GLASS-FORMING ABILITY OF Cu_(74)Ni_(12-x)Sn_xP_(14) ALLOYS
ZHANG Heng; ZHANG Bangwei; TAN Zhaosheng (Hunan University; Changsha)
Cite this article:
ZHANG Heng; ZHANG Bangwei; TAN Zhaosheng (Hunan University; Changsha). GLASS-FORMING ABILITY OF Cu_(74)Ni_(12-x)Sn_xP_(14) ALLOYS. Acta Metall Sin, 1992, 28(12): 49-54.
Abstract Effect of Sn on the glass-forming ability of liquid quenched Cu_(74)Ni_(12-x)Sn_xP_(14) alloys has been studied by X-ray diffraction and differential scanning calorimetry. Suitable addition of Sn, saying x=2-6 at.-%, may improve the glass forming ability till a complete amorphous structure of the alloy. Expermental facts were also considered from aspects of dynamics of phase transition and structural chemistry.
1 Zhang Hen, Tan Zhaosheng, Zhang Bangwei, Shu Xiaoklin, Yu Jueqi. J Mater Sci Lett, 1991; 9:45 2 Zhang Hen, Zhang Bangwei, Tan Zhaosheng, Yu Jueqi, Huang Yin. Phys Rev, 1991; 43B: 6430 3 Unlman D R. J Non-Cryst Solids, 1977; 25: 42 4 Donald I W, Davies H A. J Non-Cryst Solids, 1978; 30: 77 5 Turnbull D. J Appl Phys, 1950; 21: 1022 6 Zhang Bangwei. Physica, 1983; 121B: 405 7 Zhang Bangwei. Physica, 1985; 132B: 319 8 Miedema A R, De Chatel P F, De Boer F R. Physica, 1980; 100B: 1 9 Ghosh G, Chandrasekaran M, Delaey L. Acta Metall Mater, 1991; 39: 37 10 Miedema A R, De Boer F R, Boom R. CALPHAD, 1977; 1: 341 11 Naka M, Tomizawa S, Watanabe T, Msumoto T. In: Grant N J, Giessen B C eds., Rapidly Quenched Metals, 2nd Int Conf, Cambridge: Massachusetts Institute of Technology, 1976: 273 12 Zhao Xiujian, Sakka Z. J Non-Cryst Solids, 1987; 95/96: 487 13 Deyong L, Tremblay R, Angers R. Mater Sci Eng, 1990; 124A: 223 14 Lefvre B G, Dannessa A T, Kalish D. Metall Trans, 1978; 9A: 57