| ON THE IN SITU FORMING TiB_2 REINFORCED Al COMPOSITE |
| MA Zongyi; BI Jing; LU Yuxiong; SHEN Hongwei; GAO Yinxuan (Institute of Metal Research; Academia Sinica; Shenyang) |
|
Cite this article:
MA Zongyi; BI Jing; LU Yuxiong; SHEN Hongwei; GAO Yinxuan (Institute of Metal Research; Academia Sinica; Shenyang). ON THE IN SITU FORMING TiB_2 REINFORCED Al COMPOSITE. Acta Metall Sin, 1992, 28(9): 87-90.
|
|
|
Abstract The in situ forming TiB_2 reinforced AI composite was favourably prepared by reaction-sintering of pure AI, Ti and B powders under vacuum. It is of microsize and free from lattice defect practiclly. A superior room temperature strength and modulus, as well as good elevated temperature properties were obtained as comparison with that of pure Al.
|
|
Received: 18 September 1992
|
1 Westwood A R C. Metall Trans, 1988; 19A: 749 2 Bose A, Mooer B, German R M, StoloffN S, J Met, 1988; 40(9) : 14 3 Ronald T M F. Adv Mater Process, 1989; 135(5) : 29 4 Rawers J C, Wrzesinski W R, Roub E K, Brown R R. Mater Sci Technol, 1990; 6: 187 5 Kuruvilla A K, Prasad K S, Bhanuprasad V V, Mahajan Y R. Scr Metall Mater, 1990; 24: 873R |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|