Please wait a minute...
Acta Metall Sin  1992, Vol. 28 Issue (2): 25-29    DOI:
Current Issue | Archive | Adv Search |
METASTABLE PHASE IN RAPIDLY SOLIDIFIED Ni_3Al ALLOY
YANG Wenying;ZHANG Shouhua;LU Fanxiu University of Science and Technology Beijing
Cite this article: 

YANG Wenying;ZHANG Shouhua;LU Fanxiu University of Science and Technology Beijing. METASTABLE PHASE IN RAPIDLY SOLIDIFIED Ni_3Al ALLOY. Acta Metall Sin, 1992, 28(2): 25-29.

Download:  PDF(883KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A laminar biphase structure may occur in rapidly solidified Ni_3Al and Ni_3Al(B)with over stoichiometrical Al content (25at.--%). Both electron and X--ray diffraction analyses showed that one is matrix phase γ' and other is a metastable phase. After calculation of lattice parameter by reduced cell method, the metastable phase is an orthorhombic structure of a=0.2355 nm, b=0.4157 nm and c=0.1683 nm. It was also proved experimentally that boron alloying does not influence the formation of laminar structure.
Key words:  rapid solidification      Ni_3Al      metastable phase     
Received:  18 February 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I2/25

1 青木清,和泉修.金属,1979;49(10) :38
2 Liu C T, Stiegler J O. Science, 1984: 226: 63
3 Takasugui T, Lzumi O. Acta Metall, 1985; 33: 1247
4 Masahashi T, Takasugi T, Lzumi O. J Mater Sci, 1987; 22: 2599
5 Taub A I, Huang S C, Chang K M. Metall Trans, 1984; 15A: 399
6 Huang S C, Taub A I, Chang K M. Acta Metall, 1984; 32: 1703
7 Schulson E M, Barker D R. Scr Metall, 1983; 17: 519
8 Baker I, Ichishita F, Shulson E M. In: Kear B H, Giessen B C eds., Rapidly Solidified Metastable Materials. Symposium held November, 1983, Boston, New York: North-Holland, 1984: 395
9 Niggli P. Handbuch der Experimental Physik. Band Ⅶ, Leipzig: Aked-Verlag, 1928: 108
10 杨文英.北京科技大学博士学位论文,1988
11 杨文英,吕反修,章守华.金属学报,1990;26:A385,
[1] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[2] Bin ZHAI, Kai ZHOU, Peng Lü, Haipeng WANG. Rapid Solidification of Ti-6Al-4V Alloy Micro-Droplets Under Free Fall Condition[J]. 金属学报, 2018, 54(5): 824-830.
[3] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[4] Jinfu LI, Yaohe ZHOU. Remelting of Primary Solid in Rapid Solidification of Deeply Undercooled Alloy Melts[J]. 金属学报, 2018, 54(5): 627-636.
[5] Qianqian GU, Ying RUAN, Haizhe ZHU, Na YAN. Influence of Cooling Rate on Microstructural Formation of Melt-Spun Fe-Al-Nb Ternary Alloy[J]. 金属学报, 2017, 53(6): 641-647.
[6] Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability[J]. 金属学报, 2017, 53(2): 233-238.
[7] Lei ZHAO,Hongxiang JIANG,Tauseef AHMAD,Jiuzhou ZHAO. STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY[J]. 金属学报, 2015, 51(7): 883-888.
[8] CHEN Feng, SU Dexi, TONG Yunxiang, NIU Liqun,WANG Haibo, LI Li. MICROSTRUCTURE AND PHASE TRANSFORMATION OF Ni43Co7Mn41Sn9 HIGH TEMPERATURE SHAPE MEMORY ALLOY RIBBON[J]. 金属学报, 2013, 49(8): 976-980.
[9] CHEN Shu, ZHAO Jiuzhou. SOLIDIFICATION OF MONOTECTIC ALLOY UNDER LASER SURFACE TREATMENT CONDITIONS[J]. 金属学报, 2013, 49(5): 537-543.
[10] LI Shaoqiang, CHEN Zhiyong, WANG Zhihong, LIU Jianrong, WANG Qingjiang, . MICROSTRUCTURE STUDY OF A RAPID SOLIDIFICATION POWDER METALLURGY HIGH TEMPERATURE TITANIUM ALLOY[J]. 金属学报, 2013, 29(4): 464-474.
[11] SHENG Liyuan, ZHANG Wei, LAI Chen, GUO Jianting,XI Tingfei, YE Hengqiang. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LAVES PHASE STRENGTHENING NiAl BASE COMPOSITE FABRICATED BY RAPID SOLIDIFICATION[J]. 金属学报, 2013, 49(11): 1318-1324.
[12] MO Yunfei, LIU Rangsu, LIANG Yongchao, ZHENG Naichao, ZHOU Lili,TIAN Zean, PENG Ping. MOLECULAR DYNAMICS SIMULATION ON THE EVOLUTION OF MICROSTRUCTURES OF LIQUID ZnxAl100−x ALLOYS DURING RAPID SOLIDIFICATION[J]. 金属学报, 2012, 48(8): 907-914.
[13] HUANG Lian, GAO Kunyuan, WEN Shengping, HUANG Hui, WANG Wei, NIE Zuoren. VALENCE ELECTRON STRUCTURE ANALYSIS OF EQUILIBRIUM AND METASTABLE PHASES OF Al3M(M=Ti, Zr, Hf)[J]. 金属学报, 2012, 48(4): 492-501.
[14] ZHAO Lei ZHAO Jiuzhou. STUDY OF THE SOLIDIFICATION OF Ni-Ag MONOTECTIC ALLOY[J]. 金属学报, 2012, 48(11): 1381-1386.
[15] CAO Yongqing LIN Xin WANG Zhitai YANG Haiou HUANG Weidong. MICROSTRUCTURE EVOLUTION OF Ni-Sn EUTECTIC ALLOY IN LASER RAPID SOLIDIFICATION[J]. 金属学报, 2011, 47(5): 540-547.
No Suggested Reading articles found!