PREPARATION AND PROPERTIES OF AMORPHOUS Si COATING TiFe HYDROGEN STORAGE MATERIAL |
XU Wenyang;LI jinping;DONG Jinxiang;PAN Junde Taiyuan Polytechnical University |
|
Cite this article:
XU Wenyang;LI jinping;DONG Jinxiang;PAN Junde Taiyuan Polytechnical University. PREPARATION AND PROPERTIES OF AMORPHOUS Si COATING TiFe HYDROGEN STORAGE MATERIAL. Acta Metall Sin, 1992, 28(1): 81-84.
|
Abstract An evident improvement on activation properties of hydrogen storage was made by sputtering an amorphous coating of commercial Si on TiFe alloy. SEM observation revealed an obvious difference betwwen the morphologies before and after hydrogen storage for TiFe al-loy with or without amorphous Si coating. It is believed that this may be quite a developable hydrogen storage material.
|
Received: 18 January 1992
|
1 Hiraki A, Imura T, Kanmura W. Eur Pat, EP, 64 760, 1982 2 唐宾,高原,苏永安,王从曾,徐重.太原工业大学学报,1990;(3) :8 3 Selvam P, Viswanathan B, Swamy C S, Srinivasan V. Int J. Hydrogen Enengy, 1987; 12: 245 4 Reilly J J, Wiswall R H Jr. Inorg Chem, 1974; 13: 218 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|