OXIDATION OF NdFeB PERMANENT MAGNETS IN HUMID ATMOSPHERE
HUA Hongci;WANG Geya Shanghai Institute of Metallurgy; Academia Sinica; XU Qingzhen;JIN Huijuan;XU Guiqin Shanghai Iron and Steel Research Institute
Cite this article: 

HUA Hongci;WANG Geya Shanghai Institute of Metallurgy; Academia Sinica; XU Qingzhen;JIN Huijuan;XU Guiqin Shanghai Iron and Steel Research Institute. OXIDATION OF NdFeB PERMANENT MAGNETS IN HUMID ATMOSPHERE. Acta Metall Sin, 1991, 27(1): 141-144.

Download:  PDF(1211KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The oxidation of sintered NdFeB magnets in humid atmosphere at90℃ has been studied by TEM, AES, X-ray and Mossbauer spectroscopy. The blackoxidized structure, enriched with Nd and oxygen and depleted of Fe, was found inthe surface layer by the selective corrosion of the Nd-rich boundary phase and thenpenetrated along grain boundary and spreaded into Nd_2Fe_(14)B matrix phase. Thebrown rust powder, consisting of residual Nd_2Fe_(14)B particles and oxides, e. g., Fe_3O_4,Nd_2O_3, α-Fe_2O_3 and cubic Fe_2O_3, was found after 500 h oxidation. The changes indistribution of Fe atoms at six crystalline sites, especially the loss of Fe atoms atc-site, in oxidized Nd_2Fe_(14)B lattice was measured. The decreaslng in magnetizationof oxidized NdFeB magnets was reported.
Key words:  NdFeB permanent magnet      oxidation      corrosion      Nd_2Fe_(14)B      Nd-rich     
Received:  18 January 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I1/141

1 Sagawa M, Fujimura S, Togawa N et al. J Appl Phys. 1984; 55: 2083
2 Croat J J, Herbst J F, Lee R W et al. J Appl Phys, 1984; 55: 2078
3 Sagawa M Hirosawa S, Yamamoto H et al. Jpn J Appl Phys, 1987; 26: 785
4 Jacobson J. Kim A. J Appl Phys, 1987; 61: 3763
5 Willman C J, Narasimhan K S V L. J Appl Phys, 1987; 61: 3766
6 Nakamura H, Pukuno A, Yoneyama T. In: Proc 10th Int Workshop Rare Earth Magnets and Their Applications, Tokyo, 19 May, 1989, Tokyo, 1989; 315
7 Hasebe A, Otsuki E. In; Proc 10th Int Workshop Rare Earth Magnets and Their Applications, Tokyo, 1989: 383
8 Sagawa M. Fujimura S, Yamamoto H et al. In: Strnat. K J ed. Proc 8th Int Workshop on Rare Earth Magnets and Their Applications and the 4th Int Symp on Magnetic Anisotropy and Coercivity in Rare Earth-Transition Metal Alloys, Dayton, Ohio: Univ of Dayton. 1985: 587
9 Boller H, Oesterreicher H. J Less-Common Met, 1984; 103: L5
10 Herbst J F. Croat J J. Pinkerton F E et al. Phys Rev, 1984; B29: 4176
11 Qian Xiangrong, Jin Huijuan, Xu Ouiqing, et al. In: Strnat K J ed. Proc 8th Int Workshop on Rare Earth Magnets and Their Applicattons and the 4th Int Symp on Magnetic Anisotropy and Coercivity in Rare Earth-Transition Metal Alloys, Dayton. Ohio: Univ of Dayton. 1985: 693
12 Pan S. In: 5th International Symposium on magnetic anisotropy and Coercivity in Rare Earth-Trasiotion metal alloys, September 3, 1987, Bad Soden. FRG, 1987: 419
13 Bate G. In: Wohlfarth E P ed. Ferromagnetic Materials: A Handbook on the Properties of Magn etically Ordered Substances, Vol.II, Amsterdam: North-Holland. 1980: 381
14 华宏慈.钕铁硼永磁材料氧化行为及防护(内部报告).19901
[1] CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang. Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment[J]. 金属学报, 2023, 59(7): 926-938.
[2] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[3] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[4] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[5] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[6] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[7] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[8] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[9] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[10] XU Linjie, LIU Hui, REN Ling, YANG Ke. Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy[J]. 金属学报, 2023, 59(4): 577-584.
[11] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[12] LIU Laidi, DING Biao, REN Weili, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Multilayer Structure of DZ445 Ni-Based Superalloy Formed by Long Time Oxidation at High Temperature[J]. 金属学报, 2023, 59(3): 387-398.
[13] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[14] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[15] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
No Suggested Reading articles found!