| ELECTROCHEMICAL BEHAVIOUR OF Nd~3+ REDUCED ON LIQUID Ga ELECTRODE IN MOLTEN CHLORIDE |
| DU Senlin;SU Mingzhong;Changchun Institute of Applied Chemistry; Academia Sinica |
|
Cite this article:
DU Senlin;SU Mingzhong;Changchun Institute of Applied Chemistry; Academia Sinica. ELECTROCHEMICAL BEHAVIOUR OF Nd~3+ REDUCED ON LIQUID Ga ELECTRODE IN MOLTEN CHLORIDE. Acta Metall Sin, 1991, 27(3): 111-115.
|
|
|
Abstract The kinetics of electrochemical reaction of Nd~(3+) reduced on liquid Gaelectrode has been studied by cyclic voltammetry (CV) in molten chloride at 1073K.The results show that the reduction of Nd~(3+)? on Ga electrode proceeds in consequenttwo steps. For the first step, it is found to be a diffusion controlled reversible re-action at higher rate of potential scan, i. c., Nd~(3+)+e=Nd~(2+) and an irreversible rea-ction controlled by following chemical reaction at lower rate, i. c., Nd~(3+)+e?Nd~(2+)+mCl NdCl'_m~(-m). For the second step, alloying reaction of deposited Nd with Ga canbe observed and the reaction is found to irreversible, Nd~(2+)+2e→Nd(Ga). The stand-ard rate constant of this reactiin is estimated to be 7.0×10~(-3) cm/s.
|
|
Received: 18 March 1991
|
1 杜森林,杜富英,李宝善,路连清,唐定骧.中国稀土学报,1986;4(4) :11 2 Khasgiwale K A, Mehta M M, Pappachan A L, Sundaresan M. J Electrochem Soc, India. 1978; 27(2) : 107 3 Khasgiwale K A, Mehta M M, Pappachan A L, Sundaresan M. J Electrochem Soc India. 1982; 31(2) : 13 4 杨绮琴,伍泽荣,洪惠婵.中国稀士学报,1989;7(1) :1 5 Zing C A, Su Mingzong, Du Senlin, Tang Dingxiang, J Electroanal Chem and Interfacial Electrochem, 1989; 263(2) : 399 6 杨登五,稀有金属,1988;7(3) :225 7 1987; (4) : 770 8 苏明忠,杜森林,唐定骧.中国稀土学报,1988;6(2) :81 9 Nicholson R S, Shain I, Anal Chem, 1964; 36: 706 10 Bard A J, Faulkner L R. Electrochemical Methods, Fundamentals and Applications, New York, Wiley, 1980 11 Nicholson R S, Anal Chem, 1965; 37: 1351 12 Su M, Du S. Tang D. Rare Metals. 1990; 9(3) : 12 13 杨振国,杜维玺,杜森林,刘素兰.中国稀土学报,1989;7(4) :54 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|