EUTECTIC GROWTH OF CAST IRON UNDER RAPID SOLIDIFICATION |
GUO Jingjie;JIA Jun;LI Qingchun;LI Bangsheng Harbin Institute of Technology |
|
Cite this article:
GUO Jingjie;JIA Jun;LI Qingchun;LI Bangsheng Harbin Institute of Technology. EUTECTIC GROWTH OF CAST IRON UNDER RAPID SOLIDIFICATION. Acta Metall Sin, 1991, 27(6): 56-59.
|
Abstract The eutectic growth of cast iron during rapid solidification has been studied with laser remelting and deep etching. A new mode of the mushroom eutectic growth was revealed other than the usual honeycomb and lammellar ones. The mushroom eutectic growth may finally form the lamellar dendrite structure.
|