Please wait a minute...
Acta Metall Sin  1992, Vol. 28 Issue (9): 91-94    DOI:
Current Issue | Archive | Adv Search |
TENSILE AND ADHESIVE STRENGTHS OF FINE TiN FILM ON Ti SUBSTRATE
LIU Changqing; LI Meishuan; JIN Zhujing; WU Weitao (Corrosion Science Lab.; Institute of Corrosion and Protection of Metals; Academia Sinica. Shenyang 110015)
Cite this article: 

LIU Changqing; LI Meishuan; JIN Zhujing; WU Weitao (Corrosion Science Lab.; Institute of Corrosion and Protection of Metals; Academia Sinica. Shenyang 110015). TENSILE AND ADHESIVE STRENGTHS OF FINE TiN FILM ON Ti SUBSTRATE. Acta Metall Sin, 1992, 28(9): 91-94.

Download:  PDF(548KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The cantilever bending test, particularly monitored by an acoustic emission technique, was adopted to measure the tensile and interfacial adhesive strengths of the HCD ion-plated fine TiN film on pure Ti substrate. The behaviours of film damaging were found due to: for TiN facing upward, an exceeded internal tensile stress over its tensile strength, and for TiN facing downward, an exceeded shearing stress along film/substrate interface over its adhesive strength. The measured tensile and adhesive strengths are 603 and 242 MPa respectively.
Key words:  tensile strength      adhesive strength      TiN film     
Received:  18 September 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I9/91

1 Wu W, Liu C, Jin Z, Yu L, Shi C, Mater Sci Eng, 1991; A131: 203.
2 Randhawa H. J Vac Sci Technol, 1986; A4: 2755.
3 Coghill M E, St John D H, Surf Coat Technol, 1990; 41: 135.
4 Perry A J, Thin Solid Films, 1981; 78: 77.
5 刘长清,金柱京,吴维(屮又),戴少侠,李美栓,师昌绪,金属学报,1990;26:B27`
[1] ZHANG Lin, GUO Xiao, GAO Jianwen, DENG Anyuan, WANG Engang. Effect of Electromagnetic Stirring on Microstructure and Mechanical Properties of TiB2 Particle-Reinforced Steel[J]. 金属学报, 2020, 56(9): 1239-1246.
[2] Hanchen FENG,Xuegang MIN,Dasheng WEI,Lichu ZHOU,Shiyun CUI,Feng FANG. Effect of Low Temperature Annealing on Microstructure and Mechanical Properties of Ultra-Heavy Cold-DrawnPearlitic Steel Wires[J]. 金属学报, 2019, 55(5): 585-592.
[3] Ran TAO, Yutao ZHAO, Gang CHEN, Xizhou KAI. Microstructure and Properties of In-Situ ZrB2 np/AA6111 Composites Synthesized Under an Electromagnetic Field[J]. 金属学报, 2019, 55(1): 160-170.
[4] Huiying SHI, Chao YANG, Bailing JIANG, Bei HUANG, Di WANG. Influences of Target Peak Current Density on the Microstructure and Mechanical Properties of TiN Films Deposited by Dual Pulsed Power Magnetron Sputtering[J]. 金属学报, 2018, 54(6): 927-934.
[5] Peibei JI, Lichu ZHOU, Xuefeng ZHOU, Feng FANG, Jianqing JIANG. Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire[J]. 金属学报, 2018, 54(4): 494-500.
[6] Linna BAI,Fuping LIU,Sui WANG,Feng JIANG,Jun SUN,Liangbin CHEN,WANG,Fengyuan. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Fe-C-Cu POWDER-FORGED CONNECTING ROD[J]. 金属学报, 2016, 52(1): 41-50.
[7] Xiaolin LI, Zhaodong WANG. EFFECT OF ONE STEP Q&P PROCESS ON MICRO- STURCTURE AND MECHANICAL PROPERTIES OF A DUAL MARTENSITE STEEL[J]. 金属学报, 2015, 51(5): 537-544.
[8] Shude JI,Quan WEN,Lin MA,Jizhong LI,Li ZHANG. MICROSTRUCTURE ALONG THICKNESS DIRECTION OF FRICTION STIR WELDED TC4 TITANIUM ALLOY JOINT[J]. 金属学报, 2015, 51(11): 1391-1399.
[9] AN Tong, QIN Fei, WANG Xiaoliang. MICROSTRUCTURE EVOLUTION AND MECHANICAL BEHAVIOR OF INTERMETALLIC COMPOUNDS IN SOLDER JOINT[J]. 金属学报, 2013, 49(9): 1137-1142.
[10] YAN Shu, LIU Xianghua, LIU WJ, LAN Huifang, WU Hongyan. MICROSTRUCTURE, MECHANICAL PROPERTIES AND STRENGTHENING MECHANISMS OF A Cu BEARING LOW-CARBON STEEL TREATED BY Q&P PROCESS[J]. 金属学报, 2013, 49(8): 917-924.
[11] YANG Jinxia , LI Jinguo, WANG Meng, WANG Yanhui,JIN Tao, SUN Xiaofeng. EFFECTS OF HEAT TREATMENT PROCESS ON THE MICROSTRUCTURE AND PROPERTIES OF A NEW CAST NICKEL-BASED SUPERALLOY[J]. 金属学报, 2012, 48(6): 654-660.
[12] SHI Jing PEI Zhiliang,GONG Jun SUN Chao, MUDERS C M, JIANG Xin. EFFECT OF Si CONTENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ti-Al-Si-N FILMS DEPOSITED BY CATHODIC VACUUM 
ARC ION PLATING
[J]. 金属学报, 2012, 48(11): 1349-1356.
[13] JIA Lina GAO Ming GE Jingru ZHENG Lijing SHA Jiangbo ZHANG Hu. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Nb-16Si-22Ti--2Hf--2Cr--2Al INGOT PREPARED BY VACUUM INDUCTION MELTING[J]. 金属学报, 2011, 47(1): 88-94.
[14] LI Weizhou WANG Qimin GONG Jun SUN Chao JIANG Xin. ONE-STEP DEPOSITION AND INTERFACIAL ADHESIVE STRENGTH OF THE MULTILAYER SYSTEM WITH A DIFFUSION BARRIER[J]. 金属学报, 2010, 46(5): 561-568.
[15] XIANG Hongliang HUANG Weilin LIU Dong HE Fushan. EFFECTS OF N CONTENT ON MICROSTRUCTURE AND PROPERTIES OF 29Cr CASTING SUPER DUPLEX STAINLESS STEEL[J]. 金属学报, 2010, 46(3): 304-310.
No Suggested Reading articles found!