Acta Metall Sin  1990, Vol. 26 Issue (3): 99-105    DOI:
Current Issue | Archive | Adv Search |
NUMERICAL SIMULATION ON SOLIDIFICATION OF HORIZONTALLY CONTINUOUSLY CAST IRON BAR
ZHU Xianhua;DONG Zengzhang;SU Junyi Xi'an Jiaotong University Foundry Division;Department of Mechanical Engineering;Xi'an Jiaotong University; Xi'an 710049
Cite this article: 

ZHU Xianhua;DONG Zengzhang;SU Junyi Xi'an Jiaotong University Foundry Division;Department of Mechanical Engineering;Xi'an Jiaotong University; Xi'an 710049. NUMERICAL SIMULATION ON SOLIDIFICATION OF HORIZONTALLY CONTINUOUSLY CAST IRON BAR. Acta Metall Sin, 1990, 26(3): 99-105.

Download:  PDF(584KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The solodification process of horizontal continuous cast gray iron barof 4.6 cm in diameter was simulated. The function for distribution of heat fluxon the internal surface of graphite sleeve, which is equal to that on the surface ofiron bar, was inversely derived by using numerical calculation from the tempera-ture distribution in the sleeve measured in real production. By using the distribu-tion of heat flux as a boundary condition on the surface of iron bar, numericalsimulation on solidification of iron bar taking longitudinal heat conduction intoaccount was made. The profile of solidification front obtained from numerical si-mulation was approximately similar to that in real production. In addition, thequantitative relationships of the thickness of solidified layer at the exit of crys-tallizer with the main technological parameters, including the temperature of liq-uid iron at entrance of crystallizer, the moving speed of the bar and the intensityof water cooling, were obtained by using numerical simulation.
Key words:  continuous casting      cast iron      solidification      numerical simulation     
Received:  18 March 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I3/99

1 (木昌)山正孝,梅田高照.金属材料,1970;10(8) :101--105
2 Lewis D M, Savage J. Metall Rev. 1956; 1: 65--71
3 Savage J, Pritchard W H. J Iron Steel Inst. 1954; 178: 269~277
4 堀川一男.铁钢,1975;61:543--545
5 金俊泽,郑贤淑,郭可讱.钢铁,1985;20(5) :19--27F
[1] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[4] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[5] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[6] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[7] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[8] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[9] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[10] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[11] XIA Dahai, DENG Chengman, CHEN Ziguang, LI Tianshu, HU Wenbin. Modeling Localized Corrosion Propagation of Metallic Materials by Peridynamics: Progresses and Challenges[J]. 金属学报, 2022, 58(9): 1093-1107.
[12] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[13] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[14] GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing. A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing[J]. 金属学报, 2022, 58(6): 827-836.
[15] WU Guohua, TONG Xin, JIANG Rui, DING Wenjiang. Grain Refinement of As-Cast Mg-RE Alloys: Research Progress and Future Prospect[J]. 金属学报, 2022, 58(4): 385-399.
No Suggested Reading articles found!