Please wait a minute...
Acta Metall Sin  1992, Vol. 28 Issue (3): 49-54    DOI:
Current Issue | Archive | Adv Search |
METASTABLE EXTENSION OF SOLID SOLUBILITY OF RARE EARTH ELEMENTS IN Al
NING Yuantao;ZHOU Xinming;DAI Hong Institute of Precious Metals; Kunming
Cite this article: 

NING Yuantao;ZHOU Xinming;DAI Hong Institute of Precious Metals; Kunming. METASTABLE EXTENSION OF SOLID SOLUBILITY OF RARE EARTH ELEMENTS IN Al. Acta Metall Sin, 1992, 28(3): 49-54.

Download:  PDF(1525KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The splat foils, 0.04--0.06 mm thick, of Al--RE (RE=Y, La, Ce, Pr, Nd, Sm,Eu, Gd, Tb, Dy, Er, Yb) binary alloys were made by arc--melting and hammer--anvil techniqueat cooling rate in 10~6 K / s order of magnitude. The metastable extended solid solubilities ofthese RE elements have been evaluated by measurements of the lattice spacings of the rapidlysolidified Al--RE alloys, they are 0.4, 0.15, 0.21, 0.21, 0.3, 0.5, 0.1, 0.6, 0.65, 0.7, 0.75, 0.2at.--% for above mentioned individual RE metal, respectively. The secondary phase in rapidlysolidified Al--RE alloys was identified to be Al_4RE for alloys containing light RE and Eu andAl_3RE for alloys containing heavy RE and Y. Some factors influencing the extension of solidsolubility of Al--RE alloys were discussed.
Key words:  rapid solidification      solid solubility      Al-RE alloy     
Received:  18 March 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I3/49

1 Falkenhagen G, Hofmann W. Z Metallk, 1952; 43: 69
2 Duwez P, Willens R H, Klement W Jr. J Appl Phys, 1960; 31: 1136
3 Anantharaman T R, Ramachandrarao P, Suryanarayana C, Lele S, Chattopadhyay K. Trans Indian Inst Met, 1977; 30: 423
4 Jones H. Aluminium, 1978; 54: 274
5 Ning Yuantao, Zhou Xinming, Dai Hong. Chin J Met Sci Technol, 1991; 7: 391
6 Jones H. J Mater Sci, 1984; 19: 1043
7 Staudihammer K P, Murr L E. Atlas of Binary Alloy. New York: Marcel Dekker Inc, 1973: 6
8 JCPDS, Set 19--26, in Powder Diffraction File, Inorganic Volume, No. PDIS--20iRB, 1979: 9
9 JCPDS, Set 18--20, in Powder Diffraction File, Inorganic Volume, No. PDIS--18iRB, 1974: 571
[1] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[2] Jinfu LI, Yaohe ZHOU. Remelting of Primary Solid in Rapid Solidification of Deeply Undercooled Alloy Melts[J]. 金属学报, 2018, 54(5): 627-636.
[3] Bin ZHAI, Kai ZHOU, Peng Lü, Haipeng WANG. Rapid Solidification of Ti-6Al-4V Alloy Micro-Droplets Under Free Fall Condition[J]. 金属学报, 2018, 54(5): 824-830.
[4] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[5] Qianqian GU, Ying RUAN, Haizhe ZHU, Na YAN. Influence of Cooling Rate on Microstructural Formation of Melt-Spun Fe-Al-Nb Ternary Alloy[J]. 金属学报, 2017, 53(6): 641-647.
[6] Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability[J]. 金属学报, 2017, 53(2): 233-238.
[7] Lei ZHAO,Hongxiang JIANG,Tauseef AHMAD,Jiuzhou ZHAO. STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY[J]. 金属学报, 2015, 51(7): 883-888.
[8] CHEN Feng, SU Dexi, TONG Yunxiang, NIU Liqun,WANG Haibo, LI Li. MICROSTRUCTURE AND PHASE TRANSFORMATION OF Ni43Co7Mn41Sn9 HIGH TEMPERATURE SHAPE MEMORY ALLOY RIBBON[J]. 金属学报, 2013, 49(8): 976-980.
[9] CHEN Shu, ZHAO Jiuzhou. SOLIDIFICATION OF MONOTECTIC ALLOY UNDER LASER SURFACE TREATMENT CONDITIONS[J]. 金属学报, 2013, 49(5): 537-543.
[10] LI Shaoqiang, CHEN Zhiyong, WANG Zhihong, LIU Jianrong, WANG Qingjiang, . MICROSTRUCTURE STUDY OF A RAPID SOLIDIFICATION POWDER METALLURGY HIGH TEMPERATURE TITANIUM ALLOY[J]. 金属学报, 2013, 29(4): 464-474.
[11] SHENG Liyuan, ZHANG Wei, LAI Chen, GUO Jianting,XI Tingfei, YE Hengqiang. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LAVES PHASE STRENGTHENING NiAl BASE COMPOSITE FABRICATED BY RAPID SOLIDIFICATION[J]. 金属学报, 2013, 49(11): 1318-1324.
[12] MO Yunfei, LIU Rangsu, LIANG Yongchao, ZHENG Naichao, ZHOU Lili,TIAN Zean, PENG Ping. MOLECULAR DYNAMICS SIMULATION ON THE EVOLUTION OF MICROSTRUCTURES OF LIQUID ZnxAl100−x ALLOYS DURING RAPID SOLIDIFICATION[J]. 金属学报, 2012, 48(8): 907-914.
[13] ZHAO Lei ZHAO Jiuzhou. STUDY OF THE SOLIDIFICATION OF Ni-Ag MONOTECTIC ALLOY[J]. 金属学报, 2012, 48(11): 1381-1386.
[14] CAO Yongqing LIN Xin WANG Zhitai YANG Haiou HUANG Weidong. MICROSTRUCTURE EVOLUTION OF Ni-Sn EUTECTIC ALLOY IN LASER RAPID SOLIDIFICATION[J]. 金属学报, 2011, 47(5): 540-547.
[15] ZHOU Shengyin HU Rui JIANG Li LI Jinshan KOU Hongchao CHANG Hui ZHOU Lian. DENDRITE GROWTH IN SOLIDIFICATION OF UNDERCOOLED Co80Pd20 ALLOY[J]. 金属学报, 2011, 47(4): 391-396.
No Suggested Reading articles found!