Abstract  The kinetics of electrochemical reaction of Nd~(3+) reduced on liquid Gaelectrode has been studied by cyclic voltammetry (CV) in molten chloride at 1073K.The results show that the reduction of Nd~(3+)? on Ga electrode proceeds in consequenttwo steps. For the first step, it is found to be a diffusion controlled reversible re-action at higher rate of potential scan, i. c., Nd~(3+)+e=Nd~(2+) and an irreversible rea-ction controlled by following chemical reaction at lower rate, i. c., Nd~(3+)+e?Nd~(2+)+mCl NdCl'_m~(-m). For the second step, alloying reaction of deposited Nd with Ga canbe observed and the reaction is found to irreversible, Nd~(2+)+2e→Nd(Ga). The stand-ard rate constant of this reactiin is estimated to be 7.0×10~(-3) cm/s.
Key words:  Ga-Nd alloy      molten salt      Nd      cyclic voltammetry     
Received:  18 March 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I3/111

1 杜森林,杜富英,李宝善,路连清,唐定骧.中国稀土学报,1986;4(4) :11
2 Khasgiwale K A, Mehta M M, Pappachan A L, Sundaresan M. J Electrochem Soc, India. 1978; 27(2) : 107
3 Khasgiwale K A, Mehta M M, Pappachan A L, Sundaresan M. J Electrochem Soc India. 1982; 31(2) : 13
4 杨绮琴,伍泽荣,洪惠婵.中国稀士学报,1989;7(1) :1
5 Zing C A, Su Mingzong, Du Senlin, Tang Dingxiang, J Electroanal Chem and Interfacial Electrochem, 1989; 263(2) : 399
6 杨登五,稀有金属,1988;7(3) :225
7 1987; (4) : 770
8 苏明忠,杜森林,唐定骧.中国稀土学报,1988;6(2) :81
9 Nicholson R S, Shain I, Anal Chem, 1964; 36: 706
10 Bard A J, Faulkner L R. Electrochemical Methods, Fundamentals and Applications, New York, Wiley, 1980
11 Nicholson R S, Anal Chem, 1965; 37: 1351
12 Su M, Du S. Tang D. Rare Metals. 1990; 9(3) : 12
13 杨振国,杜维玺,杜森林,刘素兰.中国稀土学报,1989;7(4) :54
[1] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[2] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[5] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[6] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[7] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[8] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[9] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[10] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[11] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[12] FENG Li, WANG Guiping, MA Kai, YANG Weijie, AN Guosheng, LI Wensheng. Microstructure and Properties of AlCo x CrFeNiCu High-Entropy Alloy Coating Synthesized by Cold Spraying Assisted Induction Remelting[J]. 金属学报, 2023, 59(5): 703-712.
[13] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[14] XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui. Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing[J]. 金属学报, 2023, 59(5): 693-702.
[15] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
No Suggested Reading articles found!