In Situ Study on Liquid-Solid Electromigration Behavior in Cu/Sn-37Pb/Cu Micro-Interconnect |
ZHANG Zhijie1, HUANG Mingliang2( ) |
1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China |
|
Cite this article:
ZHANG Zhijie, HUANG Mingliang. In Situ Study on Liquid-Solid Electromigration Behavior in Cu/Sn-37Pb/Cu Micro-Interconnect. Acta Metall Sin, 2020, 56(10): 1386-1392.
|
Abstract Electromigration (EM), which describes the mass transport due to momentum exchange between conducting electrons and diffusing metal atoms under an applied electric field, has become a serious reliability issue in high-density packaging. With the increasing demands for miniaturization, liquid-solid (L-S) EM will pose a critical challenge to the reliability of solder interconnects. In this work, synchrotron radiation real-time imaging technology is used to in situ study the interfacial reaction and atom migration in Cu/Sn-37Pb/Cu solder interconnects undergoing L-S EM at 185 ℃ with a current density of 1.0×104 A/cm2. In the heating stage, Pb atoms directionally migrate from the cathode toward the anode, resulting in the growth of Pb-rich phase at the anode. In the dwelling stage, Pb atoms diffuse backward, then equilibrium phase is obtained. In the cooling stage, Pb atoms directionally migrate from the cathode toward the anode again until the solder solidified, three phases is obtained: the Pb-rich phase, the Sn-Pb phase and the Sn-rich phase. The abnormal migration behavior of Pb atoms in different stages is determined by the combined effect of the chemical potential gradient flux (Jchem) and EM-induced flux (Jem). Jem is determined by the effective charge number (Z*) of Pb atoms, which was calculated to be -3.20 at 185 ℃ based on the growth kinetics of the Pb-rich layer model.
|
Received: 07 January 2020
|
|
Fund: National Natural Science Foundation of China(51801079);National Natural Science Foundation of China(U1837208);National Natural Science Foundation of China(51671046);Natural Science Foundation for Young Scientists of Jiangsu Province(BK20180987) |
[1] |
Tu K N, Gusak A M. A unified model of mean-time-to-failure for electromigration, thermomigration, and stress-migration based on entropy production [J]. J. Appl. Phys., 2019, 126: 075109
|
[2] |
Attari V, Ghosh S, Duong T, et al. On the interfacial phase growth and vacancy evolution during accelerated electromigration in Cu/Sn/Cu microjoints [J]. Acta Mater., 2018, 160: 185
|
[3] |
Liu Y C, Yu Y S, Lin S K, et al. Electromigration effect upon single- and two-phase Ag-Cu alloy strips: An in situ study [J]. Scr. Mater., 2019, 173: 134
|
[4] |
Tu K N, Liu Y X, Li M L. Effect of Joule heating and current crowding on electromigration in mobile technology [J]. Appl. Phys. Rev., 2017, 4: 011101
|
[5] |
Zhang Z H, Cao H J, Chen H T. Formation mechanism of a cathodic serrated interface and voids under high current density [J]. Mater. Lett., 2018, 211: 191
doi: 10.1016/j.matlet.2017.09.111
|
[6] |
Chen C, Liang S W. Electromigration issues in lead-free solder joints [J]. J. Mater. Sci. Mater. Electron., 2007, 18: 259
doi: 10.1007/s10854-006-9020-8
|
[7] |
Yeh E C C, Choi W J, Tu K N. Current-crowding-induced electromigration failure in flip chip solder joints [J]. Appl. Phys. Lett., 2002, 80: 580
|
[8] |
Cahoon J R. A modified "hole" theory for solute impurity diffusion in liquid metals [J]. Metall. Mater. Trans., 1997, 28A: 583
|
[9] |
Huang J R, Tsai C M, Lin Y W, et al. Pronounced electromigration of Cu in molten Sn-based solders [J]. J. Mater. Res., 2008, 23: 250
|
[10] |
Zhang Z J, Huang M L. Abnormal migration behavior and segregation mechanism of Bi atoms undergoing liquid-solid electromigration [J]. J. Mater. Sci., 2019, 54: 7975
|
[11] |
Huang M L, Zhou Q, Zhao N, et al. Abnormal diffusion behavior of Zn in Cu/Sn-9wt.%Zn/Cu interconnects during liquid-solid electromigration [J]. J. Electron. Mater., 2013, 42: 2975
|
[12] |
Huang M L, Zhang Z J, Zhao N, et al. A synchrotron radiation real-time in situ imaging study on the reverse polarity effect in Cu/Sn-9Zn/Cu interconnect during liquid-solid electromigration [J]. Scr. Mater., 2013, 68: 853
|
[13] |
Huang M L, Zhang Z J, Zhao N, et al. In situ study on reverse polarity effect in Cu/Sn-9Zn/Ni interconnect undergoing liquid-solid electromigration [J]. J. Alloys Compd., 2015, 619: 667
|
[14] |
Huang M L, Zhou Q, Zhao N, et al. Reverse polarity effect and cross-solder interaction in Cu/Sn-9Zn/Ni interconnect during liquid-solid electromigration [J]. J. Mater. Sci., 2014, 49: 1755
|
[15] |
Huang M L, Zhang Z J, Zhao N, et al. Migration behavior of indium atoms in Cu/Sn-52In/Cu interconnects during electromigration [J]. J. Mater. Res., 2015, 30: 3316
|
[16] |
Zhang Z J, Huang M L. Liquid-solid electromigration behavior of Cu/Sn-52In/Cu micro-interconnect [J]. Acta Metall. Sin., 2017, 53: 592
|
|
(张志杰, 黄明亮. Cu/Sn-52In/Cu微焊点液-固电迁移行为研究[J]. 金属学报, 2017, 53: 592)
|
[17] |
Qi Y, Lam R, Ghorbani H R, et al. Temperature profile effects in accelerated thermal cycling of SnPb and Pb-free solder joints [J]. Microelectron. Reliab., 2006, 46: 574
|
[18] |
Zeng X Z. Thermodynamic analysis of influence of Pb contamination on Pb-free solder joints reliability [J]. J. Alloys Compd., 2003, 348: 184
|
[19] |
Hu Y C, Lin Y H, Kao C R, et al. Electromigration failure in flip chip solder joints due to rapid dissolution of copper [J]. J. Mater. Res., 2003, 18: 2544
|
[20] |
Liao C N, Chung C P, Chen W T. Electromigration-induced Pb segregation in eutectic Sn-Pb molten solder [J]. J. Mater. Res., 2005, 20: 3425
doi: 10.1557/jmr.2005.0420
|
[21] |
Tammaro M. Investigation of the temperature dependence in Black's equation using microscopic electromigration modeling [J]. J. Appl. Phys., 1999, 86: 3612
doi: 10.1063/1.371268
|
[22] |
Fiks V B. On the mechanism of the mobility of ions in metals [J]. Soviet Phys. Solid State, 1959, 40: 14
doi: 10.1134/1.1130222
|
[23] |
Tu K N. Electromigration in stressed thin films [J]. Phys. Rev., 1992, 45B: 1409
|
[24] |
Adams P D, Leach J S L. Resistivity of liquid lead-tin alloys [J]. Phys. Rev., 1967, 156: 178
doi: 10.1103/PhysRev.156.178
|
[25] |
Kumar P, Howarth J, Dutta I. Electric current induced flow of liquid metals: Mechanism and substrate-surface effects [J]. J. Appl. Phys., 2014, 115: 044915
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|