EXTENSION OF SOLID SOLUBILITY BY MECHANICAL ALLOYING IN Fe-Cu SYSTEM
YANG Yuanzheng; MA Xueming; DONG Yuanda (Institute of Solid State Physics; Academia sinica; Hefei)
Cite this article: 

YANG Yuanzheng; MA Xueming; DONG Yuanda (Institute of Solid State Physics; Academia sinica; Hefei). EXTENSION OF SOLID SOLUBILITY BY MECHANICAL ALLOYING IN Fe-Cu SYSTEM. Acta Metall Sin, 1992, 28(9): 25-29.

Download:  PDF(385KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Mechanical alloying was employed to produce super-saturated solution of Fe_(1-x)Cu_x, which is virtually immiscible under an equilibrium condition at ambient temperature. XRD results show that the solutions formed in the concentration ranges of x≤0.15 and x≥0.40 are of bcc structure of α-Fe and fcc structure of Cu, respectively. For the region in between (0.15
Key words:  mechanical alloying      Fe-Cu      immiscible system      super-saturated solid solution     
Received:  18 September 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I9/25

1 Steeb S, Warlimont H. Rapidly Quenched Metals. Amstrdam: North-Holland, 1985
2 Kneller E F. J Appl Phys, 1964; 35: 2210
3 Van Mourik P, Mittemeiser E J, De Keijser T H. J Mater Sci, 1983; 18:2706
4 Sumiyama K, Nakamura Y. Phys Status Solidi, 1984; a81:K109
5 Benjamin J S. Metall Trans, 1970; 1: 2943
6 Schultz L. Mater Sci Eng, 1988; 97: 15
7 Eckert J, Schultz L. J Less-Common Met, 1991; 166:293
8 Shingu P H, Ishihara K N, Uenishi K. In: Clauer A H, De Barbadillo J J eds., Solid State Powder Processing, The Minerals Metals and Materials Society, 1990: 20
9 Campbell S J. Clark P E. J Phys F: Metal Phys, 1974; 4:1073
10 Uenishi K, Kobayashi K F, Ishihara K N, Shingu P H, Mater Sci Eng, 1991; A134: 1342
11 Schumacher S, Birringer R, StrauB R, Gleiter H. Acta Metall, 1989; 37: 2485*
[1] LIU Xuxi, LIU Wenbo, LI Boyan, HE Xinfu, YANG Zhaoxi, YUN Di. Calculation of Critical Nucleus Size and Minimum Energy Path of Cu-Riched Precipitates During Radiation in Fe-Cu Alloy Using String Method[J]. 金属学报, 2022, 58(7): 943-955.
[2] ZHU Xiaohui, LIU Xiangbing, WANG Runzhong, LI Yuanfei, LIU Wenqing. Effects of Ar Ion Irradiation on Microstructure of Fe-Cu Alloys at 290oC[J]. 金属学报, 2022, 58(7): 905-910.
[3] Bin CHEN,Jie HE,Xiaojun SUN,Jiuzhou ZHAO,Hongxiang JIANG,Lili ZHANG,Hongri HAO. Liquid-Liquid Phase Separation of Fe-Cu-Pb Alloy and Its Application in Metal Separation and Recycling of Waste Printed Circuit Boards[J]. 金属学报, 2019, 55(6): 751-761.
[4] Baojun ZHAO,Yuhong ZHAO,Yuanyang SUN,Wenkui YANG,Hua HOU. Effect of Mn Composition on the Nanometer Cu-Rich Phase of Fe-Cu-Mn Alloy by Phase Field Method[J]. 金属学报, 2019, 55(5): 593-600.
[5] Min ZHU, Zhongchen LU, Renzong HU, Liuzhang OUYANG. DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION[J]. 金属学报, 2016, 52(10): 1239-1248.
[6] HU Na, XUE Lihong, GU Jian, LI Heping, YAN Youwei. OPTIMIZATION OF GRADING ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Al13Fe4/Al COM- POSITES IN SITU SYNTHESIZED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2015, 51(2): 216-222.
[7] GU Jian, GU Sasa, XUE Lihong, WU Shusen, YAN Youwei. MICROSTRUCTURE EVOLUTION OF Al-Fe ALLOYS PREPARED BY MECHANICAL ALLOYING AND SPARK PLASMA SINTERING[J]. 金属学报, 2013, 29(4): 435-442.
[8] WANG Man, ZHOU Zhangjian, YAN Zhigang, YU Pengfei, SUN Hongying. TEM CHARACTERIZATION OF DISPERSOIDS AND MICROSTRUCTURE OF ODS-316 AUSTENITIC STEEL[J]. 金属学报, 2013, 49(2): 153-158.
[9] LU Zheng, LU Chenyang, ZHANG Shouhui, XIE Rui, Liu Chunming. PREPARATION AND CHARACTERIZATION OF NANO-STRUCTURED 14Cr-ODS FERRITIC STEEL[J]. 金属学报, 2012, 48(6): 649-653.
[10] HE Xinfu YANG Peng YANG Wen. MOLECULAR DYNAMICS SIMULATION OF MATRIX RADIATION DAMAGE IN Fe-Cu ALLOY[J]. 金属学报, 2011, 47(7): 954-957.
[11] ZHANG Laichang; SHEN Zhiqi; XU Jian. The Role of Sn Substitution for Si And B to Enhance the Amorphization of Mechanically-Milled Ti50Ni22Cu18Al4Si4B2 Alloy[J]. 金属学报, 2004, 40(9): 981-986 .
[12] ZHANG Xiaoqiang; XU Jian. Formation of W Particles /La55Al25Cu10Ni5Co5 Glassy Alloy Matrix Composites By Mechanical Milling[J]. 金属学报, 2004, 40(6): 647-.
[13] HANG Laichang; SHEN Zhiqi; XU Jian. MECHANICALLY--DRIVEN AMORPHIZATION IN A (Ti, Zr, Hf)--(Cu, Ni, Ag)--Al MULTICOMPONENT ALLOY SYSTEM[J]. 金属学报, 2004, 40(4): 421-428 .
[14] REN Shan; HONG Lan; ZHANG Jinxiu (Department of Physics; Zhongshan University; Guangzhou 510275)LU Manqi; HU Zhuangqi (State Key Lab of RSA; Institute of Metal Research; Shenyang 110015). HYDROGEN INDUCING AMORPHIZATION OF Ti-Fe SYSTEM IN MECHANICAL ALLOYING[J]. 金属学报, 1998, 34(4): 373-377.
[15] WANG Zhi;HE Kaiyuan;YIN Jun;ZHANG Yumei;ZHANG LuO;LIANG Zhide (Department of Material Science and Engineering; Northeastern University; Shenyang 110006)(Institute of Materials Physics; Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940). TEMPERATURE DEPENDENCE OF PERMEABILITY FOR Fe-Cu-Nb-V-Si-B NANOCRYSTALLINE ALLOY[J]. 金属学报, 1998, 34(2): 200-204.
No Suggested Reading articles found!