yuan LIU. EFFECTS OF B ON HIGH TEMPERATURE MECHA-NICAL PROPERTIES AND THERMAL FATIGUE BEHAVIOR OF COPPER DIE-CASTING DIE STEEL[J]. 金属学报, 2015, 51(5): 519-526.
[11] ZHUO Weijia, LIU Yuan, LI Yanxiang. EFFECT OF WITHDRAWING RATE ON PORE MORPHOLOGY OF LOTUS-TYPE POROUS COPPER PRODUCED BY SINGLE-MOLD GASAR TECHNIQUE[J]. 金属学报, 2014, 50(8): 921-929.
[12] JIANG Yanbin, LIU Xinhua, WANG Chunyang, MO Yongda, XIE Jianxin. INFLUENCE OF INDUCTION HEATING CONTINUOUS ANNEALING ON RECRYSTALLIZATION AND INTER- FACIAL INTERMETALLIC COMPOUND OF COPPER-CLAD ALUMINUM WIRE[J]. 金属学报, 2014, 50(4): 479-488.
[13] WANG Changgang, DONG Junhua, KE Wei, LI Xiaofang. INVESTIGATION ON PITTING CORROSION BEHAVIOR OF COPPER IN THE MIXED SOLUTION OF HCO3-, SO42- AND Cl-[J]. 金属学报, 2013, 49(2): 207-213.
[14] SUN Feilong, LI Xiaogang, LU Lin, WAN Hongxia, DU Cuiwei, LIU Zhiyong. CORROSION BEHAVIOR OF COPPER ALLOYS IN DEEP OCEAN ENVIRONMENT OF SOUTH CHINA SEA[J]. 金属学报, 2013, 49(10): 1211-1218.
[15] XIANG Hongliang FAN Jinchun LIU Dong GU Xing. EFFECTS OF ANTIBACTERIAL AGING TREATMENT ON MICROSTRUCTURE AND PROPERTIES OF COPPER-CONTAINING DUPLEX STAINLESS STEEL
II. Corrosion Resistance and Antibacterial Properties
[J]. 金属学报, 2012, 48(9): 1089-1096.
No Suggested Reading articles found!