Abstract Polycrystalline Ni was implanted with 50 keV B~+ to a dose of 3×10~(17) ions/cm~2 at room temperature. The specimens with and without B~+ implantation were tested in micro-hardness and load or unload tensile fatigue under stress-controlled condition. The surface layer structure was observed with IMA, SEM and TEM before and after implantation and/or fatigue. The B~+ implanted surface region consists of amorphous Ni-B phase, Ni_3B and Ni_4B_3 second phases, and damage structure. The corresponding measurements indicate that both surface micro-hardness and endurance limit of the specimens have increased after implantation. Compared with unimplanted specimens under the same fatigue condition, all implanted specimens show the smallest overall fatigue damage. The cyclic loading at room temperature can lead to migration of implanted B~+ out of surface layer and recrysatallization of amorphous Ni-B phase. Possible strengthening mechanisms for these experimental results were discussed.
|
|
Received: 18 September 1992
|
1 Picraux S T, Pope L E, Science, 1984; 226: 615 2 Hohmuth K, Richter E, Rauschenbach B, Blochwitz C. Mater Sci Ehg, 1985; 69:191 3 Herman H. Nucl Instrum Methods, 1981; 182/183: 887 4 Perry A J. Surf Eng, 1987; 3(2) : 154 5 Vardiman R G, Cox J E. Acta Metall, 1985; 33: 2033 6 Kujre A, Charkabortty S B, Starke E A Jr. Nucl Instrum Methods, 1981; 182/183:949 7 Xu M H, Patu S, Wang Z G. Phys Status Solidi, 1988; 105a; 419 8 McHargue C J. Int Met Rev, 1986; 31(2) : 49 9 Hirvonen J K, Clayton C R. In: Poate J M, Foti G, Jacobson D C eds., Surface Modification and Alloying by Laser, Ion and Electron Beams, New York: Plenum, 1983: 323 10 Grummon D S, Jones J W. Scr Metall, 1986; 20: 311 11 Han J G, Hochman R F. Mater Sci Eng, 1987: 90: 317 12 陈立凡.中国科学院金属研究所硕士学位论文.198 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|