| IN SITU OBSERVATION OF TRANSGRANULAR GROWTH OF MARTENSITE IN A CuZnAl SHAPE MEMORY ALLOY |
| JIN Jialing;Xu Cihuai;SHAO Zichang Shanghai Iron and Steel Research InstituteShanghai Iron and Steel Research Institute;Shanghai |
|
Cite this article:
JIN Jialing;Xu Cihuai;SHAO Zichang Shanghai Iron and Steel Research InstituteShanghai Iron and Steel Research Institute;Shanghai. IN SITU OBSERVATION OF TRANSGRANULAR GROWTH OF MARTENSITE IN A CuZnAl SHAPE MEMORY ALLOY. Acta Metall Sin, 1988, 24(3): 213-216.
|
|
|
Abstract The transgranular growth of martensite in a CuZnAl shape memory alloy was ob-served by using TEM and optical microscope with heating attachment. The analysis shows that thetransgranular growth seems to be a general behavior of thermoelastic martensite at low anglegrain boundaries.
|
|
Received: 18 March 1988
|
1 金嘉陵,邵自昌,金属学报,1986;22:A249 2 冯端,王业宁,丘第荣.金属物理,上册,北京:科学出版社,1964:283 3 冯端,王业宁,丘第荣.金属物理,上册,北京.科学出版社,1964:297 4 金嘉陵.待发表工 |